310S Stainless hlau - Thaum tshav kub kub Resistant

Feb 26, 2026

Tso lus

What is 1.4523 Stainless Steel?316 Stainless Steel Strip - High Temperature Resistant and Industrial Application316 Stainless Steel Profile - Marine Engineering and Corrosion Resistance

 

Chemcial Composition ntawm Qib 310/310S Stainless Hlau

Cov tshuaj muaj pes tsawg leeg ntawm qib 310 thiab qib 310S stainless hlau tau sau tseg hauv cov lus hauv qab no.

Table 1.Cov tshuaj muaj pes tsawg leeg% ntawm qib 310 thiab 310S stainless hlau

Tshuaj muaj pes tsawg leeg

310

310S

Cov pa roj carbon

0.25 max

0.08 max

Manganese

max 2.00 Nws

max 2.00 Nws

Silicon

1.50 max

1.50 max

Phosphorus

0.045 max

0.045 max

Sulfur

0.030 max

0.030 max

Chromium

24.00 - 26.00

24.00 - 26.00

Nickel

19.00 - 22.00

19.00 - 22.00

Mechanical Properties ntawm Qib 310/310S Stainless Hlau

Cov khoom siv kho tshuab ntawm qib 310 thiab qib 310S stainless hlau tau sau tseg hauv cov lus hauv qab no.

Rooj 2.Mechanical zog ntawm qib 310/310S stainless hlau

Mechanical Properties

310/ 310S

Qib 0.2% Pov Thawj Stress MPa (min)

205

Tensile zog MPa (min)

520

Elongation% (min)

40

Hardness (HV) (max)

225

Lub cev muaj zog ntawm Ferritic Stainless hlau

Lub cev lub cev ntawm qib 310 thiab qib 310S stainless hlau tau sau tseg hauv cov lus hauv qab no.

Table 3.Lub cev muaj zog ntawm qib 310/310S stainless hlau

Cov khoom

ntawm

Tus nqi

Chav tsev

Qhov ntom

 

8,000

Kg / m3

Hluav taws xob conductivity

25 degree

1.25

% IACS

Hluav taws xob Resistivity

25 degree

0.78

Micro ohm

Modulus ntawm Elasticity

20 degree

200

GPa

Shear Modulus

20 degree

77

GPa

Poisson tus ratio

20 degree

0.30

 

Melting Rnage

 

1400-1450

degree

Tshwj xeeb kub

 

500

J/kg. degree

Sib Nqus Sib Nqus Permeability

 

1.02

 

Thermal conductivity

100 degree

14.2

W/m. degree

Coefficient ntawm Expansion

0-100 degree

15.9

/ degree

 

0-315 degree

16.2

/ degree

 

0-540 degree

17.0

/ degree