430 kub dov stainless hlau teeb

430 kub dov stainless hlau teeb

Lub npe: 430 kub dov stainless hlau Beams
Ntawv pov thawj: ISO, CE
Cov duab: h zoo li kuv ua qauv t puab
Cov txheej txheem: Kub Rolled
Nto Kho: Tsis muaj {{{.1, ba, 2b, 2d, tsis muaj.4
Qauv: Muaj
Kev Pab Cuam: Vuam, xuas nrig ntaus, txiav, khoov, decoiling
Lub sij hawm xa tuaj: 7-15 hnub
Daim Ntawv Thov: Kev Tsim Kho, Kev Lag Luam Automotive, Tsev neeg
Cov Lus Qhia Tshwj Xeeb: Raws li cov neeg yuav tsum tau ua
Xa kev nug
Tsham tam sim no

Dab tsi yog 430 stainless hlau kab teeb?

430 kub dov stainless hlau teebyog ferritic tsis-hardening stainless hlau uas muaj mob corrosion thiab zoo heev.
Lub ntsiab nta:
Qeb: AISI 430 / EN 1.4016
Txheem: Astm A276 / A484
Nto: Kub Rolled (Dub), Yeem Pickling
Cov duab: H-Beam / I-Beam / Customized profiles

430 Hot Rolled Stainless Steel Beams 

Qhov Zoo

🔹 yog 430 ferritic stainless ha nqaj xeb-pov thawj?
Nws muaj cov corrosion tsis kam, zoo tagnrho rau cov chaw qhuav lossis npog ib puag ncig {{} Tsis haum rau cov tubrog nkoj lossis cov}}

🔹 Dab tsi yog tus nqi ntawm AISI 430 h nqaj?
430 h cis feem ntau yog 30-50% pheej yig dua 304 stainless hlau, nyob ntawm qhov loj thiab ua tiav {{4}

🔹 muaj 430 kub dov lub nqaj hlau nplaum?
Yog . tsis zoo li 304/316, 430 yog sib nqus, ua kom haum rau cov ntawv thov ferromagnetism {}}

ASTM 430 Stainless Cuab Nrig Ci

Yam Kev qhia tshwj xeeb
Khoom Siv Khoom AISI 430 / EN 1.4016 / UNRY S43000
Lub hom phiaj ASTM A276, ASTM A484 (kub dov qauv duab)
Khoom Yam H nqaj / i Beooj / kev cai profile nqaj
Nto tas Kub rolled (dub), pickled (yeem)
Cov txheej txheem tsim khoom Kub Rolling + Ncaj Ncees
Qhov ntau thiab tsawg (h × b) 100 × 100 hli rau 300 × 300 hli (Customizable)
Ntev ntev li cas 6 m, 9 m, 12 m lossis kev cai
Thickness Ntau Yam Web: 4-12 hli; Flange: 6-20 mm
Lub zog tensile Ntau dua los yog sib npaug rau 450 MPa
Tawm Zog (0.2% offset) Ntau dua los yog sib npaug rau 275 mpa
Elongation Ntau dua los yog sib npaug rau 22%
Kev nyuaj Tsawg dua los yog sib luag rau 200 HB
Ceev 7.7 g / cm³
Hlau Yog (Ferritic qauv)

430 Stainless Hlau Nqaj Nqe Siv (2025)

Dimension (mm) Nyhav (kg / m) Kwv yees . tus nqi (USD / METJ)  
100x100x6x8 17.2 $18 – $25  
150x150x7x10 31.5 $28 – $38  
200x100x5.5x8 21.3 $23 – $32  

Vim li cas thiaj xaiv GNEE

ISO 9001 Ntawv pov thawj zeb nrog Adever Rolling thev naus laus zis
Saj zawg zog Moq rau me me lossis loj-teev kos duab kos duab kos duab
Precision Machining thiab Nrov Tas Rau A Astm A484
Cov Khoom Siv Hauv Ntiaj Teb Cov saw nrog cov xa khoom ceev rau Tebchaws Europe, Asia, Asmeskas
Thov cov lus tsocai tam sim no!

Txawm hais tias koj nyob nraum sidcing 430 kub dov stainless kab teeb rau kev tsim kho, lossis cov khoom siv coj mus muag ua ke hauv Suav teb nrog lub chaw ua haujlwm txawv teb chaws.

Hu rau tam sim no


Gnee Stainless Hlau Hoobkas

magnetic stainless I beams

Gnee Cov Khoom Tsheb Thauj

AISI 430 H beam China manufacturer

Gnee Cov Neeg Siv Khoom

 430 Stainless Steel Beam

Cim npe nrov: 430 KUB ROLDED Stainless Hlau Beams, Tuam Tshoj 430 Kub Rolled Stainless Hlau Beams Manufacturers, lwm tus neeg, Hoobkas

Tug:Tsis muaj

Xa kev nug