ASTM A790 UNS S32205 Seamless Duplex Stainless Hlau Tube
Zoo: puag ncig
Cov txheej txheem: Cold Rolled
Kev kho deg: Sanded / Daim iav / Hairline Txhuam
Thickness: 0.3-30 hli
Tawm Dav: 8-219mm
Ntev: 5.8 / 6m lossis Custom
Tshuag: hauv Tshuag
Qauv: Muaj
Thauj Pob: Txheem Hiav Txwv - Tsim nyog ntim
GNEE yog tus xa khoom ntawm ASTM A790 UNS S32205 yeeb nkab, muab ntau qhov ntau thiab tsawg, suav nrog iav- polished, tiaj tus, beveled, thiab threaded. Lub roundness thiab phab ntsa tuab tolerances ntawm ASTM A790 yeeb nkab ua raws li ASTM A999 cov qauv.
GNEE muab cov khoom siv siab -zoo, qhov tseeb qhov tseeb, thiab tshwj xeeb tshaj yog du A790 UNS S32205 welded thiab seamless yeeb nkab. Raws li ASTM A790 tus qauv, UNS S32205 welded thiab seamless kav ua tau raws li ANSI B36.19 tus qauv, nrog cov txheej txheem sab nraud xws li NPS 1/8 txog NPS 30, thiab phab ntsa tuab qib suav nrog Sch 5S, SCH10S, SCH40S, thiab SCH80S. Lwm qhov ntau thiab tsawg yog muaj raws li qhov kev thov.

Peb ASTM A790 Duplex Steel Tube nrog cov ntsiab lus hauv qab no Mill Test Certificate raws li EN 10204 3.1, PMI Test, Test Report los ntawm NABL Pom Zoo Lab, 3.2 Certification los ntawm External Testing Authority thib peb, ultrasonic test report, thiab X-ray report.
Nyem kom tau MTC daim ntawv pov thawj
Duplex Stainless Hlau S32205 Yeeb Nkab Specification
| Specification | ASTM A790, SAME SA790 |
| Txuj | ASTM, ASME thiab API |
| Loj | Seamless - 1/2" NB TO 18" NB Welded / ERW- 1" NB TO 16" NB EFW - 8" NB TO 110" NB |
| Hom | Seamless / Welded / ERW / EFW / Cold Draw / Kub tiav / Txias tiav |
| Ntev |
01 Meter rau 12.5 Meters, Ib Leeg Random Length, Ob Chav Random Length Thiab Customize Loj. |
| Sab nraud | 6.00 hli OD txog 914.4 hli OD, Qhov ntau thiab tsawg mus txog 24 "NB |
| Phab ntsa Thickness |
(3 hli txog 100 hli Thickness) SCH20, SCH30, SCH40, STD, SCH80, XS, TSW 60 SCH 80 SCH 120 SCH 140 SCH 160 XXS |
Chemical Composition Standard ntawm ASTM A790 Qib S32205 Yeeb Nkab
| Tshuaj muaj pes tsawg leeg | Min Tensile (KSI) | Min.Yield (KSI) |
Elongation % |
|---|---|---|---|
| C 0.30 Qhov siab tshaj plaws Cr 22 au 23 Mn 2 Qhov siab tshaj plaws 3.00 Nws 3.50 N 0.14 txog 0.20 4.50 – 6.50 Nws P 0.030 Qhov siab tshaj plaws S 0.020 max Si1.00 max |
95 | 65 | 25 |
ASTM A790 UNS S32205 Seamless Yeeb Nkab Mechanical Cwj Pwm
| Qhov ntom | Melting Point | Yield zog (0.2% Offset) | Tensile zog | Elongation |
|---|---|---|---|---|
| 7,8g 3 | 1350℃(2460℃F) | Psi - 80000, MPa - 550 | Psi - 116000, MPa - 800 | 15 % |
A790 UNS S32205 Pipe nqi
| UNS S32205 Seamless Pipes Nqe | Nqe hauv USD |
|---|---|
| Astm A790 Uns S32205 Duplex - 21.3mm Odx2.77mm Wx 6000mm | USD 227.28 |
| A-790 Uns S32205 Seamless Duplex Stainless Hlau Kav | 7290.89 Nws |
| ASTM A790 UNS S32205 2SCH 10S SMLS PIPE | USD 5564.27 |
Nyem Kom Tau Txais Cov Qauv Dawb
Duplex SS S32205 Yeeb Nkab Daim Ntawv Thov
Marine & Coastal Environments: Zoo tagnrho rau seawater tuav systems, offshore platforms, thiab desalination nroj tsuag.
Pulp & Ntawv: Siv nyob rau hauv cov ntawv tshuab, cawv tanks, thiab pulp digesters.
Khoom noj khoom haus & dej haus: Ua hauj lwm nyob rau hauv breweries thiab zaub mov ntau lawm qhov twg kub siab los yog txhoj puab heev ntxuav cov neeg ua hauj.
General Engineering: Tsim nyog rau cov khoom siv hluav taws xob sib hloov, cov raj condenser, thiab cov khoom siv tswj cov pa phem.
kev tshuaj xyuas
Peb ua 100% kev pab cuam ultrasonic (UT) thiab eddy tam sim no (ET) kuaj ntawm tag nrho cov S32205 seamless hlab. Ua raws li ASTM A790 tus qauv, peb ntsuas qhov rhiab heev rau V- theem zawj kom ntseeg tau tias lub phab ntsa ntawm lub raj tsis muaj qhov porosity, tawg, lossis delamination.


Stainless hlau 2205 TubeHoobkas
Peb kuj xyuam xim rau kev kho deg. Los ntawm kev ua tus phooj ywg zoo ib puag ncig thiab cov kab passivation lossis cov txheej txheem ci ntsa iab, ua ke nrog German - imported Ra digital deg roughness meter, peb tswj cov phab ntsa sab hauv thiab sab nrauv roughness Ra ntawm peb cov kav dej S32205 mus rau hauv 0.8μm - 1.2μm. Qhov saum npoo du no ua rau txo cov kua dej ua haujlwm thiab tiv thaiv kev ua haujlwm hauv zos pitting corrosion tshwm sim los ntawm microbial adhesion.


Ntim thiab Marking
Peb ASTM A790 Duplex Steel Tube tau ntim los xyuas kom tsis muaj kev puas tsuaj thaum caij tsheb npav. Nyob rau hauv cov ntaub ntawv ntawm export, tus txheem export packing yog nyob rau hauv ib lub thawv ntoo. Tag nrho cov ASTM A790 Duplex Steel Tube yog cim nrog peb qib, batch tooj, loj thiab cim. Peb tseem tuaj yeem ua cov khoom lag luam kev cai ntawm peb cov khoom raws li tus neeg yuav khoom qhov tshwj xeeb.

Stainless Hlau Tubes PE Fabric Bundles

Txheem export ntoo crate ntim
Cim npe nrov: Tuam Tshoj astm a790 uns s32205 seamless duplex stainless hlau raj, Tuam Tshoj astm a790 uns s32205 seamless duplex stainless hlau raj manufacturers, lwm tus neeg, Hoobkas