ASTM A376 TPP36N Stainless Hlau Kub Txheej Txheej

ASTM A376 TPP36N Stainless Hlau Kub Txheej Txheej

Lub npe: ASTM A376 Tp316N stainless hlau stainless hlau xovxwm tiav lawm cov yeeb nkab
Ntawv pov thawj: ISO, ROHS, IRHS, AISI, AISI, ASTM, GB, En, Din, JIS
Puab: Round
Cov txheej txheem: Rolled txias
Nto Kho: Sanded / Daim iav / Txhuam Hniav
Thickness: 0.3-30mm
Tawm Diam: 8-219mm
Ntev: 5.8 / 6m lossis kev cai
Tshuag: Hauv Tshuag
Qauv: Muaj
Pob Thauj: Cov Hiav Txwv Txheem -} deals packing
Xa kev nug
Tsham tam sim no

Yeeb nkab hauv Tp3E16N, TPP36N KUB KUB TEEBTus xa tawm

 

Nrhiav rau corrosion -} awnant ausustenitic stainless hlau kav rau high}} kub, thiab corrosive ib puag ncig? ASTM A376 TP316N kub -} tiav kav dej yog qhov kev daws teeb meem zoo tagnrho.

Gnee yog ib lub chaw tsim khoom lag luam thoob ntiaj teb thiab cov khoom siv ntawm Hwm Hwm Stainless hlau. Peb muab lub Tp316N kub- ua tiav cov kav hlau ua tiav uas ua tiav nrog Astm A376 / ASME SA376 tus qauv. Cov kav dej no tau tsim tshwj xeeb rau cov khoom siv hnyav xws li cov tshuaj lom neeg ua noj, roj av, thiab dej hiav txwv {6} Kev lag luam siab. TPP316N yog qhov tsim nyog rau cov kev pabcuam uas muaj feem cuam tshuam nrog chlorides, sulfides, thiab huab cua sov heev.

 

TP316N Hot Finished Pipe

Hu rau tam sim no

Qhov Zoo

 

GNee cov khoom siv siab - Zoo }3} Zoo AVTM A376 Tp3Emal Stainless Hlau Kav Dej XEEM. Muaj nrog cov diameters sab nraud mus txog 610 hli thiab phab ntsa thicknesses txog li 30mm, cov kav dej no tuaj yeem yog kev cai nyob rau hauv ntev txog 12 meters. Qhov kev txhawb nqa no tau txais txiaj ntsig zoo hauv qhov loj - teev muaj kev siv vuam, thiab txo qis kev pheej hmoo. All pipes are 100% tested, including hydrostatic and eddy current inspections, and are supplied with EN 10204 3.1 material certificates and third-party inspection reports.

 

Ib qho ntxiv, Tp316N kub - Cov khoom lag luam tiav lawm, ua rau lawv muaj kev cia siab rau cov kev ntseeg tau zoo tshaj plaws hauv qab cov chaw xav tau.

 

Tp316N Yeeb Nkab Hauv Tshuag

17
TPP316N Stainless Hlau Kub Ua Tas
28
Tp316N Khaub Ncaws
A376 TP316N seamless pipe
A376 TP316N Seamamless Yeeb Nkab
 

316N Stainless Hlau Yeeb Nkab Nqe

316N cov yeeb nkab stainless hlau nqe yog nyob ntawm cov ntaub ntawv nyoos, cov kev xav tau {{{1} Hu rau peb tam sim no rau cov lus qhia raug thiab kev sib tw!

Hu rau tam sim no

kev qhia tshwj xeeb

Kev qhia tshwj xeeb

ASTM A-376 & ASTM / ASME SA376

Cov menyuam kawm qib

316,316h, 316N, 316LN,

Ntaus

Tsis ntse

Txheej ntawm txoj taub loj

6mm-630mm.

Phab Ntsa Thickness

1 hli-30mm.5s, 10s, 40s, 80s

Qho ntev

4-13m, 5.8m, 6m lossis raws li cov neeg thov kev thov.

Kev thev

Ntsib tus qauv.

Nplaim

Pickled & annealed.

SS 316N Seamam Yeeb Nkab Tshuaj Muaj Zog

Lub ntsiab Cov ntsiab lus (%)
Chromium, cr 16.0-18.0
Npib tsib xee, ni 10.0-14.0
Molybdenum, mo 2.0-3.0
Manganese, mn 2.00
Silicon, si 1.00
Nitrogen, n 0.10-0.30
Phosphorous, p 0.045
Carbon, c 0.03
Sulphur, s 0.03

TPP316N Stainless Hlau Seamless Yeeb Nkab Yeeb Nkab

Cov Khoom Siv Me me Muaj huab tais
Lub zog tensile 515 MPa 74694 psi
Paib lub zog 205 MPa 29732 psi
Modulus ntawm elasticity 190-210 GPA 27557-30457 Ksi
Poisson tus piv 0.27-0.30 0.27-0.30
Elongation thaum so (hauv 50 hli) 60% 60%

kev kuaj xyuas

ASTM A376 TP316N pipe
TP316N hot finished pipe

Chaw Tsim Tshuaj Tp3 116N Seamerless Cov Chaw Tsim Tshuaj

A376 TP316N seamless pipe
TP316N stainless steel pipe