309S Stainless Hlau Yeeb & Tube: Siab -CrNi Nruab Nrab-High Temp Oxidation Resistant Piping
Jan 30, 2026
Tso lus
Dab tsi yog 309S Stainless Hlau Yeeb Nkab & Tube?
309S yog siab -chromium-nickel austenitic stainless hlau yeeb nkab, engineered nrog siab Cr thiab Ni cov ntsiab lus los txhim kho siab - kub oxidation kuj. Nws ua haujlwm raws li tus nqi -kev daws teeb meem zoo rau nruab nrab- qhov kub thiab txias kev lag luam xwm txheej, ntsuas kev ua tau zoo thiab kev lag luam zoo.
Qib sib npaug (Horizontal)
UNS: S30908|JIS: SUS309S|GB: 06Cr23Ni13|EN: X5CrNi23-12|PIB: 1.4828
Chemical Composition (wt%, Kab rov tav)
C: Tsawg dua lossis sib npaug rau 0.08|Si: Tsawg dua lossis sib npaug rau 1.00|Mn: Tsawg dua lossis sib npaug rau 2.00|P: Tsawg dua lossis sib npaug rau 0.045|S: Tsawg dua lossis sib npaug rau 0.030|Cr: 22.00-24.00 Nws Nia: 12.00-15.00|Fe: Sib npaug
Cov khoom tseem ceeb (20 degree, Annealed, Kab rov tav)
Qhov ceev: 7.98g / cm³|Melting Point: 1400-1450 degree|Tensile Strength: Ntau dua lossis sib npaug ntawm 515N / mm²|Yield Strength: Ntau dua lossis sib npaug rau 205N / mm²|Elongation: Ntau dua lossis sib npaug li 40%|Hardness: Tsawg dua los yog sib npaug rau 217HB
Cov yam ntxwv tseem ceeb
• Zoo heev -kub oxidation tsis kam: Ua ib tug tuab oxide zaj duab xis, ua rau ntev - lub sij hawm kev pab cuam ntawm mus txog 1050℃nyob rau hauv oxidizing atmospheres • Txhim khu kev qha siab - kub creep kev ua tau zoo: Resistant deformation nyob rau hauv cyclic siab - kub siab, kev ruaj ntseg thiab kev ua haujlwm yooj yim. siab - cov khoom kub tsis muaj kev ua haujlwm tsis zoo • Nqis - lwm txoj hauv kev zoo rau 310S: Haum rau nruab nrab -siab kub tsis yog- qhov xwm txheej hnyav corrosion zoo li lub tshuab cua sov
309S vs 310S Stainless hlau yeeb nkab (kab rov tav)
Cr Cov ntsiab lus: 309S (22.00-24.00%)|310S (24.00-26.00%)|Ni Cov ntsiab lus: 309S (12.00-15.00%)|310S (19.00-22.00%)|High-Temp txwv: 309S (tsawg dua lossis sib npaug rau 1050 degree)|310S (tsawg dua lossis sib npaug rau 1150 degree)|Tus nqi: 309S (nruab nrab)|310S (siab)
| Element | 309 | 309S | 309H |
|---|---|---|---|
| Chromium | 22.0 feeb-24.0 max. | 22.0 feeb-24.0 max. | 22.0 feeb-24.0 max. |
| Nickel | 12.0 feeb-15.0 max. | 12.0 feeb-15.0 max. | 12.0 feeb-15.0 max. |
| Cov pa roj carbon | 0.20 | 0.08 | 0.04 min.-0.10 max. |
| Manganese | 2.00 | 2.00 | 2.00 |
| Phosphorus | 0.045 | 0.045 | 0.045 |
| Sulfer | 0.030 | 0.030 | 0.030 |
| Silicon | 0.75 | 0.75 | 0.75 |
| Hlau | Tshuav | Tshuav | Tshuav |
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, lossis ntim raws li cov neeg siv khoom xav tau.


Xa kev nug