Yog hais tias koj tab tom nrhiav rau siab- zoo stainless hlau sawb nrog superior corrosion kuj, uniform thickness, thiab zoo formability, AISI 316L (UNS S31603) yog ib qho ntawm cov ntaub ntawv txhim khu kev qha tshaj plaws rau kev siv hauv kev lag luam. 316L stainless hlau sawb muaj cov ntsiab lus carbon tsawg thiab nplua nuj molybdenum, zoo tiv thaiv pitting thiab crevice corrosion, tshwj xeeb tshaj yog nyob rau hauv chloride- nplua nuj los yog marine ib puag ncig.

Gnee Stainless tsim thiab xa tawm 316L stainless hlau sawb ua raws li ASTM, AISI, JIS, thiab EN cov qauv, tsim nyog rau kev siv hauv cov khoom siv tshuaj, cov khoom siv hluav taws xob, cov khoom siv hauv hiav txwv, thiab cov cuab yeej precision.

Peb cov khoom: 316L Kub-Rolled Sawb, 316L Hard Strip, 1.4404 Txias-Rolled Sawb, SUS316L Bright Annealed Sawb, Laser-Txiav Sawb, Coated Sawb, Caij nplooj ntoos hlav Sawb, Custom-Txoj Sawb, thiab lwm yam.

 

 1.4404 Cold-Rolled Strip

ASTM A240 316L stainless hlau strip specifications

Txuj

ASTM A240, EN 1.4404, JIS G4305

Qib

00Cr17Ni14Mo2, 0Cr18Ni12Mo2Ti, 1.4404, SUS316L, X2CrNiMo17-12-2

Thickness

0.1 hli-6 hli (0.004-2.36 nyob rau hauv), Customized

Dav dav

10mm-1500mm (3.94-590.55 nyob rau hauv), Customized

Ntev

Customized

Nto tiav

2B, 8K, BA, Customized, Tsis yog . 1, NO. 4, Tsis yog. 8

Cov txheej txheem

Txias Rolling, Customized, Kub Rolling, Polishing, Vuam

Daim ntawv

316L Stainless Hlau Sheet, Phaj & Coil, Annealed Sawb, Txias Drawn Sawb, Customized, Kub Rolled Sawb / Coil, Polished Sawb

 

Tshuaj muaj pes tsawg leeg

QIB Tshuaj muaj pes tsawg leeg
  C Si Mn P S Ni Cr Mo
% % % % % % % %
316L Tsawg dua los yog sib npaug li 0.03 Tsawg dua los yog sib npaug rau 1.0 Tsawg dua lossis sib npaug li 2.00 Tsawg dua lossis sib npaug li 0.045 Tsawg dua lossis sib npaug li 0.030 10.00-14.00 16.00-18.00 2.00-3.00

 

Mechanical Properties

Khoom Metric nqi Imperial nqi
Tensile zog 485 MPa (min) 70,000 psi (min)
Yield zog 170 MPa (min) 25,000 psi (min)
Vickers Hardness 152 hwv 152 hwv
Brinell Hardness 146 HB 146 HB
Rockwell Hardness 80 PAB 80 PAB
Elongation 40% 40%
Elastic Modulus 193 gp ua 28 x 10^6 psi

 

316L Stainless Hlau Sawb Nqe Ib Kilogram

Tus nqi ntawm 316L stainless hlau sawb feem ntau yog li ntawm $ 4.8 txog $ 6.5 ib kilogram, nyob ntawm qhov tuab, kev kho deg, thiab kev txiav txim kom muaj nuj nqis. 316L stainless hlau sawb yog tsim raws li ASTM A240 / A480 tus qauv.

 

Corrosion Resistance Sib piv ntawm 316L thiab 304 Stainless Hlau Sawb

Thaum muab piv 316L thiab 304 stainless hlau sawb, lub ntsiab kom zoo dua ntawm 316L yog nyob rau hauv nws molybdenum cov ntsiab lus (2-2.5%), uas ho txhim kho nws tsis kam mus rau pitting thiab crevice corrosion nyob rau hauv chloride los yog saltwater ib puag ncig. Yog li, 316L yog cov khoom siv zoo tshaj plaws rau kev siv tshuaj lom neeg, dej hiav txwv, thiab ntug dej hiav txwv, thaum 304 stainless hlau sawb tuaj yeem pom cov cim ntawm kev xeb hauv lub sijhawm.

 

 

UNS S31603 stainless hlau sawb tsum

Nrog rau ntau tshaj 18 xyoo ntawm kev xa tawm stainless hlau thiab cov khoom lag luam loj ntawm 316L stainless hlau coils thiab strips, GNEE siv cov khoom siv dov thiab polishing siab heev kom ua tiav kev tswj xyuas kom meej. Txhawb ntau yam kev lag luam xws li FOB, CIF, thiab DDP, thiab muab kev xa khoom thoob ntiaj teb, GNEE txaus siab rau kev ntseeg siab ntawm cov neeg siv khoom hauv Tebchaws Europe, Middle East, thiab Southeast Asia.

cold rolled stainless steel strip 316L

Cov ntaub ntawv muab khoom & khoom siv

Yam khoom Paub meej
Muaj Cov Qauv Coil, Sawb, Ntawv Nyiaj, Txiav - mus rau -Length Sheets
Ntim Cov dej noo- ntawv pov thawj + ntoo pallet lossis lub thawv
Cov ntsiab lus xa khoom EXW, FOB, CIF thoob ntiaj teb
Lub Sijhawm Lead 7-15 hnub rau cov qauv Tshuag; customized tsis pub dhau 25 hnub
Cov ntawv pov thawj ISO 9001, SGS, BV, TUV
Kev lav zoo 100% PMI test + EN 10204 3.1/3.2 daim ntawv pov thawj
Yam tsawg kawg nkaus Flexible – me me txiav txim tau txais

stainless steel strip 316L

 

Xa kev nug