Dab tsi yog AISI 416 Stainless Hlau Round Bar?

Oct 27, 2025

Tso lus

​Dab tsi yog AISI 416 Stainless Hlau Round Bar?​

AISI 416 yog martensitic stainless hlau paub rau nws zoo heev machinity thiab zoo tsis kam rau ib puag ncig corrosive me me. Nws yog dav siv hauv cov ntawv thov xws li cov tshuab nqus dej, cov tshuab nqus tsev, zog, bolts uas yuav tsum muaj qhov ua kom haum corrosion thiab siab dua.

 

Yog tias koj tab tom nrhiav rau AISI 416 stainless hlau round bars rau machining seem, lossis cov khoom siv ua kom muaj zog thiab cov khoom siv zoo uas ntseeg tau los xaiv. Txhua 416 SS puag ncig bar peb muab yog tsim los ntawm high}}}}}}}}}}}}}}}} oxgenen / hydrogen impurity kuaj.

SS 416 puag ncig cov pob khoom muaj nyob hauv kev muag khoom muag muag (hardness tsawg dua lossis sib npaug thiab muaj zog tshaj plaws (hardness 220-260hbw, hardile lub zog ntau dua los yog sib npaug zos). Cov xim ua tiav suav nrog cov oxide dub (kub}}}}}} polled), muab (du) Txhua pob yog kuaj rau qhov tseeb raug (± 0.000 0.02 hli- {{{{{{{{} 9 {{{} 9001 Daim Ntawv Pov Thawj Cov Ntawv Pov Thawj.

AISI 416 Stainless Steel Round Bar

AISI 416 Stainless Hlau Round BarKev qhia tshwj xeeb

Hom Kev qhia tshwj xeeb
Lub hom phiaj ASTM A582 / A276 / A484 / EN 10088-3
Teem nqi AISI 416 / EN 1.4005 / SUS416
Puab Round Bar, Hex Bar, Xwmfab Bar, Forged Bar
Yam tseem ceeb Annealed, tawv, tempered
Cov kab uas hla 6 hli - 500 hli
Qho ntev 1000 mm - 6000 mm lossis kev cai txiav
Nto tas Dub, ci, polished, tev
Kev Kho Cua Sov Quenched thiab tempered (Q & T)
Luam Machinyar 110% (piv rau free-} Txiav cov hlau)

 

Kev siv tshuaj lom neeg muaj pes tsawg leeg ntawm AISI 416 stainless hlau bar

Lub ntsiab Cov ntsiab lus (%)
Carbon (c) Tsawg dua los yog sib npaug rau 0.15
Chromium (cr) 12.0 – 14.0
Manganese (mn) Tsawg dua los yog sib npaug rau 1.25
Silicon (si) Tsawg dua los yog sib npaug rau 1.00
Phosphorus (p) Tsawg dua los yog sib npaug rau 0.04
Sulphur (s) 0.15 – 0.35
Hlau (FE) Seem

 

Cov Khoom Siv Neeg Kho Tshuab (Anealed Mob)

Ntiag tug Cov nqi raug
Lub zog tensile 620 mpa - 760 MPa
Yield zog (0.2% pov thawj) 275 mpa
Elongation 18%
Hardness (Brinell) Tsawg dua los yog sib npaug rau 217 hb
Ceev 7.75 g / cm³
Hlau Yog (sib nqus hauv txhua qhov xwm txheej)

 

Yog 416 stainless hlau corrosion - tiv taus?
Yog lawm, 416 muaj kev tiv thaiv corrosion tsis kam, tab sis nws tsis tshua tiv taus cov qib qis xws li 304 lossis 316 vim nws cov lus faj Sulfur. Nws ua tau zoo tshaj plaws nyob rau hauv cov chaw qhuav lossis qhov twg cov siavants siv.

 

Muaj peev xwm 416 stainless hlau yuav welded?
Vuam yog qhov ua tau tab sis tsis pom zoo vim muaj kev pheej hmoo ntawm kev tawg. Preheating (200-300 degree) thiab tshaj tawm - Weld annealing yog qhov yuav tsum tau ua rau cov txiaj ntsig zoo.

 

Dab tsi yog lub hardness ntawm 416 stainless hlau tom qab kev kho cua sov?
Tom qab ua kom tawv nqaij tawv thiab tempering, nws tuaj yeem ncav cuag HRC 40-45, muab cov siab coj kev tiv taus.

 

Dab tsi yog qhov sib txawv ntawm 410 thiab 416 stainless hlau?
Lub ntsiab txawv yog Sulphur cov ntsiab lus - 416 muaj ntau dua cov txiv sulfur, uas tau txhim kho cov tshuab xaim hluav taws xob tab sis me ntsis qis dua corrosion.

 

416 stainless hlau tsis muaj polished?
Yog, 416 tuaj yeem ua polished rau qhov kaj ci, tshwj xeeb tshaj yog nyob rau hauv daim ntawv thov bar thiab ncej.

 

416 Stainless Hlau Hloov Bar Nqe Rau Ib KG

Khoom Yam Qhov loj loj (hli) Kwv yees li. Nqe (USD / KG) Hais lus
AISI 416 Stainless Hlau Round Bar 6 - HLI 50 hli $2.80 – $3.50 Kaj / annealed
AISI 416 Forged Bar 60 - 200 hli $3.50 – $4.20 Quenched & tempered
AISI 416 polished round bar Kab lig kev cai Ntawm kev thov Precision Machined

Cov nqi ua lag luam sib txawv, cov lus faj sulfur, thiab cov nqi machining. Kev yuav ncaj qha los ntawm cov ntawv pov thawj lossis cov neeg muag khoom uas ntseeg tau zoo li GNEE ua kom zoo ib yam thiab ruaj khov.sales@gneestainless.com

Ntim: ntoo crates, yas ntim, anti - xeb roj txheej
Lub sij hawm xa tuaj: 7-15 hnub tom qab kev txiav txim kev pom zoo

 416 stainless steel round bar

 

Xa kev nug