Teem nqi |
C |
Mn |
P |
S |
Si |
Ni |
Cr |
Mo |
N |
CU |
|
S32750 |
Tsawg dua los yog sib npaug rau 0.03 |
Tsawg dua los yog sib npaug rau 1.20 |
Tsawg dua los yog sib npaug rau 0.035 |
Tsawg dua los yog sib npaug rau 0.002 |
Tsawg dua los yog sib npaug rau 0.80 |
6.00-8.00 |
24.00-26.00 |
3.00-5.00 |
0.24-0.32 |
Tsawg dua los yog sib npaug rau 0.50 |
ASTM A789 S32750 SUPER DUPLEX Hlau Rau Hiav Txwv Dej Solutation
Puab: Round
Cov txheej txheem: Rolled txias
Nto Kho: Sanded / Daim iav / Txhuam Hniav
Thickness: 0.3-30mm
Tawm Diam: 8-219mm
Ntev: 5.8 / 6m lossis kev cai
Tshuag: Hauv Tshuag
Qauv: Muaj
Pob Thauj: Cov Hiav Txwv Txheem -} deals packing
ASTM A789 S32750 sup dupleX steel yeeb nkab rau dej hiav txwv kua txiv
Gnee yog ib qho chaw tsim khoom lag luam ntawm ASTM A789 S32750 S32750 sup duplex kav hlau. Lub 2507 super duplex cov kav hlau stainless hlau ua tiav nrog ntau yam qauv. Ob leeg seamless thiab welded unic unic unic tsis s32750 kav dej ua tau raws li A789 specification. Cov ntaub ntawv no muaj lub zog siab, nrog tsawg kawg los lub zog ntawm 80 ksi thiab tsawg kawg tensile lub zog ntawm 116 ksi. Lub ASTM A789 unic s32750 Seamless kav yog qhov tsim nyog rau cov ntawv thov uas xav tau precision tubing. Cov noob txiv ntseej no tsis tshua muaj qhov tseeb ntawm kev ntxhib, kom ua kom cov phab ntsa tsis zoo nkauj.

Tus Hlau Stainless 2507 Yeeb Nkab Tshwj Xeeb
| Qhov tuab | 0.3 hli - 50 hli, Sch10, Sch10, Sch 40, Sche, Sch XXS, SCH Xs |
| Txheej hauv lub taub | 6.00 mm od li 914.4 mm od, ntau thiab tsawg txog 24 "nb |
| Ntaus | Seamless / Erw / Welded / Fabricated / CDW |
| Puab | Puag ncig cov hlab, cov raj kab plaub, cov leeg roj, "u" duab, lauj kaub ncuav mog qab zib chev, hlab ntsha hydraulic |
| Qho ntev | Ib leeg random, ob npaug random & xav tau ntev |
| Qhov kawg | Dawb kawg, beveled kawg, tsuj las. |
UNR UNS UNR UNR TSIS TXAUS SIAB S32750 SAF {{1} f} f}}}} cr25ni7mo4n Tshuaj Muaj Tshuaj (%)
Cov Khoom Siv Neeg Kho Tshuab Ntawm Super Duplex Uns S32750 Kev Siv Tub
| Melting ntau yam (degree) | 1350 |
| Melting ntau yam (Qib F) | 2460 |
| Tsis yog | S32750 |
| Ntom ntom (G / Centimeter 3) | 7.8 |
| Ntom ntom (lb / nti 3) | 0.281 |
ATM A789 UNSENT S32750 RAJ NQE
| Daim Ntawv Teev Nqi | Nqe hauv USD |
|---|---|
| Sa789 unc unic s32750 raj loj me: 12.70x0.65 | US $ 22.30 |
| ASTM A789 Unict S32750 Raj Loj: 6.35X2040.25 | US $ 1.25 |
Nyem kom tau txais cov qauv dawb
kev kuaj xyuas
Flange thiab flare tshuaj ntsuam, rov qab ntsuas qhov ntsuas, hydrostatic / eddy kev kuaj, dos ua tiav kev kuaj xyuas, kev tshuaj ntsuam tas nrho, khoom pov thawj


Stainless hlau 2507 rajTsev tsim khoom


Ntim thiab kos cim
Ntim yuav tsum nyob rau hauv bundles lossis laminated ntoo crates, qhwv hauv cov yas, thiab tsim nyog tiv thaiv kev tiv thaiv kom ntseeg tau tias seaworthiness rau kev thauj lossis raws li qhov xav tau.
Kev cim yuav tsum ua raws li cov kev cai ntawm A1016 / A1016M cov lus qhia tshwj xeeb thiab yuav tsum suav nrog seb puas tau ua haujlwm lossis tus lej loj, thiab cov lej pob.


Cim npe nrov: ASTM A789 S32750 SUPER DUPLEX RAU LUB Hiav Txwv Dej Solutation, Tuam Tshoj ASTM A72750 Super Duplex Rau Hiav Txwv Dej Solutioners, Chaw muag khoom, Hoobkas