Lub npe: ASTM A312 Tp3 116 stainless hlau welded raj
Hom: Welded
Cov txheej txheem: tiav tiav / Argon arc vuam
Khoom siv: Stainless hlau
Nto Kho: Annealing thiab Pickling / polished
Ntu puab: Round
Ntev: Mekas Los Ntawm Cov Neeg Siv Khoom thiab Feem Ntau 6000mm
Cov Lus Qhia Tshwj Xeeb: Od 6.35 ~ 762mm
Xa kev nug
Tsham tam sim no

ASTM A312 Tp3 116 Stainless hlau welded Tube

 

ASTM A312 Tp336 yog molybdenum (mo) uas muaj Austenitic Stainless hlau Welded yeeb nkab tsim los ntawm arc vuam lossis induction vuam txheej txheem. Nws tau ua tau zoo heev corrosion tsis kam thiab muaj kev kub ntxhov siab thiab tau siv dav hauv cov kua zaub lub tshuab hauv cov chaw hnyav.

 

ASTM A312 Tp3 116 Txias Yeem Rolled Fais Welded Tubing

ASTM A312 TP316 Cold Rolled Electric Welded Tubing

Qhov Zoo Ntawm Astm A312 Tp3 116 Stainless Hlau ERw Yeeb Nkab

 

Piv nrog rau Tp304, TP316 muaj 2-3% molybdenum, uas nce nws pitting thiab crevice corrosion tiv taus los ntawm 30-50%. Nws muaj qhov zoo rau cov sulfuric acid, phosphoric acid, organic acid, thiab yog tsim nyog rau high-corrosion scenarios xws li tshuaj lom neeg thiab tshuaj.
ASTM A312 Welded Austenic steel tubing tswj hwm qhov kub thiab txias, thiab muaj cov pa hluav taws xob ruaj khov, thiab cov tshuab kub.

 

Vim li cas thiaj xaiv GNEE

Gnee muaj thawj chav kawm cov khoom siv ntau lawm thiab tuaj yeem tsim ntau hom stainless hlau muaj cov kav dej welded.
1. Cov khoom siv hauv online txhua yam, npog 14-273 caliber stainless hlau welded yeeb cov khoom lag luam.
2.
3. Nruab nrog online Weld Bead Leveling, Online ci analing thiab lwm cov yeeb nkab tsim khoom siv kom paub tseeb.

 

Hu rau tam sim no

TPP31 Welded thiab kos cov hlau stainless tubingKev qhia tshwj xeeb

Chaw ua uas tsis tau haus Cov ntsiab lus
Sab Nraum Incha (OD) 1/8 "-24" (DN6-DN600), Customizable (piv txwv li, 6.35mm-609.6mm)
Phab Ntsa Thickness SCH 5S-SCH 160, cov sijhawm uas ib txwm muaj: SCH 10s, 40s, 80s, phab ntsa tuab: 1.65mm)
Qho ntev Txheem: 6M / 12m (20ft / 40ft); Customizable ncua ntev (tsawg dua los yog sib luag rau 18m)
Kawg hom Dawb kawg, beveled kawg (37.5 Degree ± 2.5 degree), xov kawg, Tri-clamp (lub tsev kawm raug kaw)
Nto tas Muaj Qib Muaj Qib (RA tsawg dua lossis sib npaug rau 1.6μm); Kev Huv Qis (RA tsawg dua lossis sib npaug rau 0. 8μm, polishing sab hauv)

SS 316 Welded Tubes Lub Cev thiab Cov Neeg Kho Tshuab

Ntiag tug Tus nqi
Tensile lub zog (mpa) Ntau dua los yog sib npaug rau 515
Paib lub zog ({0. 2% offset, mpa) Ntau dua los yog sib npaug rau 205
Elongation (%) Ntau dua los yog sib npaug rau 30
Ntom ntom (g / cm³) 7.98
Qhov siab tshaj plaws kev pab kub Cov kev pabcuam txuas ntxiv qis dua lossis sib npaug rau 870 degree, luv-lo lus tsawg dua lossis sib npaug rau 980 degree

316 ERW Stainless Hlau Yeeb Nkab Tshuaj Muaj Zog (%)

Lub ntsiab Cov ntsiab lus ntau
Cr 16.0–18.0
Ni 10.0–14.0
Mo 2.0–3.0
C Tsawg dua los yog sib npaug rau 0. 08
Mn Tsawg dua los yog sib npaug rau 2. 0

Stainless hlau Welded Yeeb Nkab Chaw Tsim Tshuaj

 Stainless Steel Welded Pipe Manufacturer

Cov qhua tuaj noj mov

Customer Visit

Gnee koom rau hauv Nyab laj Exhibor

GNEE Participated In Vietnam Exhibition

Cim npe nrov: ASTM A312 TP316 Stainless Hlau Welded Tube, Tuam Tshoj Astm A312 Tp3Tort cov hlau welded raj manufacturers, lwm tus neeg, Hoobkas

Xa kev nug