Qhov sib txawv ntawm 316 thiab 316L

Thawj qhov sib txawv ntawm 316 thiab 316L stainless hlau nyob hauv lawv cov ntsiab lus carbon thiab qhov no cuam tshuam rau lawv cov khoom:

Cov ntsiab lus carbon:

316 stainless hlau feem ntau muaj cov ntsiab lus carbon txog li 0.08%.

316L stainless hlau muaj cov ntsiab lus qis dua, capped ntawm 0.03%. Qhov kev txo qis hauv carbon no txhim kho nws cov kev tiv thaiv corrosion.

Corrosion Resistance:

Ob qib muab kev tiv thaiv zoo rau corrosion, tshwj xeeb tshaj yog nyob rau hauv ib puag ncig chloride. Txawm li cas los xij, 316L cov ntsiab lus qis dua ua rau nws tiv taus corrosion me ntsis, tshwj xeeb tshaj yog nyob rau hauv qhov chaw welded uas carbon tuaj yeem ua rau muaj kev cuam tshuam rau corrosion.

Vuam thiab Fabrication:

316L feem ntau nyiam rau kev siv vuam vim nws txo qis kev pheej hmoo ntawm carbide nag lossis daus thaum lub sijhawm vuam, uas tuaj yeem tshwm sim hauv cov qib siab dua li 316. Qhov no ua rau 316L tsim nyog rau cov haujlwm uas muaj kev vuam dav.

Daim ntawv thov:

Cov qib ob feem ntau yog siv rau hauv ib puag ncig marine, kev ua tshuaj lom neeg, thiab kev siv zaub mov thiab kev kho mob. Txawm li cas los xij, 316L feem ntau nyiam nyob rau hauv cov xwm txheej uas cov ntsiab lus qis dua muab cov txiaj ntsig tseem ceeb, xws li hauv cov khoom siv tshuaj lossis tshuaj ua haujlwm.

316/316L Stainless Hlau Phaj Daim Ntawv Thov:

Zog thiab Hnyav Industries - Roj thiab Roj, Hluav Taws Xob Hlau (Silicon Steel), Hnub Ci Board.

Fais fab nroj tsuag.

Kub Exchangers, boilers

Chemical Storage Vessels

Automotive thiab Tsheb thauj mus los

Architectural thiab kev tsim kho

Marine Building

Khoom siv kho mob

Khoom noj khoom haus tshuab Manufacturing, Khoom noj khoom haus thiab Catering.

Xa kev nug