High Pressure Stainless Hlau Seamless Pipes
Section Shape: Round
Cov Qauv Txuj Ci: ASTM A312
Khoom siv: Stainless hlau
Kev kho deg: Oiled, Polished, Txheej
Hom Lub Npe: Round, Square, Rectangular
Txheej Txheem: Kub Rolled, Cold Rolled
Thauj Pob: Hiav Txwv - Tsim nyog ntim
Specification: 6mm-2500mm (3/8 "-100")
Cov txiaj ntsig tseem ceeb ntawm High Pressure Stainless Steel Seamless Pipes
Siab -siab stainless steel seamless kav yog siab - cov kav dej ua tau zoo los ntawm kub dov los yog kos duab txias. Cov ntaub ntawv muaj xws li 304/304L, 316/316L, thiab lwm yam. Lawv tsis muaj qhov tsis xws li vuam, ultra- siab tsis kam thiab corrosion kuj. Lawv tuaj yeem tiv taus ultra{10}}siab siab ntawm 150,000 psi (sib npaug li 1034MPa), thiab cov yeeb nkab txoj kab uas hla npog 1/4 nti rau 1 nti.
Siab - cov kav hlau tsis muaj zog yog dav siv nyob rau hauv cov tshuaj, petrochemical, roj thiab roj thiab nuclear zog ua kom tau raws li qhov xav tau ntawm siab - kev thauj mus los ntawm cov dej thiab corrosion kuj.
Stockist ntawm 316 304 High Pressure Stainless Tubing

Vim li cas thiaj xaiv GNEE
GNEE yog cov chaw tsim khoom lag luam, xa tawm, thiab cov khoom lag luam siab - siab stainless hlau seamless kav, tshwj xeeb hauv seamless siab - cov kav dej siab ua los ntawm 304/316 stainless hlau. Peb muab siab -lub zog, corrosion- cov kav dej ntawm tus nqi zoo tshaj plaws, nrog rau qhov ntau thiab tsawg thiab kev ntsuas siab, ua kom muaj kev xa khoom zoo thiab txhim khu kev qha rau cov neeg siv khoom thoob ntiaj teb.
Rau Kev Kub Siab Stainless Hlau Seamless Yeeb Nkab nqe nqe, cov qauv ntsuas ntsuas siab lossis kuaj dawb, nyem lub pob hauv qab no los tham nrog peb pab neeg ua haujlwm!
Stainless hlau High Pressure Tubing Specification
Khoom siv: SS304, SS316, SS304L, SS316L
Qhov Loj: 1/4 "-1
Max siab: 19000
Hom: Raws li seamless
Ntev: 4-7 meters
Custom Length: mus txog 16 meters.
Seamless Ultra High Pressure Tubing Chemical Composition
| QIB | UNS | Si | Mn | S | C | P | Cr | Ni | Mo |
|---|---|---|---|---|---|---|---|---|---|
| TIAB SA 304 | S30400 | 1 | 2 | 0.03 | 0.08 | 0.045 | 18.0-20.0 | 8.0-11.0 | - |
| TP 304 L | S30403 | 1 | 2 | 0.03 | 0.035 | 0.045 | 18.0-20.0 | 8.0-13.0 | - |
| TIAB SA 316 | S3160 | 1 | 2 | 0.03 | 0.08 | 0.045 | 16.0-18.0 | 11.0-14.0 | 2.0-3.0 |
| TP 316 L | S31603 | 1 | 2 | 0.03 | 0.035 | 0.045 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 |
Ultra High Pressure SS Tubing Mechanical Properties
| Khoom siv | Kub | Kub | Tensile zog | Yield zog | Elongation %, Min |
|---|---|---|---|---|---|
| Kev kho mob | Min.º F (º C) | Ksi (MPa), Min. | Ksi (MPa), Min. | ||
| TIAB SA 304 | Kev daws | 1900 (1040) | 75(515) | 30(205) | 35 |
| TP 304 L | Kev daws | 1900 (1040) | 70(485) | 25(170) | 35 |
| TIAB SA 316 | Kev daws | 1900(1040) | 75(515) | 30(205) | 35 |
| TP 316 L | Kev daws | 1900(1040) | 70(485) | 25(170) | 35 |
SS 304/304L Seamless yeeb nkab Manufacturers nyob rau hauv Suav teb

Cov neeg tuaj xyuas

SS Seamless Pressure Tubing Ntim

Cim npe nrov: Tuam Tshoj siab siab stainless hlau seamless kav, Tuam Tshoj siab siab stainless hlau seamless kav manufacturers, lwm tus neeg, Hoobkas