ASTM A 479 316}} stainless hlau hloov bar
Ntawv pov thawj: ISO, AISI, ASTM, GB, en, din, jis
Puab: Round
Cov txheej txheem: Rolled txias
Thickness: 2mm-300 hli
Dav: 1000mmm -2000 hli
Ntev: raws li koj qhov yuav tsum tau ua
Txoj kab uas hla tsis kam: H9, H11, H13, K9, K11, K13 thiab lwm yam
Qauv: Dawb Qauv
Nto: Tsis muaj, tev, polishing, ci, ci me me,
Pob Thauj: Ntoo Pob
Dab tsi yog ovm 479 316}} Stainless Hlau Round bar?
316 Stainless Hlau Round Bars ua raws liATM A 479-23thiab sib raug zoo mus rau qib 316 stainless hlau (uns tsis yog ({}
316 stainless hlau bar rau siab cov hlab

Qhov Zoo Ntawm 316 Stainless Hlau Round Bars
🔹316 corrosion-resistant stainless hlau tuavmuaj 2-3% molybdenum (mo), muab ob zaug chloride ion (cl ion) corrosion tsis kam ntawm 304 stainless hlau. lawv dhau lub{{01000- teev ntsev ntsuas (ISO 9227)uas tsis muaj xeb liab nyob saum npoo av, ua rau lawv haum rau nkoj cov khoom thauj khoom, thiab cov cuab yeej tshuaj tiv thaiv kab ke tawm tsam, thiab cov pa hluav taws xob tua hluav taws xob "{0}}
🔹Faj Hoog-Qib 316 Stainless Hlau Round BarsUa raws li GB 4806 {. 9 (Tuam Tshoj) thiab EU 10/06) thiab lwm yam rau cov khoom siv cov khoom siv tshuab hluav taws xob thiab cov khoom siv tshuaj pab txhawb nqa cov khoom.
🔹Kev Tshuaj Khwv-Qib 316 Stainless Hlau Tuavyog siv rau lub nkoj siab bolts, tiv taus hluav taws xob thiab txhim kho kev kho mob hnyav ntawm 650℃lub cev yuag tsawg dua lossis sib npaug rau 1. 0 g / m²).
Vim li cas thiaj xaiv GNEE
Gnee muaj AN479 ntawv pov thawj thiab ISO 9001: 201}}}}}}}}}}}}}}}}} Cov khoom siv tshuab hluav taws xob tau xa hauv 7-15 hnub {10. nws txhawb nqa me me kev txiav txim (qhov kawg txiav txim kom muaj nuj nqis 50kg) thiab muab cov qauv ntsuas dawb {12}
Nyem lub pob hauv qab no kom tau:
Real-lub sij hawm hais rau 316 Stainless Hlau Round Bar (suav nrog cov nqi rau cov kev kho cov sib txawv)
Cov ntaub ntawv ntawv pov thawj ntaub ntawv (ASTM A479 daim ntawv pov thawj + ROHS daim ntawv tshaj tawm)
Kev ua cov ntaub ntawv siv (nrog cov qhua tuaj noj mov cov ntaub ntawv uas yog corrosion)
ASTM A 479 316} stainless hlau hloov bar specifications
| Yam | Cov ntsiab lus |
|---|---|
| Teem nqi | ATM ASTM A 479-23}}, tsis yog S31600, 316 Stainless hlau (sib npaug rau en 1.4401, Jis Sus316) |
| Cov kab uas hla | - Kub dov: φ10mm - φ300mm - Khaub Niag Dright Bright: φ6mm - φ100mm - precision polished: φ6mm - φ20mm (ra tsawg dua lossis sib npaug rau 0.8μm, tsom iav tiav) |
| Kev nyiaj tau | - Kub dov: ± 0.5 hli - ± 2 hli - Khaub thuas: ± 0.01 hli - ± 0.0mm (H6 / h7 / h8 precision) - polished: ± 0.02mm (rau φ 6-20 hli) |
| Qho ntev | - Txuj Ci: 6M tsau ntev - Nchuav: Txiav kom txiav txim (qhov tseeb ± 5mm, tsawg kawg nkaus ntev 500 hli) |
| Cov Khoom Siv Neeg Kho Tshuab | - Lub zog tensile: ntau dua los yog sib npaug rau 515 MPa - Putt lub zog: ntau dua los yog sib npaug rau 205 MPa - elongation: ntau dua lossis sib npaug rau 40% - Hardness: tsawg dua los yog sib luag rau 217 HB (as-annealed) |
| Qauv Ua Haujlwm | - ASTM A479, ASME SAU SA -479 - en 10088-2}, jis g4303 - FDA 21 CFR 174.5 (Kev Hu Dawb Ua Raws Li:, EU 10/2011 |
316 stainless hlau bar rau ib kg
Tus nqi siv (2025):
Conventional kaj ci (10-50 mm): 18-22 Yuan / kg;
Precision polished bar (6-20 mm): {}} yuan / kg .