ASTM A213 TP304 Stainless Hlau Tube Rau Chav
Hom: Seamless
Section Shape: Round
Sab nraud: 6 ~ 914mm / (1/8 "~ 36")
Thickness: 1 ~ 45mm / Sch10s ~ Sch XXS
Ntev: 1500mm ~ 12000mm, raws li kev cai.
Cov txheej txheem: Kub-rolled/Cold-rolled/Cold drawing
ASTM A213 TP304 Stainless Hlau Tube Chaw tsim tshuaj paus
ASTM A213 TP304 steel kav yog tsim los siv seamless kub- ua hauj lwm los yog txias - cov txheej txheem ua hauj lwm thiab muab nyob rau hauv ib lub tshav kub - kho mob. ASTM A213 TP304 stainless hlau kav xa los ntawm GNEE tau txais ntau- dhau los ntawm kev kos duab txias lossis txias dov los ntawm kub- dov hollows. Kev daws annealing yog ua nyob rau hauv lub cub tawg tas li ntawm 1040℃(1900℃F), ua raws li dej quenching lossis cua txias sai; Qhov no ua kom cov pa roj carbon yog tag nrho yaj mus rau hauv austenite matrix, tshem tawm kev ua haujlwm nyuaj, thiab rov ua kom zoo dua corrosion. Txhua lub tshav kub yog nrog los ntawm EN 10204 3.1 Material Test Certificate (MTC).
Hais txog qhov raug qhov tseeb, GNEE's ASTM A213 TP304 seamless kav feem ntau muaj qhov dav sab nraud (OD) xws li 6.35 hli txog 127 hli (1/4 "-5") thiab phab ntsa tuab ntawm 0.5 hli txog 12.7 hli, nrog qhov ntev customizable rau qhov yuav tsum tau ua. Rau cov ntawv thov xws li cov khoom siv hluav taws xob sib pauv thiab cov khoom siv hluav taws xob uas xav tau ntau dua, GNEE muaj cov kev pabcuam suav nrog kev tswj kom nruj dua, kho-ntev txiav, thiab U- khoov fabrication.
Hais txog qhov zoo ntawm qhov chaw, peb muab ntau yam tiav, suav nrog Bright Annealed (BA), Annealed thiab Pickled (AP), thiab Pickled nto. Ob qho tib si sab hauv thiab sab nrauv qhov zoo yog tswj hwm nruj kom ntseeg tau tias cov pa ntws zoo, txo qhov kev pheej hmoo ntawm kev ntsuas, thiab txhim kho cov cua sov ua haujlwm. Rau cov ntawv thov precision, qhov roughness tuaj yeem ua tau raws li qhov tshwj xeeb ntawm Ra Tsawg dua lossis sib npaug li 0.8 μm.


GNEE tuav cov khoom npaj npaj ntawm ASTM A213 TP304 stainless hlau kav uas npog cov kev qhia tshwj xeeb rau chav tshuab- xws li ODs ntawm 19.05 hli, 25.4 hli, 31.75 hli, 38.1 hli, thiab 50.8 hli Cov khoom lag luam txheem muaj nyob rau hauv kev xa khoom sai hauv 7-15 hnub ua haujlwm, thaum kev txiav txim nrog qhov ntau thiab tsawg, tshwj xeeb nto tiav, lossis loj - cov phiaj xwm loj tuaj yeem ua tiav hauv 20-30 hnub.
Kev cai 304 Stainless Hlau Tube
ASTM A213 TP304 Stainless hlau yeeb nkab specification
| Txuj | ASTM A213 / ASME SA213 |
| Qib / UNS | TP304/S30400 |
| Hom | Seamless (kub dov / txias kos) |
| Daim ntawv thov | Boiler, superheater, cua sov- cov raj xa hluav taws xob (chaw pabcuam chav) |
| Kev kho cua sov | Kev daws anneal ntawm 1040℃(1900℃F), dej los yog txias ceev |
| OD Ntau | 6.35-101.6 hli (¼ "- 4") |
| Phab ntsa Thickness | 0.89-12.7 hli (SCH 5S - XXS) |
| Ntev | 6-12 m (los yog raws li xav tau) |
Chemical Composition (wt%)
| Element | C | Si | Mn | P | S | Cr | Ni |
| TIAB SA 304 | Tsawg dua los yog sib npaug li 0.08 | Tsawg dua lossis sib npaug li 1.00 | Tsawg dua lossis sib npaug li 2.00 | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.030 | 18.0 – 20.0 | 8.0 – 11.0 |
Mechanical Properties (tom qab kho kev daws teeb meem, chav sov)
| Khoom | TIAB SA 304 |
| Tensile zog, min | 515 MPa (75 ksi) |
| Yield zog (0.2% pov thawj), min | 205 MPa (30 ksi) |
| Elongation hauv 50 mm, min | 35 % |
| Hardness, max | 192 HBW / 200 HV / 90 HRB |
Cov Lus Qhia rau Kev Pab Cuam:
Qhov siab tshaj qhov kev pabcuam kub: ~ 650℃(oxidizing cua); saum toj no, TP304H yog qhov zoo dua rau kev nkag siab dua - tawg lub zog.
Corrosion kuj: zoo heev tiv thaiv acids, alkalis, chlorides, thiab sulfates; haum rau superheated chav thiab kub - dej circuits.
Cov qauv sib npaug: EN 10216-5, DIN 17458, GOST 9941-81.
Yog tias koj xaiv tubing rau ib qhov project tshwj xeeb, qhia rau kuv paub:
• Dab tsi yog qhov kev khiav hauj lwm siab thiab qhov kub thiab txias ntawm chav dej?
• Dab tsi sab nraud (OD) thiab phab ntsa thickness yuav tsum tau?
Kev soj ntsuam zoo
Txhua lub raj steel yuav tsum tau ntxuav thiab tshuaj xyuas ua ntej ua zaub mov xa tuaj. Kev soj ntsuam zoo suav nrog kev tshuaj xyuas cov tshuaj muaj pes tsawg leeg, kev ntsuas tensile, kuaj hardness, flattening tests, flaring tests, thiab eddy tam sim no los yog hydrostatic testing kom ntseeg tau tias txhua batch ua tau raws li ASTM A213 cov qauv kev ua tau zoo.






