10 Tons SUH409L Stainless Steel Coils Ua tiav xa tuaj rau Australia
Sep 22, 2026
Tso lus
Tsis ntev los no, GNEE tau ua tiav tiav tag nrho ntawm 10 tons ntawm SUH409L ferritic tshav kub-cov hlau stainless coils rau lub qhov dej zoo- paub Australian cov chaw tsim khoom tshwj xeeb hauv tsheb tso hluav taws xob thiab cov khoom siv hluav taws xob sib pauv. Cov khoom xa tawm SUH409L stainless hlau coils tau tsim nruj raws li JIS G4304 / JIS G4305 tus qauv thiab muab cov ntaub ntawv ua tiav, suav nrog EN10204 3.1 Cov Ntawv Pov Thawj Cov Khoom Siv (MTC).
Thaum lub sijhawm ua haujlwm export no, GNEE tau siv cov kev tswj xyuas zoo thoob plaws hauv tag nrho cov txheej txheem, suav nrog kev xaiv cov khoom siv raw, sijhawm teem sijhawm, kev kho saum npoo, kev tshuaj xyuas zoo, ntim thiab kev thauj mus los thoob ntiaj teb. Los ntawm kev tswj xyuas kom zoo thiab muaj txiaj ntsig zoo - cov txheej txheem daws teeb meem, cov khoom xa tuaj tau tiav thiab ua tiav raws li cov neeg siv khoom xav tau rau qhov raug qhov tseeb, qhov zoo ntawm qhov chaw thiab ua tiav cov ntaub ntawv traceability.
Dab tsi yogSUH409L stainless hlau coils?
SUH409L yog ferritic stainless hlau uas muaj kwv yees li 10.5% - 12.5% chromium thiab stabilized nrog titanium; nws muaj oxidation kuj zoo heev, corrosion kuj, thiab siab -kub durability. Piv nrog rau cov pa roj carbon steel, SUH409L qhia tau hais tias muaj kev ruaj khov zoo dua thiab lub neej ua haujlwm ntev dua hauv cov ntawv thov cuam tshuam nrog cov pa roj carbon monoxide, thermal cycling, thiab sab nraum zoov ib puag ncig, ua rau nws siv dav rau cov kav dej hauv tsheb, mufflers, tshav kub tiv thaiv, thiab cov khoom siv hauv tsev.
SUH409L Stainless Hlau Chev Export rau Australia
| Khoom npe | SUH409L Stainless hlau kauj |
| Stainless Hlau Qib | SUH409L (Sib npaug rau UNS S40900 / EN 1.4512) |
| Txuj | JIS G4304 / JIS G4305 |
| Ntau | 10 Tons |
| Daim ntawv khoom | Stainless hlau Cold Rolled Chev |
| Thickness | 1.5mm (Customized Muaj) |
| Dav | 1219 hli (Customized Muaj) |
| Coil Nyhav | Kwv yees li . 3–5 Tons ib Coil |
| Nto tiav | 2B / Pickled nto |
| Daim ntawv thov | Automotive Exhaust Systems, Thaum tshav kub kub Shields, Thaum tshav kub kub -Resistant Cheebtsam |
| Txheej txheem ntau lawm | Txias Rolling → Annealing → Pickling → Surface Inspection → Slitting |
| Kev soj ntsuam Standard | Chemical, Mechanical, Dimensional thiab Surface Inspection |
| Daim ntawv pov thawj | EN 10204 3.1 MTC |
| Kev ntim khoom | Waterproof ntawv + Hlau Strapping + Export Ntoo Txhawb |
| Lub sij hawm xa tuaj | Kwv yees li . 15–25 Hnub Ua Haujlwm |
Chemical Composition Test Report ntawm SUH409L Stainless Steel Coils xa hauv cov khoom xa tuaj no
Chemical Composition (Measured Values, wt%)
| Chemical Element | C | Si | Mn | P | S | Cr | Ni | Ti |
|---|---|---|---|---|---|---|---|---|
| JIS G4312 Txuj | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 1.00 | Tsawg dua lossis sib npaug li 1.00 | Tsawg dua lossis sib npaug li 0.040 | Tsawg dua lossis sib npaug li 0.030 | 10.50–11.75 | Tsawg dua lossis sib npaug li 0.60 | 6×C–0.75 |
| Cov txiaj ntsig kev xeem tiag tiag ntawm Kev Xa Khoom No | 0.012 | 0.45 | 0.32 | 0.022 | 0.003 | 11.35 | 0.18 | 0.28 |
Mechanical Properties Comparison (Measured Values)
| Mechanical Property | Tensile zog Rm (MPa) | Yield zog Rp0.2 (MPa) | Elongation A5 (%) | Hardness (HRB) | 180℃Bending Test (d=1a) |
|---|---|---|---|---|---|
| JIS G4312 Txuj | Ntau dua lossis sib npaug rau 360 | Ntau dua lossis sib npaug li 175 | Ntau dua lossis sib npaug li 25 | Tsawg dua lossis sib npaug li 88 | Tsis muaj kab nrib pleb |
| Cov txiaj ntsig kev xeem tiag tiag ntawm Kev Xa Khoom No | 435 | 268 | 32.5 | 74 | Hla tsis muaj kab nrib pleb |
Kev sib tw thiab kev daws teeb meem hauv qhov project Implementation

