ASTM A213 TP321 Cov Hlau Stainless Hlau Cua Sov Hluav Taws Xob

ASTM A213 TP321 Cov Hlau Stainless Hlau Cua Sov Hluav Taws Xob

Lub npe: ASTM A213 Tp3
Hom: Seamless
Txheem: ASTM A213 / ASME SA213
Puab: Round
Cov txheej txheem: Rolled txias
Nto Kho: Ci
Thauj Pob: Txheem Pob
Cov Lus Qhia Tshwj Xeeb: 10.3-610mm
Ntau Lawm Muaj Peev Xwm: 50000 tons
Xa kev nug
Tsham tam sim no

ASTM A213 Tp321 Seamless Stainless Hlau Tube Rau Cov Khoom Siv Hluav Taws Kub

 

Cov txheej txheem tsim khoom ntawm Tp321 Cov Khoom Siv Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob kom nruj ua raws li cov txheej txheem xws li kub kub, relding thiab seamless.
ASTM A213 TP321 Stainless Hlau Seamless Tubes Tswj siab rau cov pa hluav taws kub hauv qab no 900 qhov kev daws teeb meem ntau dua rau cov tshuaj tiv thaiv kub) Tom qab vuam.

 

ASTM A213TP321Stainless hlau yeeb nkab kho

ASTM A213 TP321 Stainless steel heat exchanger tubes
ASTM A213 TP321 Cov Hlau Stainless Hlau Cua Sov Hluav Taws Xob
20250402095916
ASTM A213 TP321 Stainless Hlau Superheater Tres

Vim li cas xaiv GNEE

 

Gnee yog nruab nrog high - prececision colling (xws li cov cheeb tsam uas tsis muaj zog (xws li phab ntsa.
Tsis tas li ntawd, nws tseem muaj siab - kub flaring, khoov thiab lwm yam kev tsim cov txheej txheem ntawm cov txheej txheem ua haujlwm (xws li U {kua txiv thiab Serpentine tub).

Yog koj muaj lus nug txog txoj haujlwm no, thov hu rau peb!

 

Hu rau tam sim no

ASTM A213 TP 321 Seamless Boiler Tube Kev qhia tshwj xeeb

Txheem: ASTM A213 / ASME SA213 Khoom siv: TP321; Tp321h; 1.4541; 1.4878
Hom Tube: U - bend / ncaj seamless raj Ntev: 6m lossis cov lus ntev raws li yuav tsum tau ua
Daim Ntawv Thov: Cov Hluav Taws Kub, Bolier Kev Xa Khoom: Daws anealed & pickled; Ci Ntsej Muag
Ntsuam xyuas: Eddy ntsuas, hilostatic kuaj, ultrasonic xeem, grain loj sim, Pob: Plywood rooj plaub / woven hnab hauv pob

ASME SA213 TPORUCLESS BOILER BOILER ROJ RAJ CIA TSHUAJ:

Teem nqi Tsis yog C Mn P S Si Cr Ni Ti
TP321 S32100 0.08 max 2.00 Max 0.045 Max 0.03 max 1.00 Max 17.0-19.0 9.0-12.0 5(C+N)-0.07

SA213 TPAP31 Kev Kub Siab Siab Seamless Boiler Tube Cov Khoom:

Teem nqi Lub zog tensile, min, ksi (mpa)

Paib muaj zog,

min, ksi (mpa)

Elongation nyob rau hauv 2 hauv.

lossis 50 hli, min (%)

Kev nyuaj

Soloring kub,

min,℃f (degree)

Ua las voos Brinell / vickers
TP321 75(515) 30(205) 35 90HRB 192hbw / 200hv 1900(1040)

Suav Teb A213 Tp313 stainless hlau stainless hlau raj manufacturers

China A213 TP321 Stainless Steel Tube Manufacturers

ASTM A213 / ASME SA213 TP321 Yeeb NkabKhoom

ASTM A213/ASME SA213 TP321 Steel Pipe Stockist

Cim npe nrov: ASTM A213 TP321 Cov Khoom Siv Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob, Tuam Tshoj ASTM A213 Tp3erless

Xa kev nug