Standard export ntim
Kev ntim khoom xa tawm yog ua haujlwm: lub kaus mom yas tiv thaiv yog haum rau ob qho kawg ntawm cov kav dej, thiab cov chaw sab nrauv yog qhwv hauv cov dej noo- cov ntaub ntawv pov thawj thiab tiv thaiv ntxiv los ntawm cov hnab ntim khoom lossis cov yeeb yaj kiab tsis zoo. Tom qab ntawd cov kav dej raug txheeb xyuas los ntawm cov lus qhia tshwj xeeb thiab ntim rau hauv cov ntoo crates lossis rau hauv cov ntoo pallets uas muaj zog dua - ruaj ntseg nrog cov hlua khi hlau qhov tsim nyog - kom txo tau qhov kev pheej hmoo ntawm kev cuam tshuam, khawb, lossis deformation thaum lub sij hawm thauj mus los. Txhua pob ntawv yog sau nrog cov lus qhia tshwj xeeb, ntau, qib khoom, thiab cov khoom siv hluav taws xob / cov khoom siv hluav taws xob kom ntseeg tau tias cov ntawv ntim khoom sib haum nrog EN 10204 3.1 cov ntaub ntawv pov thawj; ntim kuj tuaj yeem hloov kho kom tau raws li qhov yuav tsum tau ua rau lub thawv xa khoom, tawg - thauj khoom ntau, lossis cov kev xav tau tshwj xeeb.


FAQ
Dab tsi yog qhov kub siab tshaj plaws TP304 tuaj yeem tiv taus?
TP304 pom zoo oxidation tsis kam ntawm qhov kub thiab txias. Feem ntau, qhov pom zoo ntev -lub sijhawm ua haujlwm kub tsis siab tshaj 525℃(kwv yees . 977℃F). Yog tias qhov kub kub tsis tu ncua tshaj 550 degree, lub zog creep ntawm TP304 poob; Nyob rau hauv cov xwm txheej zoo li no, nws raug pom zoo kom hloov mus rau qib siab - kub xws li TP321 (stabilized nrog titanium) lossis TP316H.
Puas yog TP304 raug rau "intergranular corrosion"? Yuav zam tau qhov no li cas?
Teb: Yog, TP304 yog feem ntau cuam tshuam rau intergranular corrosion nyob rau hauv tshav kub- cuam tshuam cheeb tsam (HAZ) tom qab vuam. Txhawm rau zam qhov no:
Qhia kom meej tias cov khoom yuav tsum tau ua nruj me ntsis kev kho cua sov thaum lub sij hawm yuav khoom.
Tswj cov khoom siv hluav taws xob thaum vuam, lossis xaiv TP304L (ntxiv- cov pa roj carbon tsawg) kom txo tau qhov kev xav tau.
Xyuas kom meej tias Cov Txheej Txheem Tsim Nyog Cov Ntaub Ntawv (PQR) ua raws li cov txheej txheem vuam cuam tshuam rau cov kav dej siab.
Vim li cas nws tseem ceeb kom qhia meej "kev daws teeb meem" thaum lub sijhawm yuav khoom?
Kev daws annealing yog txheej txheem ntawm kev tshem tawm cov kev ntxhov siab uas tshwm sim los ntawm kev ua haujlwm txias. Yog tias tsis muaj kev kho kom txaus, cov kav dej tsis muaj steel hlau muaj qhov cuam tshuam rau "kev ntxhov siab corrosion cracking (SCC)" nyob rau hauv siab - qhov kub thiab txias qhov chaw, ua rau ua tsis tiav ntxov ntxov.