1.4310 Stainless Hlau Sawb Nqe Ib kg

Apr 10, 2026

Tso lus

Txawm hais tias koj tab tom tsim cov tshuab hluav taws xob, cov khoom siv hluav taws xob zoo, lossis cov khoom siv kho mob, ib qho ntawm cov lus nug feem ntau ntawm cov thawj coj yuav nug thaum nrhiav 1.4310 stainless hlau sawb yog: "Dab tsi yog tus nqi tiag tiag ntawm ib kilogram? Thiab vim li cas cov nqi sib txawv li ntawd?"


Hauv phau ntawv qhia no, peb muab ntau tshaj li ib daim ntawv teev nqi yooj yim xwb. Peb yuav muab ib qho kev soj ntsuam hauv - qhov tob ntawm cov yam uas ua rau muaj kev hloov pauv ntawm tus nqi, qhia koj yuav ua li cas xam cov khoom hnyav hnyav, thiab piav qhia yuav ua li cas kom tau siab - lub zog EN 1.4310 (AISI 301) stainless hlau sawb.

 

Tus nqi ntawm 1.4310 Stainless Hlau Sawb ib kg yog dab tsi?

Tus nqi rau 1.4310 (AISI 301) stainless hlau sawb feem ntau yog li ntawm $ 1,500 txog $ 5,000 USD ib tuj ($ 1.50– $ 5.00 / kg) nyob ntawm tuab, txias - dov temper, thiab tus neeg muag khoom. Precision-qib los yog cov ntawv tshwj xeeb nyias nyias strips feem ntau hais kom tus nqi siab dua, thaum cov khoom lag luam xaj ntau rau tus qauv txias{11}} dov coils nyob rau hauv qis kawg.

Thickness Nto Qhov xwm txheej Nqe (USD / kg)
0.1-0.3 hli 2B / IB Mos (Annealed) $2.20 – $3.00
0.3-1.0 hli 2B / IB Ib nrab Hard $2.40 – $3.30
0.5-2.0 hli 2B / IB Full Hard $2.60 – $3.80
Kev cai HL / Polished Customized $3.00 – $4.50+

 

Yuav ua li cas xam 1.4310 Sawb Luj?

Txhawm rau kom tsis txhob overcharged, koj yuav tsum paub yuav ua li cas xam qhov hnyav ntawm koj qhov kev txiav txim. Stainless hlau 1.4310 muaj qhov ceev ntawm kwv yees li7.9 g / cm³.

Cov Formula:

Qhov hnyav (kg)=Thickness (mm) × Dav (mm) × Length (m) × 0.0079

 

Piv txwv li: Yog tias koj xav tau ib daim kab xev uas yog 0.5 hli tuab, 100 hli dav, thiab 1000 meters ntev:
0.5 × 100 × 1000 × 0.0079 = 395kg ua.

 

 

Cov yam ntxwv cuam tshuam rau tus nqi ntawm 1.4310 Stainless Hlau Sawb

 

1. Raw Material Surcharge (Nickel & Chromium)

1.4310 stainless hlau muaj kwv yees li6-8% npib tsib xeethiab16-18% chromium. Thaum nickel nqi ntawm lubLondon Hlau Txauv (LME)sawv sharply, covalloy surchargence raws li, ncaj qha cuam tshuam tus nqi ib kg.

 

2. Thickness & Precision

Ultra- cov ntawv nyias nyias (xws li0.02mm los yog 0.05mm) xav tau ntau dua dov hla thaum lub sijhawm tsim khoom thiab xav tau kev tswj hwm nruj heev. Qhov no ua rau nce tus nqi ua ib kilogram.

 

3. Temper thiab Hardness

1.4310 steel sawb feem ntau raug txiav txim rau qee yam kev kub ntxhov, suav nrog: Annealed, 1/4 Hard, 1/2 Hard, 3/4 Hard, Full Hard, los yog Ntxiv Hard. Ua kom tiav cov hom phiaj tensile lub zog tshwj xeeb (xws li, 1300+ MPa) yuav tsum tau siv cov txheej txheem tshwj xeeb ntawm kev kho cua sov thiab kev txawj ntse hauv cov txheej txheem txias dov.

 

4. Qhov yuav tsum tau ua tiav

Tus qauv2B tiavyog qhov kev xaiv pheej yig tshaj plaws. Txawm li cas los xij, yog tias koj daim ntawv thov yuav tsum tau ua tiav tshwj xeeb xws liBA (Zoo Annealed), Cov plaub hau (Brushed), los yogPolished, tus nqi ntxiv ntawm kwv yees li$0.20 - $0.50 ib kgyuav tsum tau tos.

 

5. Order Volume (MOQ)

Yuav 20-tuj Tag Nrho Cov Thawv Thauj Khoom (FCL) yuav ib txwm muab tus nqi zoo dua li 500kg LCL (Less than Container Load) xaj vim kev xa khoom thiab cov nqi teeb tsa.

