2 hli 304 stainless hlau daim ntawv nqi

Sep 15, 2025

Tso lus

Yog tias koj tab tom nrhiav 2 hli 304 stainless hlau ntawv ntawm tus nqi zoo tshaj plaws, GNEE yog koj cov khoom siv txhim khu kev qha. Nrog ntau dua 18 xyoo ntawm kev xa tawm thiab cov neeg siv khoom ntau tshaj 60 lub teb chaws, peb muab cov ntawv tshaj tawm zoo 304 stainless cov nqi sib tw. Peb cov ntawv ua raws li Astm, AISI, JIS, DIN, DIN, thiab FICTENS, ua rau lawv cov khoom siv, ua zaub mov, thiab cov ntawv thov marrine.

 

2 hli 304 stainless hlau ntawv tus nqi nqi rau hauv kg

Qhov tuab Qhov loj me (hli) Nto tas Nqe (USD / KG) Kev yuav tau
2.0 hli 1000 × 2000 2b / ba $2.30 – $2.60 Hauv Tshuag
2.0 hli 1219 × 2438 Hl / No.4 $2.40 – $2.70 Hauv Tshuag
2.0 hli 1500 × 3000 Daim iav (8k) $2.60 – $2.90 Hauv Tshuag
2.0 hli Kev Cai Txiav Txhuam hniav / matte $2.40 – $2.80 Ntawm kev thov

Nco tseg: Cov nqi sib txawv raws qhov chaw ua tiav, kom muaj nuj nqis, thiab qauv kev lag luam. Tiv tauj peb rau qhov tseeb hais tshiab.

 

2mm 304 stainless hlau ntawv specifications

Chaw ua uas tsis tau haus Cov ntsiab lus
Lub hom phiaj ASTM A240 / AISI / EN / JIS
Teem nqi 304 (uns undat400)
Qhov tuab 2 hli
Qhov dav 1000 mm / 1219 mm / 1500 hli / Mekas
Qho ntev 2000 mm / 2438 hli / 3000 mm / Mekas
Nto tas 2b, BA, No.4, HL, Daim iav 8K
Ceev 7.93 g / cm³
Lub zog tensile Ntau dua los yog sib npaug rau 520 mpa
Paib lub zog Ntau dua los yog sib npaug rau 205 MPa
Elongation Ntau dua los yog sib npaug rau 40%
Cov Ntawv Thov Chav ua mov, kev tsim kho, kev ua khoom noj, tshuaj siv tshuaj, kho kom zoo nkauj

 

Cov ntawv thov ntawm 2 hli 304 stainless hlau los xij

Chav Ua Noj thiab Khoom Noj Khoom Haus - Togs, countertops, tso tsheb hlau luam, cia tso tsheb hlau luam.

Kev tsim kho & Architecture - phab ntsa phab ntsa, of elevator interiors, tes.

Tshuaj lom neeg & petrochemical - cia vessels, pipelines, kev hloov cua sov.

Automotive & Tubrog nkoj - Hniav txiav, corrosion - Cov panels tiv taus.

Kev kho mob kev lag luam - cov rooj ua kom tsis muaj menyuam, cov khoom siv, thiab cov khoom siv lab.

 

GNEE muab 304 stainless hlau los xij, tsim los ntawm Austenitic Stainless hlau muaj 18.0,5% npib thiab 8.0%, muab cov txiaj ntsig zoo tshaj plaws cov pa roj carbon ntau, muaj kev muaj txiaj ntsig, thiab weldability, thiab weldability.

 

Peb lub 304 stainless hlau los suav nrog txias- rolled nplooj ntawv 2} {rolled nplooj ntawv hauv non.1 tiav cov ntawv hauv no, muaj nyob rau hauv thicknesses ntawm 0.3 {{- 6.0mm (txias-}}}}} }.cm (kub-rolled), thiab dav ntawm 1000 submm. Cov ntawv no muaj zog ntawm 520-750MPA thiab tawm los ntawm kev siv hauv chav ua noj, thiab kev ua kom zoo nkauj, ua kom zoo nkauj, thiab kev ua kom ncaj ncees yog qhov tseem ceeb.

 

Txhua nplooj ntawv yog muab nrog cov ntawv pov thawj sib xeem (en 10204 3.1 {}}}}}}}}}}}}}}}}}} {

Nyem kom tau txais cov qauv dawb

2mm 304 Stainless Steel Sheets
304 stainless steel sheets
 

Xa kev nug