Puas yog koj tab tom nrhiav rau cov ntawv zoo stainless hlau nrog zoo corrosion kuj?Yog tias koj qhov project xav tau siab -zoo SUS316 stainless hlau ntawv ci, peb cov ntawv 316 annealed nrog 2B nto tiav yog qhov kev xaiv zoo tshaj plaws. Tsim los rau kev ua haujlwm ntev, kev ua tau zoo, thiab kev ua haujlwm ntev -, nws zoo meej rau kev siv tshuaj lom neeg, hluav taws xob, aerospace, thiab zaub mov kev lag luam.
Dab tsi yog SUS316 stainless hlau annealed ntawv ci?
SUS316 stainless hlau ntawv ci yog austenitic corrosion-resistant alloy dav lees paub rau nws cov kev ua tau zoo nyob rau hauv ib puag ncig hnyav. SUS316 annealed foil yog hais txog cov ntaub ntawv hloov tau yooj yim uas tau ua tiav kev kho kom zoo, ua kom yooj yim txiav, khoov, thiab daim ntawv. Nrog rau 2B nto tiav, nws muaj qhov du, matte nto thiab yog siv dav hauv kev lag luam thiab cov ntawv kho kom zoo nkauj.

Dab tsi yog qhov txawv ntawm 316 foil thiab 316L ntawv ci?
316L muaj cov ntsiab lus qis dua, ua rau nws zoo dua rau cov ntawv thov welded kom txo tau qhov kev sib txhuam ntawm intergranular. Peb cov ntawv SUS316 yog qhov zoo tagnrho rau feem ntau cov hom phiaj fabrication.
SUS316 stainless hlau annealed ntawv ci Specifications
| Yam khoom | Specification |
|---|---|
| Khoom siv | SUS316 (1.4401 / 316) |
| Nto tiav | 2B (txias- dov, du) |
| Thickness | 0.02 hli - 1.0mm (Customizable) |
| Dav | 10mm-1000mm (customizable) |
| Daim ntawv | Coil / Ntawv |
| Txuj | ASTM A240, JIS G4304, EN 10088 |
Dab tsi kev lag luam feem ntau siv 316 annealed ntawv ci?
Chemical & Petrochemical: Siv rau corrosion{0}}cov ntaub ntawv tiv taus, diaphragms, thiab hauv cov cuab yeej siv tshuaj hnyav.
Kev Kho Mob & Pharmaceutical: Siv rau hauv cov cuab yeej phais, cov cuab yeej kho mob, cov khoom cog (stents, pacemakers), thiab cov khoom siv tshuaj.
Electronics & Hluav Taws Xob: Ua haujlwm ua cov ntaub thaiv npog, hauv cov khoom siv roj teeb, rau cov khoom sib txuas, hauv Circuit Court boards, thiab tsim cov khoom siv hluav taws xob.
Aerospace & Automotive: Siv los tiv thaiv tshav kub, tso pa tawm, thiab gaskets vim nws qhov siab - qhov kub thiab txias zog.
Khoom noj khoom haus & Dej haus: Siv rau kev tu cev, tsis yog -reactive processing, wrapping, and storage equipment.

SUS316 Stainless hlau ntawv nyiaj Supplier
Peb muab tag nrho - specification SUS316 stainless hlau ntawv ua raws li JIS/ASTM/GB cov qauv, nrog thicknesses xws li 0.01-0.5mm thiab dav ntawm 5-600mm. Peb txhawb kev txiav txim rau txias-kuav los tiag tawv (H) thiab mos (2B / BA) tej yam kev mob, thiab tseem tuaj yeem muab cov nqi ntxiv xws li slitting, zaj duab xis txheej, thiab qib raws li xav tau. Cov qauv dawb muaj rau kev sim.


Lub thickness kam rau ua ntawm peb SUS316 stainless hlau ntawv yog precisely tswj rau ± 0.001mm, nrog ib tug BA daim iav nto roughness ntawm Ra tsawg dua los yog sib npaug rau 0.2μm. Cov ntawv ci saum npoo yog dawb ntawm khawb thiab pinholes, thiab lub tiaj tus siab siab yog tsawg dua lossis sib npaug li 0.1mm / m. Cov ntaub ntawv nyoos tau dhau 100% spectral muaj pes tsawg leeg kuaj, thiab cov khoom tiav raug kuaj xyuas tag nrho rau saum npoo thiab qhov ntev yob los ntawm yob. Txhua pawg los nrog EN 10204 3.1 MTC cov ntaub ntawv pov thawj thiab ua raws li RoHS/REACH ib puag ncig cov qauv. Cov qauv tshwj xeeb tau xa tuaj sai sai hauv 3-5 hnub, thiab kev cai slitting qhov ntau thiab tsawg tuaj yeem ua tiav hauv 1-3 hnub ua haujlwm.


Xa kev nug