ASTM A312 TP316L Stainless Hlau Yeeb Nkab rau Marine Daim Ntawv Thov
Hom: Seamless los yog Welded
Yeeb Nkab Hom: Round, Square, Rectangular
Stainless hlau yeeb nkab: 317L
Txheej Txheem: Kub Rolled / Cold Rolled / Cold Drawn
Nto tiav: 2b, 2D, Ba, No.1, No.4, No.8, 8K, Daim iav
Thauj Pob: Txheem Hiav Txwv - Tsim nyog ntim
TP316L stainless hlau yeeb nkab tsum
GNEE, ua tus kws tshaj lij stainless hlau xa khoom, muabASTM A312 TP316L stainless hlau kav (UNS S31603)tsim tshwj xeeb rau kev siv marine. Txhua batch ntawm cov kav dej yog muab nrog ib tugEN 10204 3.1 cov ntaub ntawv pov thawj, thiab DNV, ABS, GL thiab lwm cov ntawv pov thawj hauv zej zog muaj peev xwm muab tau, kom ntseeg tau ntev - kev pabcuam nyab xeeb nyob rau hauv ib puag ncig marine hnyav.
EN 10204 3.1 ntawv pov thawj yeeb nkab

ASTM A312 TP316L stainless hlau yeeb nkab, nrog rau qhov sib ntxiv ntawm 2% -3% molybdenum (Mo), muaj tus nqi PREN Ntau dua lossis sib npaug rau 24, txhim kho nws txoj kev tiv thaiv pitting thiab crevice corrosion. Nws lub neej kev pab cuam yog ntau tshaj ob zaug ntawm 304 stainless hlau, ua rau nws txhim khu kev qha kev daws teeb meem rau kev thauj cov dej hauv marine systems, desalination nroj tsuag, offshore platforms, thiab cov chaw ntug hiav txwv dej.
Peb kuj muab ASTM A312 TP316 welded thiab seamless kav, npog tag nrho txoj kab uas hla ntawm 1/2 "mus rau 24", nrog phab ntsa thickness qib ntawm SCH 5S mus rau SCH 80S. AOD / VOD refining kom huv si ntawm cov khoom. Cov yeeb nkab welded tau txais kev kho mob hauv online (dej quenching ntawm 1050-1100 degree) kom tshem tawm kev ntxhov siab thiab ua tiav cov qauv zoo ib yam. Nws tuaj yeem tswj xyuas corrosion tsis muaj kev kho cua sov tom qab vuam. Lub zog tawm los yog ntau dua los yog sib npaug rau 170MPa thiab lub zog tensile ntau dua los yog sib npaug rau 485MPa, ua tau raws li qhov xav tau ntawm lub siab thiab cuam tshuam cov kev xav tau ntawm cov kav dej hauv nkoj thiab marine engineering.


