304 yog cov khoom siv austenitic stainless hlau ntau tshaj plaws nyob rau hauv lub ntiaj teb no, uas yog qhov sib npaug ntawm 18.00-20.00% chromium thiab 8.00-12.00% nickel muaj pes tsawg leeg. It forms a dense, stable passive oxide film on the surface, providing excellent general corrosion resistance in atmospheric, fresh water, and mild chemical environments. Nrog lub ntsej muag -centered cubic austenitic qauv, nws tsis yog-magnetic nyob rau hauv lub xeev annealed, featuring zoo ductility, txias forming peev xwm, thiab weldability. Qib no yog tus nqi-zoo thiab muaj ntau yam, ua raws li tus qauv kev xaiv rau feem ntau cov kev siv tsis zoo corrosive thoob plaws hauv pej xeem, kev lag luam, thiab kev lag luam.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.08, Si Less dua lossis sib npaug 1.00, Mn Tsawg dua lossis sib npaug 2.00, P Tsawg dua lossis sib npaug 0.045, S Less dua lossis sib npaug 0.030, Cr: 18.00-20.00, Ni: 8.00-12.00, sib npaug

Tej yam cuab yeej cuab tam (Annealed Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug li 515 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 205 MPa; Elongation (A): Ntau dua lossis sib npaug li 40%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 187

Core Zoo

Zoo heev corrosion kuj nyob rau hauv ib puag ncig me me; non- sib nqus thiab siab ductility rau txoj kev sib sau; yooj yim rau welding tsis muaj preheating yuav tsum tau; tus nqi- zoo thiab muaj dav; ntau yam rau ntau yam kev siv.

Daim ntawv thov

Cov khoom siv hauv chav ua noj, cov khoom siv ua zaub mov, khoom vaj khoom tsev kho kom zoo nkauj, cov khoom siv hauv tsev, cov kav dej, cov rooj tog zaum stainless hlau, thiab cov khoom siv dav dav.

Qib sib npaug

UNS S30400, STS304, SUS304, EN 1.4301, GB 06Cr19Ni10

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug