309 stainless hlau yog austenitic stainless hlau

Apr 14, 2026

Tso lus

410 stainless steel sheet for mildly corrosive environmentsAISI 904L 20mmx4ftx8ft Inox UNS N08904 1.4539 S39042 Hot Rolled Stainless Steel Plate316L Stainless Steel Sheet 1.0mm Cold Rolled ASTM A240 DIN1.4404SUS304 Austenitic Stainless Steel – Versatile Corrosion-Resistant Universal Alloy

Cov ntsiab lus lag luam

Cov ntsiab lus Specification
Yam tsawg kawg nkaus Order Quantity: 5 Tons
Nqe: Yuav tsum sib tham
Ntim Cov Lus Qhia:

Raws li thov

Lub sij hawm xa tuaj: Hauv 7-10 Hnub Ua Haujlwm
Cov nqe lus them nqi: T / T, L / C, Credit Card
Muaj peev xwm muab khoom: 100000 Tons ib hlis twg
Ntawv pov thawj: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Export rau:

United States, UK, Canada, Australia, India, South Africa, Philippines, Kauslim, Brazil, Russia, New Zealand, Qaib ntxhw, Nyab Laj, Malaysia, Lub teb chaws Yelemees, Indonesia, thiab lwm yam.

Tshuaj muaj pes tsawg leeg

C Ni Si S Mn P Cr Mo
               
0.20 max 12.0 – 15.0 0.75 max 0.03 max max 2.00 Nws 0.045 max 22.0 – 24.0

Mechanical Properties

Khoom Imperial Units Metric Units
     
Tensile zog 70-90 hli 480-620 MPa
Yield zog 35-45 hli 240-310 MPa
Vickers Hardness 150-200 HV 150-200 HV
Brinell Hardness 140-160 HB 140-160 HB
Rockwell Hardness PAB 80–95 PAB 80–95
Elongation 30 – 45% 30 – 45%
Elastic Modulus 28 – 30 x 10^6 psi 190-210 GPa