AISI 304L Stainless Hlau Capillary Tube
Dec 31, 2025
Tso lus
AISI 304L stainless hlau capillary tubing yog dab tsi?
AISI 304L stainless hlau capillary tubing (UNS S30403, EN 1.4306) yog ib qho ultra-precision nyias-walled austenitic stainless hlau raj nrog cov ntsiab lus carbon tsawg dua los yog sib npaug li 0.035% (tus qauv 304 stainless hlau muaj cov ntsiab lus carbon tsawg dua 0.0%). Nws cov khoom siv tshuab muaj xws li qhov tsawg kawg nkaus lub zog ntawm 170 MPa, tensile lub zog ntawm 485-655 MPa, thiab elongation ntawm ntau dua los yog sib npaug rau 40%. Nws kuj pom zoo corrosion kuj zoo heev nyob rau hauv ib puag ncig tshuaj lom neeg, ua rau nws zoo tagnrho rau cov ntawv thov uas yuav tsum tau sealing thiab tsis kam mus rau intergranular corrosion, xws li cov cuab yeej kho mob, instrumentation, kua sampling systems, aerospace hydraulic kab, thiab semiconductor ua khoom.
Peb SS 304L capillary tubing tshwj xeeb yog tsim los rau cov ntawv thov uas yuav tsum tau nruj me ntsis kam rau ua, txhim kho intergranular corrosion kuj tom qab vuam, thiab siab purity. Nws yog tsim los ntawm kev kos duab txias lossis micro- txheej txheem extrusion thiab ua raws li ASTM A269 / A632 / ASME SA269 cov qauv. Sab nraud diameters (OD) ntau ntawm 0.3-12.7 hli, phab ntsa thicknesses (WT) los ntawm 0.1-1.65 hli (nrog rau precision kam rau ua ntawm ± 0.01 hli), thiab tus qauv ntev yog 1-6 m. Nto tiav suav nrog ci annealed (BA, Ra Tsawg dua lossis sib npaug ntawm 0.8 μm) lossis electropolished (EP, Ra Tsawg dua lossis sib npaug ntawm 0.25 μm).


304L Stainless Hlau Capillary Tube Specification
| Stainless hlau Capillary Tube Size Range | 0.35mm txog 6.35mm OD hauv thickness xws li 0.1mm txog 1.2mm. |
| Stainless hlau Capillary Tube Chaw tsim tshuaj paus Thickness | 1mm txog 20mm, SCH 5/5S, 10/10S, 20/20S, 40/40S, 80/80S, 120/120S, 160/160S as per ANSI B36.19/36.10 |
| Stainless Hlau Capillary Tube Phab Ntsa Thickness | 0.08-0.2 hli |
| Stainless hlau Capillary Tube sab nraud txoj kab uas hla | 0.3-12.0 hli |
| Stainless hlau Capillary Tube khoom | SS 304, SS 304L, SS 316, SS 316L |
| Stainless hlau Capillary Tube tiav | Pickled, Polished, Bright Annealed, Electrolytic Polished |
| Stainless hlau Capillary Tube Form | Round, Strait, Hydraulic thiab lwm yam. |
| Stainless hlau Capillary Tube Hom | Raws li Welded, EFW, ERW, Seamless, Semi Seamless, Bead Removed |
| Stainless hlau Capillary Tube Mill Test Certificate | EN 10204 3.1 |
TP304L Stainless hlau Capillary Tube tshuaj muaj pes tsawg leeg
| STAINLESS STEEL CAPILLARY TUBE QIB | UNS | C | Mn | P | S | Si | Cr | Ni | Mo | Ti | Nb | N |
| TP 304 L | S30403 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-13.0 |
TP304L Stainless Hlau Capillary Tube Mechanical Properties
| Khoom siv | Kub | Kub | Tensile zog | Yield zog | Elongation %, Min |
| Kev kho mob | Min. | Ksi (MPa), Min. | Ksi (MPa), Min. | ||
| º F(º C) | |||||
| TIAB SA 304 | Kev daws | 1900 (1040) | 75(515) | 30(205) | 35 |
| TP 304 L | Kev daws | 1900 (1040) | 70(485) | 25(170) | 35 |
Stainless Hlau Capillary Tube Nqe List
304L stainless hlau Capillary Tube FOB Nqe: US $ 1000-2100 / Tuj
201 316 Stainless hlau Capillary raj FOB Nqe: US $ 1400-2500 / Tuj
316l Stainless Hlau Capillary Tube FOB Nqe: US $ 1200-2200 / Tuj
316L Capillary Stainless Hlau Tube FOB Nqe: US $ 1500-2200 / Tuj
Zoo siab seamless Capillary Tube 316 stainless hlau FOB Nqe: US $ 1400-2200 / Metric Ton
304 stainless hlau Capillary Tube FOB Nqe: US $ 1200-2200 / Tuj
Shipping txoj kev muaj xws li hiav txwv freight (tag nrho cov thawv load / tsawg tshaj lub thawv load, tawm chaw nres nkoj: Shanghai / Ningbo / Qingdao). Qhov kev txiav txim yam tsawg kawg nkaus yog 50 kg lossis 100 meters. Lub sij hawm xa tuaj rau qhov ntau thiab tsawg (sab nraud txoj kab uas hla 0.3-6mm, phab ntsa tuab 0.1-1.0mm) yog 5-10 hnub, thiab rau qhov ntau thiab tsawg, nws yog 15-20 hnub.
AISI 304L stainless hlau capillary raj (UNS S30403, EN 1.4306) tau ntim nrog ntau- txheej ntim ntim los tiv thaiv lawv cov phab ntsa ultra- nyias nyias thiab nruj me ntsis kam rau ua: txheej sab hauv siv zaub mov- qib PVC zaj duab xis rau cov ntawv ntim dej tsis pub muaj kua qaub ntxiv, {6} tiv thaiv corrosion; nruab nrab txheej siv EPE ua npuas ncauj rau kev poob siab; thiab txheej txheej sab nrauv siv fumigated ntoo crates lossis plywood pallets ua raws li ISPM 15 tus qauv (15-25 kg ib crate), ruaj nrog cov hlua hlau, thiab lub raj kawg yog kaw nrog lub hau yas tiv thaiv kom tsis txhob khawb.