Lub Npe: ASTM A312 TP316L Seamless Muaj Steel Yeeb Nkab
Nto Kho: Pickling tiav, No.1, 2b, Polish, Sandblasting
Ntu puab: Round
Cov Khoom Muag Khoom: Stainless Hlau Seamless / Welded Yeeb Nkab
Sab nraud ntawm lub cheeb: 3.18-800mm
Kam rau: Raws li ASTM A312
Pob Thauj: Nrog lub hau yas rau ob qho kawg, ntim rau hauv pob
Xa kev nug
Tsham tam sim no

Cov Ntsiab Lus Zoo ntawm Astm A312 Tp336L Seamless Muaj Steel Yeeb Nkab

 

ASTM A312 TP316L Seamless Muaj Cov Khoom Siv Steel Yeeb Nkab, Muaj Zog Zoo Tshaj Plaws, Thiab Tsis Muaj Weld Tsis Txaus Siab.
Cov yeeb nkab tsis kam ntawm Astm A312L Stp3E steel hlau yeeb yog 50% siab dua li ntawm 304 stainless hlau
ASTM A312 TP316L Stainless Hlau Seamless Yeeb Txom Nyem yog 40% ntau dua li ntawm welded cov ntsiab lus saum 100mpa, xws li cov kev xav tau ntawm roj drilling risers.

 

ASTM A312 TPP36L Seamless Hlau Yeeb Nkab

ASTM A312 TP316L Seamless Steel Pipe
ASTM A312 TP316L Seamless Stainless Steel Pipe

Vim li cas xaiv GNEE

Raws li ib tug kws tshaj lij kev ua haujlwm, GNEE muaj kaum ob 8 {}}}}}}}}}}}}}} support្ support cold Cong lim, annealing pickling, annealing, thiab khoom siv tsis siv neeg. Cov ntau lawm cov txheej txheem tam sim tam sim no cov txheej txheem kev taug qab los ua kom muaj txiaj ntsig zoo ua haujlwm thiab ua tau zoo. Muaj peev xwm ntau lawm yog li 20,000 tons. Peb muab kev sib tham tag nrho cov kev hloov kho thiab kev coj zoo, txhawb nqa seamless / Welded Yeeb Nkab Xaiv kev sib tham, thiab ua tau raws li txoj kev sib tham nrog nruj xav tau.
Rau ATTM A312 TP316L txias kos cov yeeb nkab cov nqi, kev kuaj mob ceev, thov nias lub pob hauv qab no kom hu rau peb pab neeg sib txuas lus!

 

Hu rau tam sim no

ASTM A312 TPORYLE STENY HLAU HOM ​​TSHWJ XEEB

Tshuaj lom neeg theem ntawm SS 316L Seamless Tube

Teem nqi 316L
lub min tus zuag
C 0.08
Mn 2.0
Si 0.75
P 0.045
S 0.03
Cr 16.0 18.0
Mo 2.0 3.0
Ni 10.0 14.0
N 0.10

Cov Khoom Siv Neeg Kho Tshuab Ntawm Ss Untren S31600 Hloov Yeeb

Teem nqi 316
Tensile lub zog (mpa) min 515
Yield zog 0.2% pov thawj (MPA) min 205
Elongation (% hauv 50 hli) min 40
Kev nyuaj Rockwell B (HR B) Max 95
Rockwell B (HR B) Max 217

Kev noog

ATTM A312 TPORCE SCHPENCE Kos Seamless kavTus xa khoom

 ASTM A312 TP316L Cold Draw Seamless Pipes  Supplier

Cov qhua tuaj noj mov

Customer Visit

Stainless hlau 316L Txias Rolling Tube Nrhiav Kom Tau

Stainless Steel 316L cold Rolling Tube Detection

Cim npe nrov: ASTM A312 TP316L Seamless Muaj Cov Hlau Yeeb Nkab, Tuam Tshoj ASTM A312L Seamless Muaj Cov Hlau Yeeb Nkab Chaw Tsim Tshuaj, Chaw muag khoom, Hoobkas

Xa kev nug