Ss 304 3 mm ntawv hauv stcok

Oct 15, 2025

Tso lus

Gnee muab siab - zoo ss {{1 hli mm mm stainless hlau ntawv. Precision -}} Kuv puas kam ua rau tus qauv txuas thoob ntiaj teb xws li ASTM A240 thiab ANTM A480. Nws yog dav siv nyob rau hauv kev lag luam khoom siv, cov khoom siv ua haujlwm, kev tsim kho, thiab ua yeeb yam.


Cov Nta Tseem Ceeb:
Cov khoom siv: AISI 304 / EN 1.4301 Ausenitic Stainless hlau
Thickness: 3mm (hauv Tshuag thiab muaj nyob rau cov zaub mov xa tuaj sai)
Deg tas: 2B, BA, tsis muaj . 1, lossis kev cai ua tiav
Cov Kev Siv: Khoom Noj Khoom Haus thiab Dej Panels, Cov Khoom Siv Hniav Ua Hniav, Tso Tsheb Hlau Luam Yeeb Tshuaj

 

Tsis ntev los no tus nqi hloov kho (q 4 2025)

Raws li ntawm q 4 2025, SS 304 tus nqi tau pom muaj nce ntawm 3-5% vim muaj npib tsib xee thiab chromium nqi hauv kev ua lag luam thoob ntiaj teb. Txawm li cas los xij, Gnee Stainless Hlau muaj tus nqi txuas ntxiv thiab ntev}-}}}}}} kev xaiv ua ntawv cog lus los pab txo qis cov nqi hloov pauv.

Ss 304 3 mm daim ntawv nqe rau kg (Lub kaum hli ntuj 2025 hloov tshiab)

Ntawv luaj li cas Nqe (USD / KG) Kwv yees tus nqi ib daim ntawv
1000mm × 2000mm $3.00 – $3.50 $180 – $210
1250mm × 2500 hli $3.10 – $3.60 $230 – $270
1500 hli × 3000mm $3.20 – $3.70 $310 – $350

Nco tseg: Cov nqi yog qhov taw qhia thiab yuav sib txawv raws li kev ua lag luam hloov pauv thiab cov khoom siv RAW. Rau kev txiav txim siab ntau, ntev-} cov lus cog lus, lossis cov cim kev cai, tiv tauj peb rau cov nqi sib tw.EMAIL:sales@gneestainless.com

 

Tshuaj lom neeg tshuaj lom neeg (SS 304)

Lub ntsiab Cov ntsiab lus (%)
Chromium (cr) 18 – 20
Npib tsib caug (ni) 8 – 10.5
Carbon (c) Tsawg dua los yog sib npaug rau 0.08
Manganese (mn) Tsawg dua los yog sib npaug rau 2
Silicon (si) Tsawg dua los yog sib npaug rau 1
Phosphorus (p) Tsawg dua los yog sib npaug rau 0.045
Sulphur (s) Tsawg dua los yog sib npaug rau 0.03
Hlau (FE) Seem

 

Cov Khoom Siv Neeg Kho Tshuab

Ntiag tug Tus nqi
Ceev 8.0 g / cm³
Lub zog tensile 520 - 750 MPa
Paib lub zog Ntau dua los yog sib npaug rau 205 MPa
Elongation Ntau dua los yog sib npaug rau 40%
Kev nyuaj HRB 70 - 90
Kev khiav hauj lwm siab 870 degree
Sib Nqus Cov Khoom Tsis - sib nqus
Nto tas 2b / ba / No.1 / polished

 

Yog SS 304 daim ntawv sib nqus?
Tsis tau, 304 yog Austenic thiab feem ntau tsis yog-}} sib nqus, tseem yuav qhia me ntsis Magnetism tom qab ua haujlwm txias.

 

Muaj peev xwm ss 304 3 hli nplooj ntawv yuav welded?
Yog lawm, lawv tuaj yeem welded siv tige, Mig, lossis chaw vuam tsis muaj kev cuam tshuam corrosion.

 

Dab tsi cov chaw ib puag ncig yog tsim nyog rau SS 304 daim ntawv?
Tshuaj me me, sab hauv tsev, ua si, ua zaub mov, thiab ib puag ncig muaj kev lag luam. Zam kev ua kom muaj cov acids zoo heev tshwj tsis yog coated lossis passivated.

 

Kev Tiv Thaiv:
1. Daim ntawv Liner muaj.
2. PVC Cov yeeb yaj kiab tiv thaiv muaj.
Nqi: FOB, CIF, DDU, FCA, Exw, thiab lwm yam.
Hom tau zoo: Peb muaj kwv yees li 20,000 tons hauv Tshuag.
Cov ntawv pov thawj: ISO 9001, SGS, ABS, BV
Stainless hlau ntawv ntau thiab tsawg thiab thicknesses tuaj yeem kho tau. Thov hu rau peb kom paub ntau ntxiv.
Txhua cov khoom lag luam tsis suav cov ntawv liner lossis PVC tiv thaiv zaj duab xis. Thov qhia rau peb paub yog tias koj xav tau lawv.

SS 304 3mm stainless steel sheet
304 3mm stainless steel sheet
 

Xa kev nug