Gnee muab siab - zoo AISI 304L stainless hlau daim hlau hauv Tshuag, muab kev xa khoom sai, cov khoom siv zoo ib yam, thiab tus nqi sib tw rau kev lag luam, kev tsim kho, thiab kev tsim khoom. Raws li qis- carbon austenitic stainless hlau (tsawg dua lossis sib npaug li 0.03% C), 304L sib xyaw ua ke zoo heev corrosion resistance, weldability, thiab durability, ua rau nws zoo tagnrho rau kev ua tshuaj, khoom noj khoom haus thiab dej haus, marine, thiab architectural daim ntaub ntawv.

Muaj 304L stainless hlau phaj hauv Tshuag ua kom cov neeg siv khoom tuaj yeem txo cov sij hawm ua cov hmoov txhuas, txo qhov project qeeb, thiab tswj tau siab - cov qauv zoo yam tsis tau tos rau kev tsim khoom tshiab.

 

AISI 304 stainless steel plates
AISI 304 stainless hlau phaj
AISI 304L stainless steel plates
AISI 304L stainless hlau daim hlau

AISI 304L Stainless Hlau Phaj Specifications

Yam khoom Specification
Khoom Qib AISI 304L Stainless hlau
UNS No. S30403
Txuj ASTM A240 / ASME SA240 / EN 10088
Thickness Ntau 1mm-50mm (customizable)
Dav Txog li 2000 mm
Ntev Txog li 6000 mm
Nto tiav 2B / No.1 / BA / Pickled
Kev Xa Khoom Kev daws Annealed
Daim ntawv pov thawj MTC, Chemical Analysis Report, SGS/BV (ntawm kev thov)

Tshuaj muaj pes tsawg leeg ntawm AISI 304L Stainless hlau (wt.%)

Element Cov ntsiab lus
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 10.5
Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.03
Manganese (Mn) Tsawg dua los yog sib npaug rau 2.0
Silicon (Si) Tsawg dua los yog sib npaug rau 1.0
Phosphorus (P) Tsawg dua lossis sib npaug li 0.045
Sulfur (S) Tsawg dua lossis sib npaug li 0.03
Hlau (Fe) Tshuav

Mechanical Properties

Khoom Tus nqi
Tensile zog 485-620 MPa
Yield zog Ntau dua lossis sib npaug li 170 MPa
Elongation Ntau dua lossis sib npaug li 40%
Hardness Tsawg dua lossis sib npaug li 90 HRB

 

Qhov sib txawv ntawm 304L thiab 304 stainless hlau daim hlau
Qhov sib txawv tseem ceeb ntawm 304L thiab 304 yog cov ntsiab lus carbon: 304L Tsawg dua lossis sib npaug li 0.03%, 304 Tsawg dua lossis sib npaug li 0.08%. Cov ntsiab lus qis dua ua rau 304L tsis tshua muaj kev cuam tshuam rau intergranular corrosion tom qab vuam, thaum tuav cov ntsiab lus chromium zoo sib xws (18-20%) thiab cov ntsiab lus npib tsib xee (8-10.5%) raws li 304. Yog li ntawd, nws muaj cov khoom siv qis dua me ntsis tab sis superior weldability thiab corrosion kuj.

 

304L piv nrog 316L stainless hlau li cas?
304L muaj 18-20% chromium thiab 8-10.5% npib tsib xee, muab kev zoo corrosion kuj. Nyob rau hauv sib piv, 316L ntxiv 2-3% molybdenum, uas zoo heev txhim khu kev tiv thaiv rau pitting thiab crevice corrosion nyob rau hauv chloride- nplua nuj ib puag ncig, xws li dej hiav txwv los yog tshuaj tov tshuaj. Cov ntsiab lus carbon zoo sib xws (tsawg dua lossis sib npaug li 0.03%), yog li ob qho tib si qib vuam zoo, tab sis 316L yog qhov nyiam rau marine, tshuaj, thiab siab - chloride daim ntaub ntawv vim nws superior corrosion kuj.

 

304L stainless hlau daim hlau puas tuaj yeem welded?
Yog lawm, 304L stainless hlau daim hlau tuaj yeem welded zoo. Lub "L" hauv 304L sawv cev rau cov pa roj carbon tsawg, nrog cov ntsiab lus siab tshaj plaws ntawm 0.03%, piv rau 0.08% hauv cov qauv 304. Qhov no txo ​​cov pa roj carbon monoxide minimizes carbide nag lossis daus thaum vuam, txo qhov kev pheej hmoo ntawm intergranular corrosion. Nws yog qhov tsim nyog rau txhua txoj kev siv vuam, suav nrog TIG, MIG, thiab vuam vuam, tsis tas yuav tsum tau tshaj tawm -weld annealing feem ntau.

 

 

Txhawm rau ua haujlwm zoo dua thoob ntiaj teb cov neeg yuav khoom, GNEE muab cov txheej txheem them nqi hloov pauv, suav nrog T / T (30% them nqi, 70% them ua ntej xa khoom), pom daim credit (L/C), thiab DP / DA kev xaiv them nyiaj rau cov neeg koom tes ntev -; peb siv seaworthy ntoo crates los yog pallets rau ntim, muab ya raws - pov thawj, xeb- pov thawj, thiab ntug tiv thaiv ntsuas, thiab kom meej meej cim cov cua sov thiab qhov ntev ntawm daim hlau; peb lav kev xa khoom zoo, nroghauv - Tshuag 304 daim hlauxa tuaj nyob rau hauv 7-10 hnub thiab kev cai ntau thiab tsawg xa hauv 15-25 hnub; peb muab cov ntawv pov thawj ua tiav lub Hoobkas (MTC 3.1) thiab muaj kev paub dhau los thoob ntiaj teb kev xa tawm npog rau Middle East, Europe, United States, thiab cov teb chaws Asia.

in-stock 304 plates