Ansi \/ ASME B36.10M, B36.19M Thickness Cov Ntaub Ntawv Cov Ntaub Ntawv
May 12, 2025
Tso lus
Ansi \/ ASME B36.10M, B36.19M Thickness Cov Ntaub Ntawv Cov Ntaub Ntawv
| Nominal loj (nti) | Sch5s | SCH10S | tus sch10 | Sch20 | Sch30 | Sch40s | Std | Sch40 | tus sch60 | Sch80s | Xs | Sche0 | Sch100 | tus sch120 | Sch140 | Sch160 | Xxs | Sch160s |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1/8 | 10.29 | - | 1.24 | - | - | 1.73 | 1.73 | 1.73 | 2.41 | 2.41 | 2.41 | - | - | - | - | - | - | - |
| 1/4 | 13.72 | - | 1.65 | - | - | 2.24 | 2.24 | 2.24 | 3.02 | 3.02 | 3.02 | - | - | - | - | - | - | - |
| 3/8 | 17.15 | - | 1.65 | - | - | 2.31 | 2.31 | 2.31 | 3.20 | 3.20 | 3.20 | - | - | - | - | - | - | - |
| 1/2(15) | 21.34 | 1.65 | 2.11 | - | - | 2.77 | 2.77 | 2.77 | 3.73 | 3.73 | 3.73 | - | - | - | 4.78 | 7.47 | 4.78 | - |
| 3/4(20) | 26.67 | 1.65 | 2.11 | - | - | 2.87 | 2.87 | 2.87 | 3.91 | 3.91 | 3.91 | - | - | - | 5.56 | 7.82 | 5.56 | - |
| 1(25) | 33.40 | 1.65 | 2.77 | - | - | 3.38 | 3.38 | 3.38 | 4.55 | 4.55 | 4.55 | - | - | - | 6.35 | 9.09 | 6.35 | - |
| 1 1/4(32) | 42.16 | 1.65 | 2.77 | - | - | 3.56 | 3.56 | 3.56 | 4.85 | 4.85 | 4.85 | - | - | - | - | 9.70 | - | - |
| 1 1/2(40) | 48.26 | 1.65 | 2.77 | - | - | 3.68 | 3.68 | 3.68 | 5.08 | 5.08 | 5.08 | - | - | - | - | 7.14 | 15.15 | 7.14 |
| 2(50) | 60.33 | 1.65 | 2.77 | - | - | 3.91 | 3.91 | 3.91 | 5.54 | 5.54 | 5.54 | - | - | - | - | 9.14 | 11.07 | 8.74 |
| 2 1/2(65) | 73.03 | 2.11 | 3.05 | - | - | 5.16 | 5.16 | 5.16 | 7.01 | 7.01 | 7.01 | - | - | - | - | 9.53 | 14.02 | 9.53 |
| 3(80) | 88.90 | 2.11 | 3.05 | - | - | 5.74 | 5.74 | 5.74 | 7.62 | 7.62 | 7.62 | - | - | - | - | 11.13 | 15.24 | 11.13 |
| 3 1/2(90) | 101.60 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 4(100) | 114.30 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 5(125) | 141.30 | 2.77 | 3.40 | - | - | 6.55 | 6.55 | 6.55 | 9.53 | 9.53 | 9.53 | - | - | - | 12.70 | 15.88 | 19.05 | 15.88 |
| 6(150) | 168.27 | 2.77 | 3.40 | - | - | 7.11 | 7.11 | 7.11 | 10.97 | 10.97 | 10.97 | - | - | - | 14.09 | 19.27 | 18.62 | 19.27 |
| 8(200) | 219.08 | 2.77 | 3.76 | 6.35 | 7.04 | 8.18 | 8.18 | 9.18 | 13.20 | 12.70 | 12.70 | 15.09 | 19.26 | 20.62 | 23.81 | 22.23 | 23.81 | |
| 10(250) | 273.05 | 3.40 | 4.19 | 6.35 | 7.80 | 9.27 | 9.27 | 9.27 | 12.70 | 12.70 | 12.70 | 15.09 | 19.26 | 21.44 | 25.40 | 28.58 | 25.40 | |
| 12(300) | 323.85 | 3.96 | 4.67 | 6.35 | 8.38 | 9.53 | 9.53 | 10.31 | 14.27 | 12.70 | 12.70 | 17.48 | 21.44 | 25.40 | 28.58 | 33.32 | 25.40 | |
| 14(350) | 355.60 | 3.96 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 11.13 | 15.09 | 12.70 | 12.70 | 19.05 | 23.81 | 27.79 | 31.75 | 35.71 | 25.40 | |
| 16(400) | 406.40 | 4.19 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 12.70 | 16.66 | 12.70 | 12.70 | 21.44 | 28.39 | 30.96 | 35.53 | 40.49 | 25.40 | |
| 18(450) | 457.20 | 4.19 | 4.78 | 6.35 | 7.92 | 11.13 | 9.53 | 14.27 | 19.05 | 12.70 | 12.70 | 23.81 | 29.36 | 34.33 | 38.67 | 45.24 | 25.40 | |
| 20(500) | 508.00 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 15.09 | 20.62 | 12.70 | 12.70 | 26.19 | 32.54 | 38.10 | 44.45 | 50.01 | 25.40 | |
| 22(550) | 558.80 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 22.23 | 12.70 | 12.70 | 28.58 | 34.93 | 41.26 | 47.63 | 53.98 | 25.40 | - | |
| 24(600) | 609.60 | 5.54 | 6.35 | 6.35 | 9.53 | 14.27 | 9.53 | 17.48 | 24.61 | 12.70 | 12.70 | 30.96 | 38.89 | 46.02 | 52.37 | 59.54 | - | |
| 26(650) | 660.40 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 28(700) | 711.20 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 30(750) | 762.00 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 32(800) | 812.80 | 6.35 | 7.92 | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 34(850) | 863.60 | - | - | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 36(900) | 914.40 | - | - | 7.92 | 12.70 | - | 9.53 | 19.05 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 40(1000) | 1016.00 | - | - | 9.53 | 14.3 | - | 9.53 | 26.20 | - | - | - | - | - | - | - | - | - | - |
Dab tsi yog qhov sib txawv ntawm nominal thiab nti stainless kav hlau?
Nominal loj (DN):
Feem ntau qhia hauv millimeters (hli), lub nominal loj yog hais txog kwv yees li kwv yees lub diam lossis sab hauv cov yeeb nkab ntawm cov yeeb nkab.
Nws yog tus nqi nominal, tsis yog qhov tseeb ntawm cov yeeb nkab. Piv txwv li,Dn50taw qhia txog cov kabinal ntawm lub cheeb tsam yog kwv yees li 50mm, tab sis qhov tseeb ntawm cov cheeb yuav yog60.3mm, nyob ntawm phab ntsa tuab.
Nominal size yog siv dav hauv cov qauv thoob ntiaj teb, tshwj xeeb tshaj yog nyob hauv Europe thiab Asia.
Nti loj (nps):
Qhia nyob rau hauv nti (nti), nti nti loj hais txog cov yeeb nkab nas loj (nps).
Qhov kev sib tham noning yog feem ntau siv nyob rau hauv imperial system lub teb chaws zoo li Tebchaws Asmeskas.
Piv txwv li,NPS 1yeeb nkab muaj lub cheeb tsam tawm ntawm33.4mm, tsis yog 1 nti (25.4mm).
Xa kev nug