316/316L Stainless Hlau Daim Ntawv Thov:
Kev siv tshuaj, khoom siv
Laboratory benches thiab khoom siv
Rubber, plastics, pulp & ntawv machinery
Cov cuab yeej tswj cov pa phem
Nkoj fittings, tus nqi, thiab twj tso kua mis trim
Thaum tshav kub kub exchangers
Pharmaceutical thiab textile kev lag luam
Condensers, evaporators, thiab tanks
A312 TP316 steel raj specification
| Specifications | ASTM A / ASME A312 |
| Dimension | ASTM, ASME |
| Teem caij | TSW 10 SCH 20 SCH 30 SCH 40 STD SCH 60 SCH 80 SCH 120 SCH 140 SCH 160 XXS |
| Phab ntsa Thickness | Teem caij 5S - Teem caij XXS. |
| Loj - Seamless 304 Pipes & Tubes | 1/2″ NB - 16″ NB |
| ERW 304 Pipes & Tubes | 1/2″ NB - 24″ NB |
| EFW 304 Pipes & Tubes | 6″ NB - 100″ NB |
| Daim ntawv | Round, Square, Rectangular, Hydraulic thiab lwm yam |
| Ntev | Ib qho Random, Ob Chav Random & Txiav Ntev. |
| Hom | Seamless / ERW / Welded / Fabricated / LSAW Pipes |
| Xaus | Plain End, Beveled kawg, Threaded |
Tshuaj muaj pes tsawg leeg
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316L | Min | - | - | - | - | - | 16.0 | 2.00 | 10.0 | - |
| Max | 0.03 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 |
Lub cev muaj zog ntawm ASTM A312 TP 316 / 316L Seamless Pipes
| Qib | Qhov ntom (kg / m3) |
Elastic Modulus (GPa) |
Txhais tau tias Co-eff ntawm Thermal Expansion (m/m/0C) | Thermal conductivity (W/m.K) |
Cov cua kub tshwj xeeb 0-1000C (J/kg.K) |
Elec Resistivity (nΩ.m) |
|||
| 0-1000C | 0-3150C | 0-5380C | Thaum 1000C | Ntawm 5000C | |||||
| 316/L/H | 8000 | 193 | 15.9 | 16.2 | 17.5 | 16.3 | 21.5 | 500 | 740 |
Mechanical Properties
| Tensile Requirements | TIAB SA 316 | TP 316 L |
|---|---|---|
| Tensile zog min. MPa [ksi] |
515 [75] |
485 [70] |
| Yield zog min. MPa [ksi] |
205 [30] |
170 [25] |
| Elongation hauv 2", min, % (*L) |
35 | 35 |
| Elongation hauv 2", min, %(*T) |
25 | 25 |
TP316L puas yuav muaj kev ntxhov siab corrosion tawg (SCC) hauv ib puag ncig marine?
Yog lawm. Austenitic stainless hlau (xws li 316L) kuj tseem ceeb rau SCC nyob rau hauv ib puag ncig chloride, tshwj xeeb tshaj yog thaum muaj ob qho xwm txheej hauv qab no:
Qhov kub siab: Feem ntau siab dua 60℃(140℃F).
Kev muaj kev ntxhov siab tensile: suav nrog kev ua haujlwm seem lossis kev ntxhov siab ua haujlwm.
ASTM A312 TP316L yeeb nkab stockist tsum
Spot Stock: GNEE tuav cov khoom lag luam loj, npaj tau los npog ntau qhov ntau thiab tsawg (los ntawm 1/8 "mus rau 24" NPS) thiab phab ntsa thicknesses (Sch 5S, 10S, 40S, 80S, thiab lwm yam).
Customization: Rau cov kab tshwj xeeb, ntxiv - phab ntsa tuab, lossis ntev ntev, GNEE muab sijhawm luv luv ua tsaug rau nws txoj kev koom tes sib sib zog nqus nrog cov tuam txhab loj.
End Finishing: Beveled xaus los yog lub tiaj kawg tuaj yeem ua tau yooj yim rau ntawm - qhov chaw vuam.


AISI 316 SS Pipes Kev Tshawb Fawb
Txhua lub raj yuav tsum raug kuaj xyuas hluav taws xob tsis muaj kev puas tsuaj lossis kev sim hydrostatic, Chaw tsim khoom siv ntawv pov thawj raws li EN 10204 3.1 yuav tsum tau muab.
Tensile khoom, Elogation
Kev kuaj Hardness, Brinell, Rockwell, Vickers hardness
Kev ntsuam xyuas flattening
Flaring xeem
Hydrostatic los yog Nondestructive test
Intergranular Corrosion Test - ASTM A262/E (xaiv)

High - ntim zoo
A312 TP316L seamless steel kav yog ib tus zuj zus ntim rau hauv hnab yas, txhua cov yeeb nkab yog qhwv hauv cov khoom siv dej tsis zoo thiab ruaj nrog nylon hlua. Cov ntawv ntshiab yog affixed rau sab nraud ntawm lub ntim kom yooj yim txheeb xyuas qhov ntau thiab cov khoom naj npawb. Kev tiv thaiv nruj yog coj thaum tuav thiab kev thauj mus los.
Kev ntim khoom ntawm A312 seamless steel kav yuav ua raws li cov qauv thoob ntiaj teb, ruaj ntseg nrog cov hlua khi ua ntej muab ntim rau hauv cov thawv kom tsis txhob muaj kev puas tsuaj. Lub sij hawm xa tuaj: 10-25 hnub; yog tias muaj Tshuag txaus, kev xa khoom tuaj yeem ua sai li sai tau.

Cim npe nrov: ASTM A312 TP316L Stainless hlau yeeb nkab rau Marine Daim ntawv thov, Tuam Tshoj ASTM A312 TP316L Stainless hlau yeeb nkab rau Marine daim ntawv thov manufacturers, lwm tus neeg, Hoobkas