Tshuaj muaj pes tsawg leeg

Hom 304 qib stainless hlau muaj pes tsawg leeg yog muab rau hauv cov lus hauv qab no.

Daim ntawv 1, AISI 304 stainless hlau muaj pes tsawg leeg

Tshuaj muaj pes tsawg leeg,%
ASTM AISI (UNS) C, Tsawg dua los yog sib npaug Si, Less than or equal to Mn, Tsawg dua lossis sib npaug P, Tsawg dua los yog sib npaug S, Tsawg dua los yog sib npaug Cr Ni N, Tsawg dua los yog sib npaug Khoom
ASTM A240/A240M 304 (UAS S30400) 0.07 0.75 2.00 0.045 0.030 17.5-19.5 8.0-10.5 0.10 Phaj, Sheet, thiab Sawb
ASTM A276 / 276M ASTM A276 / 276M / 276M ASTM A276 / 276M ASTM A276 / 276M / ASTM A276 / 276M / ASTM A276 / 276M / ASTM A276 / 276M thiab ASTM A276 / 276M 0.08 1.00 2.00 0.045 0.030 18.0-20.0 8.0-11.0 Bars thiab Shapes

SS304 Stainless Hlau Mechanical Properties

Cov ntaub ntawv-2, cov lus hauv qab no sau SS304 cov khoom siv kho tshuab nrog rau cov khoom siv zog, lub zog tensile, elongation thiab hardness, thiab lwm yam.

Mechanical Properties, cov ntaub ntawv yog rau 25.4 mm (1 in.) inch bar
Hlau (UNS) Tensile zog, MPa (ksi) Yield zog, MPa (ksi) Elongation hauv 50 mm (2 in.), % Ntau dua lossis sib npaug Kev txo qis hauv cheeb tsam (%) Hardness (HB) Qhov xwm txheej
AISI 304 (UNS S30400) 585 (85) 235 (34) 60 70 149 Annealed bar
690 (100) 415 (60) 45   212 Annealed thiab txias kos
860 (125) 655 (95) 25   275 Txias kos siab tensile

Daim ntawv 3, ASTM 304 Stainless Steel Properties - Mechanical Properties

Mechanical Properties
ASTM Hom AISI (UNS) Tensile zog, MPa (ksi) 0.2% Tawm Zog, MPa (ksi) Elongation hauv 50 mm (2 in.), % Ntau dua lossis sib npaug Kev txo qis ntawm cheeb tsam, %, Ntau dua lossis sib npaug Brinell Hardness (HBW) Tsawg dua lossis sib npaug Rockwell Hardness (HRBW) Tsawg dua lossis sib npaug Khoom Qhov xwm txheej
ASTM A240/A240M 304 (UAS S30400) 515 (75) 205 (30) 40 201 92 Phaj, Sheet, thiab Sawb
ASTM A276A / 276M Cov Lus Qhia 515 (75) 205 (30) 40 50 Bars thiab Shapes Kub tiav
620 (90) 310 (45) 30 40 Txias tiav, Dia Tsawg dua lossis sib npaug rau 12.7mm (0.5 nyob rau hauv)
515 (75) 205 (30) 30 40 Txias tiav, Dia. > 12.7mm (0.5 nti)