1: Annealing Oxidation thiab Formability Control
Kev sib tw:
SUH409L yog ferritic stainless hlau uas yog rhiab heev rau annealing kub thiab txias npaum li cas. Yog tias qhov chaw tiv thaiv tsis txaus thaum lub sij hawm siab -kub annealing, nyuaj-kom- tshem chromium oxide nplai tuaj yeem tsim rau ntawm daim kab xev. Tsis tas li ntawd, cov cua txias tsis tsim nyog yuav ua rau cov nplej coarsening, cuam tshuam rau kev sib sib zog nqus nqus thiab khoov kev ua tau zoo los ntawm Australian cov neeg siv khoom thaum lub sij hawm tom qab stamping txheej txheem.
Kev daws:
Thaum lub sij hawm tsim khoom, GNEE tau siv lub tshuab hluav taws xob txuas ntxiv nrog 100% hydrogen tiv thaiv huab cua, tswj lub qhov cub hluav taws xob hauv qab -45℃kom txo qis oxidation zoo. Cov txheej txheem sib xyaw-acid pickling tau ua kom zoo kom ntseeg tau tias muaj kev sib txuam thiab huv 2B nto tiav. Los ntawm precisely tswj qhov kawg annealing kub nyob rau hauv820-850 degreethiab thov kom txias ceev, cov nplej loj tau stabilized ntawmQib 8 lossis siab dua, xyuas kom zoo elongation kev ua tau zoo (ntsuas A5: 32.5%) thiab ua tau raws li cov neeg siv khoom xav tau rau kev kos duab sib sib zog nqus thiab daim ntawv thov.
Kev Tiv Thaiv Kev Tiv Thaiv Kev Tiv Thaiv thiab Kev Tiv Thaiv Ntog rau Kev Thauj Mus Los Hauv Hiav Txwv
Kev sib tw:
Txoj kev thauj mus los rau pawg no ntawm SUH409L stainless hlau coils hla dej uas muaj qhov kub thiab txias; diurnal kub hloov nyob rau hauv lub ntim tau yooj yim ua rau condensation (feem ntau hu ua "container rain"). Muab hais tias 409L stainless hlau muaj cov ntsiab lus chromium ntawm kwv yees li 11%, qhov ntev ntev ntawm cov dej noo tuaj yeem ua rau daj staining ntawm qhov chaw, yog li cuam tshuam nws qhov zoo nkauj.
Kev daws:
Lub tswv yim tiv thaiv kev ntim khoom siv VCI (Volatile Corrosion Inhibitor) zaj duab xis thiab peb -txheej txheej xa tawm- qib system tau siv, muab ntau- txheej cais los ntawm kev siv los tiv thaiv- ntawv xeb, yas zaj duab xis, thiab galvanized steel npog. Tsis tas li ntawd, kev lag luam -qib calcium chloride desiccants tau muab tso rau hauv cov thawv, thiab cov dej noo ntawm cov ntoo pallets tau nruj me ntsis tswj kom tsawg dua lossis sib npaug li 12%. Cov kev ntsuas no tau zoo txo cov kev pheej hmoo ntawm ya raws thiab condensation thaum lub sij hawm kev thauj mus los, kom ntseeg tau tias cov hlau coils tswj tau zoo heev ntawm qhov chaw thaum tuaj txog hauv Australia.

Traceability:
Txhua lub kauj hlau muaj tus naj npawb ntawm cov cua sov tshwj xeeb thiab tus lej coil, tso cai rau kev taug qab tag nrho rov qab mus rau qhov tshwj xeeb steelmaking tshav kub, kub -rolling parameters ntawm tus tswv coil, thiab txias -rolling annealing records.


Independent Thib Peb-Party Verification:
Ntxiv nrog rau hauv -house EN 10204 3.1 daim ntawv pov thawj, ntawm - qhov chaw kuaj tau ua los ntawm thoob ntiaj teb thib peb - tog ntawv pov thawj lub cev SGS ua ntej packing. Cov txiaj ntsig tau los ntawm ob qho tib si spectroscopic tsom xam thiab kev ntsuas kev ntsuas tensile tau ua raws li cov neeg siv khoom kos duab engineering thiab JIS G 4312 cov kev qhia tshwj xeeb.

Cov lus teb rau cov neeg siv khoom:
Thaum cov khoom tuaj txog ntawm Melbourne qhov chaw, cov neeg siv khoom tau qhuas cov coils rau lawv qhov chaw tiaj tus, thickness kam rau ua (tswj nruj me ntsis hauv ± 0.02 hli), thiab kev ua haujlwm stamping; cov txheej txheem kev yuav khoom rau batch tom ntej no twb tau pib ua haujlwm lawm.



Yog tias koj tab tom nrhiav SUH409L stainless hlau coils rau automotive tso tshuab, cua sov- cov khoom tiv thaiv lossis cov ntawv thov kev lag luam, GNEE tuaj yeem muab JIS cov ntaub ntawv txheem nrog EN10204 3.1 MTC, tag nrho traceability, nruj zoo soj ntsuam thiab customized coil ua cov kev pab cuam kom tau raws li lub ntiaj teb no project yuav tsum.