Kuv yuav ua li cas thiaj paub tseeb tias kuv yuav khoom 1.4310 tiag tiag?

Ib txwm thov daim ntawv pov thawj Mill Test (MTC) uas ua raws li EN 10204 3.1 tus qauv. Gnee muab MTC nrog rau txhua qhov khoom xa tuaj, uas qhia meej txog cov khoom siv tshuaj muaj pes tsawg leeg thiab cov ntaub ntawv tensile lub zog.

Nyem kom tau txais MTC rau 1.4310 Stainless Hlau Sawb

 

Tshuaj muaj pes tsawg leeg 1.4310

Raws li EN 10088-2 Standard.

Lub ntsiab Cim Feem pua ​​(%)
Cov pa roj carbon C 0.05 – 0.15
Silicon Si Tsawg dua lossis sib npaug li 1.00
Manganese Mn Tsawg dua lossis sib npaug li 2.00
Phosphorus P Tsawg dua lossis sib npaug li 0.045
Sulfur S Tsawg dua lossis sib npaug li 0.015
Chromium Cr 16.00 – 19.00
Nickel Ni 6.00 – 9.00
Molybdenum Mo Tsawg dua lossis sib npaug li 0.80
Nitrogen N Tsawg dua lossis sib npaug li 0.10

 

Mechanical Properties (In Annealed Condition)

Cov khoom ntawm chav sov rau 1.4310 hauv cov tshuaj -annealed xeev (+AT).

Khoom Tus nqi (Metric) Tus nqi (Imperial)
Tensile zog (Rm) 500-950 MPa 72.5-138 hli
0.2% Tawm Zog (Rp0.2) Ntau dua lossis sib npaug li 230 MPa Ntau dua lossis sib npaug li 33 ksi
Elongation (A80 hli) Ntau dua lossis sib npaug li 40% Ntau dua lossis sib npaug li 40%
Hardness (Brinell) Tsawg dua lossis sib npaug li 230 HB Tsawg dua lossis sib npaug li 230 HB
Modulus ntawm Elasticity 196 gpa ua 28,4 x 10³ ksi

 

Mechanical Properties nyob rau hauv txias -Ua hauj lwm mob (Lub caij nplooj ntoos hlav Tempers)

Condition (Temper) Tensile zog Rm (MPa) Pov thawj muaj zog Rp0.2 (MPa)
+ C700 (1/4 Hard) 700 – 850 Ntau dua lossis sib npaug li 450
+ C850 (1/2 Hard) 850 – 1000 Ntau dua lossis sib npaug li 600
+ C1000 (3/4 Hard) 1000 – 1150 Ntau dua lossis sib npaug li 750
+ C1150 (tag nrho Hard) 1150 – 1300 Ntau dua lossis sib npaug li 900
+ C1300 (Lub Caij Nplooj Ntoos Hlav) 1300 – 1500 Ntau dua lossis sib npaug rau 1050
+ C1500 (Ntxiv Hard) 1500 – 1700 Ntau dua lossis sib npaug rau 1150

 

1.4310 puas tuaj yeem siv rau laser txiav?

Yog lawm, tab sis thov xyuas kom meej tias koj xaj cov khoom siv strip uas tau dhau los ntawm "nrawm qib." Qhov no tau lees tias lub sawb tseem nyob tiaj tus tom qab txiav thiab tsis muaj "caij nplooj ntoos hlav" lossis deformation.

 

Puas yog 1.4310 cov khoom sib nqus?

Hauv lub xeev annealed (mos), cov khoom tseem ceeb tsis yog -magnetic. Txawm li cas los xij, vim yog 1.4310 txoj haujlwm tseem ceeb- cov yam ntxwv hardening, thaum nws tau txias - dov kom ua tiav lub xeev siab - hardness, nws cov khoom sib nqus ua kom muaj zog heev.

 

Ntawm Gnee Steel, peb tsis tsuas yog muag 1.4310 stainless hlau strips; peb muab kev daws teeb meem kev tsim khoom. Peb tuav ib qho kev npaj ua ntej - rau - nkoj cov khoom muag ntawm ntau tshaj 10,000 tons ntawm stainless hlau strips, featuring dav tolerances nrog ib tug precision txog li 0.05mm. Peb cov khoom raug xa tawm mus rau ntau tshaj 50 lub teb chaws thoob ntiaj teb, siv cov ntim tshwj xeeb tsim los ua kom tau raws li cov qauv kev xa nkoj thoob ntiaj teb.

1.4310 Stainless Steel Strip

1.4310 Stainless Steel Strip Supplier
1.4310 Stainless Hlau Sawb Supplier
AISI 301 Stainless Steel Coil Strip
AISI 301 Stainless hlau kauj sawb

Xa kev nug