304/304L Stainless Hlau Phaj / Sheet nrog High Corrosion Resistance
Mar 16, 2026
Tso lus



| Txuj |
ASTM A240/A240M |
|---|---|
| Qib |
1.4301/1.4307/1.4948, SUS 304/304L/304H |
| Ntev |
2000mm - 6000mm (78.74 "- 236.22"), Customized |
| Thickness |
0.3 hli - 100 hli (0.012 "- 3.937"), Customized |
| Dav |
1000mm - 2000mm (39.37 "- 78.74"), Customized |
| Nto tiav |
2B, 2D, 8K, BA, Checkered, Customized, Embossed, Etching, Plaub Kab, Daim iav, No.1, No.4, No.8, Sand Blast |
| Cov txheej txheem |
Annealing, Txias Rolling, Txiav, Kub Rolling |
| Daim ntawv |
Checkered Phaj (Pib Pob Zeb Diamond), Clad Phaj, Coil, Customized, Flat Phaj, Perforated Phaj, Sheet, Sawb, Textured Phaj |
Cov ntsiab lus ua lag luam khoom
| Cov ntsiab lus lag luam | Specifications |
|---|---|
| Yam tsawg kawg nkaus Order Quantity: | 5 Tons |
| Nqe: | Yuav tsum sib tham |
| Ntim Cov Lus Qhia: |
Raws li thov |
| Lub sij hawm xa tuaj: | Hauv 7-10 Hnub Ua Haujlwm |
| Cov nqe lus them nqi: | T / T, L / C, Credit Card |
| Muaj peev xwm muab khoom: | 100000 Tons ib hlis twg |
| Ntawv pov thawj: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export rau: |
United States, Canada, Philippines, India, Australia, United Kingdom, Malaysia, Russia, Indonesia, Mexico, Brazil, Lub teb chaws Yelemees, Kauslim Teb, Thaib, United Arab Emirates, Nyab Laj, Fabkis, Hong Kong, Ltalis, Netherlands, New Zealand, Singapore, Spain, Taiwan, Argentina, Bangladesh, Cambodia, Finland, Greece, Nigeria, Pakistan, Qatar, Saudi Arabia, Qaib ntxhw, thiab lwm yam. |
Tshuaj muaj pes tsawg leeg
| Qib | Chromium (Cr) | Nickel (Ni) | Cov pa roj carbon (C) | Manganese (Mn) | Silicon (Si) | Phosphorus (P) | Sulfur (S) |
|---|
| 304 | 18.0-20.0% | 8.0-10.5% | Tsawg dua lossis sib npaug li 0.08% | Tsawg dua lossis sib npaug li 2.0% | Tsawg dua lossis sib npaug li 1.0% | Tsawg dua lossis sib npaug li 0.045% | Tsawg dua lossis sib npaug li 0.03% |
| 304L | 18.0-20.0% | 8.0-12.0% | Tsawg dua lossis sib npaug li 0.03% | Tsawg dua lossis sib npaug li 2.0% | Tsawg dua lossis sib npaug li 1.0% | Tsawg dua lossis sib npaug li 0.045% | Tsawg dua lossis sib npaug li 0.03% |
| 304H | 18.0-20.0% | 8.0-12.0% | Tsawg dua lossis sib npaug li 0.04% | Tsawg dua lossis sib npaug li 2.0% | Tsawg dua lossis sib npaug li 1.0% | Tsawg dua lossis sib npaug li 0.045% | Tsawg dua lossis sib npaug li 0.03% |
Xa kev nug