Stainless hlau sib npaug- ceg} ceg tawv tawv tawv nrog txoj cai {{2}- zoo nkauj hla ntu. Cov ntaub ntawv uas muaj xws li cov hlau tsis muaj tshuaj tiv thaiv xws li 304, thiab 904, thiab lwm yam kev ua haujlwm tau ua tiav thiab lwm txoj kev sib txuas lus kom ua tau raws li cov kev txhawb nqa cov qauv txheej txheem sib txawv.

 

Stainless Hlau Sib Xws

 

stainless steel equal angle

 

Stainless hlau sib txig lub kaum qhov kev qhia

 

Khoom Siv Khoom

304 (uns uns200), 304l (s30403), 316 (Kaum 1), 316L (S31603)

Txuj Ci

-} Astm A276 / A484
{{0- en 1.4301 (304), 1.4401 (316)
- Jis Sus304 / sus316
- gb / t 1220

Qho loj

-} ceg ntev (A × a): 20 × 20 xyoo- 200 × 200 hli
- thickness (t): 3mm-30mm

Qho ntev

6m (txuj ci), kev cai ntev: 1M-12m

Nto tas

- kub rolled zeb tiav
{{0 {}} polished (# 180- # 600)
- pickled & passivated

 

Stainless hlau sib npaug kaum

 

Teem nqi

Tshuaj Muaj Tshuaj

Cov Khoom Siv Neeg Kho Tshuab

Corrosion Kuj

304

Cr 18-20%, ni 8-10%

Tawm los ntau dua los yog sib npaug rau 205 MPa, tensile ntau dua lossis sib npaug rau 515 MPa

Tsis tawm tsam qaug zog acids / alkalis, tsawg dua los yog sib npaug rau 10,000ppm cl

316L

Cr 16-18%, NI 10-14%, MO 2-3%, C Tsawg dua lossis sib npaug rau 0.03%

Tawm los ntau dua lossis sib npaug rau 170 MPa, tensile ntau dua lossis sib npaug rau 485 mpa

ResistS seawater, tsawg dua los yog sib npaug rau 30,000ppm cl

904L

CR 19-23%, NI 23-28%, MO 4-5%, CU 1-2%

Tawm los ntau dua lossis sib npaug rau 220 mpa, tensile ntau dua lossis sib npaug 520 mpa

Tsis kam sulfuric

 

Vim li cas cov tshuaj tsim kev lag luam xaiv GNEE?

 

  • 18 xyoo kev, txhua xyoo ntau lawm muaj peev xwm ntawm 10,000 tons, tus nqi txo ntawm 15%.
  • 304/5 316L / 904L yog hauv Tshuag thiab txhawb kev hloov kho.
  • ISO 9001 / ASME BPV daim ntawv lees paub, SGS daim ntawv qhia.
  • Kev xaiv pub dawb, kev tawm tswv yim thiab kev sim ntsuas.

 

Stainless Hlau Bar Lub Tuam Tshoj Lub Kaum

 

Stainless Steel Bar Angle Suppliers

 

Cov FAQ

 

Q: Yuav ua li cas xaiv stainless hlau sib npaug lub kaum stip khoom?

A: Xaiv 304 rau ib puag ncig ib txwm muaj, 316L rau noo / chlorine-}} muaj ib puag ncig, thiab 904L rau cov muaj zog acid.

Q: Dab tsi yog qhov txawv ntawm 316L thiab 316?

A: 316L muaj cov ntsiab lus roj carbon qis (tsawg dua los yog sib npaug rau 0.03%) thiab tsis muaj kev pheej hmoo ntawm kev sib txuam corrosion tom qab vuam.

Q: Puas yuav khoov duav?

A: Nws tuaj yeem txias - bent los yog kub -}} Xav tau xaiv raws li cov tuab.

 

Cim npe nrov: Stainless hlau sib txaws kaum, Tuam Tshoj Stainless sib txig lub kaum ntse ntse tuam ntxhab, lwm tus neeg, Hoobkas

Xa kev nug