EN 10216-5 1.4462 Duplex Stainless Hlau Seamless Yeeb Nkab
Zoo: puag ncig
Cov txheej txheem: Cold Rolled
Kev kho deg: Sanded / Daim iav / Hairline Txhuam
Thickness: 0.3-30 hli
Tawm Dav: 8-219mm
Ntev: 5.8 / 6m lossis Custom
Tshuag: hauv Tshuag
Qauv: Muaj
Thauj Pob: Txheem Hiav Txwv - Tsim nyog ntim
EN 10216-5 1.4462 Stainless Hlau Tube Supplier
TS EN 10216-5 UNS32205 seamless steel kav ua tau raws li European cov qauv thiab tau dhau los ua cov khoom nyiam nyob hauv Europe lub zog, tshuaj, thiab kev tsim vaj tsev hauv hiav txwv. Lawv cov kev tsim khoom thiab kev sim nruj me ntsis ua raws li EN / ISO system, kom ntseeg tau tias muaj kev ntseeg siab nyob rau hauv siab, corrosion, thiab kub heev. Cov khoom no yog ib tug benchmark rau EU industrial sustainability lub hom phiaj
GNEE khoom siv EN 10216-5- ua raws UNS32205 (S32205/2205) duplex stainless hlau seamless kav. Cov khoom no muaj 22% chromium, 5% npib tsib xee, 3% molybdenum, thiab 0.14-0.20% nitrogen, nrog rau nws cov microstructure stabilized los ntawm cov tshuaj annealing ntawm 1050℃-1100℃(dej quenched). Nws muab cov khoom siv tshwj xeeb thiab kev tiv thaiv corrosion, nthuav tawm zoo heev rau pitting thiab kev ntxhov siab corrosion cracking nyob rau hauv ib puag ncig uas muaj chloride (xws li dej hiav txwv thiab tshuaj lom neeg). Cov tshuaj tiv thaiv corrosion zoo no tuaj yeem hloov cov pa roj carbon steel lossis austenitic stainless hlau.
1.4462 stainless hlau kav (lwm lub npe rau UNS32205) feature lub ci ntsa iab annealed nto, siab dimensional precision (xws li, txheej kab siab kam rau ua ± 0.10mm, phab ntsa thickness kam rau ua ± 10%), thiab kev txhawb nqa rau customized ua. Lawv tau siv dav hauv cov xwm txheej hnyav xws li siab - qhov kub thiab txias, siab - cua sov hloov tshuab hauv cov roj, tshuaj, thiab kev lag luam hauv hiav txwv.

Daim ntawv thov
1. Marine thiab roj thiab roj engineering (European core applications)
2. Tshuaj thiab kws tshuaj (REACH/ROHS ua raws)
3. Zog thiab qis - carbon transformation
4. Kev tsheb ciav hlau thiab nkoj
Specification
Chemical Composition UNS S32205 Duplex Stainless Hlau Seamless Tubes
| UNS Number Qib Duplex |
Typeb | C | Mn | P | S | Si | Cr | Ni | Mo | N | Cu | Lwm yam |
| S32205 | 2205 | 0.030 | 2.00 | 0.030 | 0.020 | 1.00 | 19.5-21.5 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 | ... | |
| S32750 | 2507 | 0.030 | 1.20 | 0.035 | 0.020 | 0.80 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 | 0.50 |
Mechanical Composition UNS S32205 Duplex Stainless Hlau Tubes
| Qib | Tensile zog (MPa) min |
Yield zog 0.2% Pov thawj (MPa) min |
Elongation (% hauv 50mm) min |
Hardness | |
| Rockwell C (HR C) | Brinell (HB) | ||||
| UNS S31803/2205 | 621 | 448 | 25 | 31 max | 293 max ua |
Lub cev muaj zog ntawm UNS S32205 Stainless Hlau Seamless Tubes
| Qib | Qhov ntom (kg / m3) |
Elastic Modulus (GPa) |
Txhais tau tias Co-eff of Thermal Kev nthuav dav (μm / m / degree) |
Kub Conductivity (W / mK) |
Tshwj xeeb Kub 0-100℃(J / kg.K) |
Hluav taws xob Kev tiv thaiv (nΩ.m) |
|||
| 0-100 degree | 0-315 degree | 0-538 ° C | ntawm 100 degree | ntawm 500 degree | |||||
| UNS S31803/2205 | 782 | 190 | 13.7 | 14.2 | - | 19 | - | 418 | 850 |
EN 10216-5 Seamless Tubes yuav tsum tau tsim los ntawm sab nraud txoj kab uas hla thiab phab ntsa tuab, txoj kab uas hla thiab phab ntsa tuab ntawm cov hlab yuav tsum nyob rau hauv cov kev txwv tsis pub muaj nyob rau hauv EN ISO 1127, D1, D2, D4, thiab D4 rau sab nraud txoj kab uas hla thiab T1, T2, T3 thiab T4 rau phab ntsa thickness, nruj tolerances txog li 16 EN. TC1 thiab TC2 cov kev cai xeem tuaj yeem ntsib ntawm peb lub zeb.
Nyem Kom Tau Txais Cov Qauv Dawb
kev tshuaj xyuas
Ntau qhov kev sim tshuab yuav tsum tau ua, xws li:
Hydrostatic los yog nondestructive electric test.
Kev ntsuas nruj;
Flaring xeem (rau seamless raj);
Flange xeem (rau welded raj);
Kev ntsuas hardness;
Rov qab flattening xeem;
Intergranular corrosion test;

SS 2205 yeeb nkab cua nruj ntsuas

1.4462 Stainless hlau yeeb nkab loj ntsuas
Stainless hlau 1.4462 TubeHoobkas
Peb lub Hoobkas tsim seamless duplex stainless hlau raj uas ua tau raws li ASTM A790 UNS S32205 tus qauv. Peb tau nruab nrog cov tshuab hluav taws xob siab tshaj plaws (EAF) thiab AOD refining systems, nrog rau lub xeev - ntawm -- kos duab xuas nrig ntaus thiab cov tshuab kos duab txias, kom ntseeg tau tias qhov ntev ntev ntev, du nto, thiab cov cuab yeej zoo heev, ua raws li ASTM A790 tus qauv.


Ntim thiab Marking
Ntim: Txhua 1.4462 SS Ib puag ncig lub raj yog qhwv hauv cov dej noo- cov ntawv pov thawj, kab nrog cov yeeb yaj kiab yas, thiab ruaj nrog cov hlua hlau. Cov txheej txheej txheej yog tiv thaiv los ntawm ntoo pallet lossis crate kom muaj kev nyab xeeb thaum thauj thoob ntiaj teb.
Kev Qhia Txog Tus Kheej: Txhua pob suav nrog tus lej ntawm lub tshuab hluav taws xob, qib, qhov ntev, thiab cov ntaub ntawv txheem.