Qhov twg zoo dua SUS304 lossis SUS316?

Nov 27, 2025

Tso lus

Rau engineers thiab procurement specialists, xaiv txoj cai stainless hlau yog ib qho tseem ceeb heev. Ntawm cov qib feem ntau yog SUS304 thiab SUS316, ob qho tib si austenitic stainless hlau-tab sis lawv muaj qhov sib txawv tseem ceeb hauv kev tiv thaiv corrosion, nqi, thiab kev siv.

Cov lus qhia no pab cov neeg yuav khoom txiav txim siab, muaj cov ntaub ntawv cov khoom, cov khoom siv kho tshuab, tus nqi, FAQs, thiab kev pom kev lag luam.

 

Dab tsi yogSUS304 Stainless hlau?

SUS304 yog lub npe Japanese rau stainless hlau, sib npaug rau American 304 stainless hlau, thiab raug cais raws li 06Cr19Ni10 hauv Suav teb tus qauv. Nws belongs rau 18-8 austenitic stainless hlau tsev neeg thiab muaj npe rau nws kwv yees li 18% chromium thiab 8% nickel cov ntsiab lus. Vim nws zoo heev corrosion kuj, kub-resistant, zoo mechanical zog, thiab machinability, SUS304 yog dav siv nyob rau hauv kev tsim kho, ua zaub mov, khoom siv kho mob, thiab tshuaj industries.

 

Dab tsi yog SUS316 stainless hlau khoom?

SUS316 yog austenitic stainless hlau nrog ntxiv molybdenum, muab nws superior corrosion kuj piv rau SUS304, tshwj xeeb tshaj yog nyob rau hauv chloride ib puag ncig (xws li dej hiav txwv). Nws muaj cov yas zoo, toughness, txias ua haujlwm, thiab weldability, thiab feem ntau yog siv rau hauv kev tsim cov corrosion-cov khoom siv thiab cov khoom siv, tab sis nws cov nqi kuj siab dua li ntawm 304 stainless hlau.

 

SUS304 vs SUS316 Stainless hlau:Tshuaj muaj pes tsawg leeg

Tshuaj muaj pes tsawg leeg

Cov pa roj carbon (C)

Silicon (Si)

Manganese (Mn)

Phosphorus (P)

Sulfur (S)

Nickel (Ni)

Chromium (Cr)

Mo

SUS 304

Tsawg dua 0.08

Tsawg dua 1.00

Tsawg dua 2.00

Tsawg dua 0.045

Tsawg dua 0.030

8.0-10.5

18.0-20.0

–

SUS 316

Tsawg dua 0.08

Tsawg dua 1.00

Tsawg dua 2.00

Tsawg dua 0.045

Tsawg dua 0.030

10.0-14.0

16.0-18.0

2.0-3.0

 

SUS304 vs SUS316 Stainless hlau:Mechanical Properties

Khoom SUS 304 SUS 316
Tensile zog 520 MPa rau 515 MPa ua
Yield zog 215 MPa 205 MPa
Elongation 40% 40%
Hardness 170 HB 150-190 HB
Max Service Kub 870 degree 925 degree
Qhov ntom 7.93 g/m² 8.0 g / cm³

 

SUS304 vs SUS316 Stainless hlau: Lub cev muaj zog

Lub cev muaj zog

Qhov ceev (kg / m3)

Modulus ntawm elasticity (GPa)

Kev tiv thaiv hluav taws xob tshwj xeeb (chav kub) μΩ cm

Cov cua kub tshwj xeeb ((0-100 degree) KJ / kg ・K)

Thermal conductivity ((100 degree) W / m ・ K)

Thermal expansion coefficient (0-100 degree) × 10⁻⁶ / degree

SUS 304

7930

193

72

0.5

16.3

17.3

SUS 316

7980

193

74

0.5

16.3

15.9

 

Qhov twg zoo dua, SUS304 lossis SUS316?

SUS316 muaj ntau molybdenum thiab npib tsib xee dua SUS304, uas txhawb nqa kev tiv thaiv tab sis nce nqi. Nws raug pom zoo rau ib puag ncig uas raug dej hiav txwv, huab cua ntawm ntug dej hiav txwv, lossis hiav txwv cua, qhov twg muaj kev pheej hmoo corrosion siab. Nyob rau hauv ib puag ncig hnyav, cov hlau tsis muaj steel nrog kev ua haujlwm siab dua li SUS316 yuav tsum tau.

 

SUS304 vs SUS316 stianless steel: Corrosion Resistance

SUS316 qhia tau zoo heev corrosion kuj piv rau SUS304, tshwj xeeb tshaj yog thaum raug chloride thiab acidic ib puag ncig. Qhov no yog vim SUS316 muaj kwv yees li 2% molybdenum, txhim kho nws cov kev tiv thaiv rau pitting thiab crevice corrosion, thaum SUS304 tsis muaj molybdenum. Yog li, SUS316 yog qhov tsim nyog rau thaj chaw ntug dej hiav txwv, thaj chaw marine, lossis tuav cov tshuaj corrosive.


SUS304 vs SUS316: Machinability

SUS304 yooj yim dua rau tshuab dua SUS316, muab kwv yees li 45% machinability piv rau SUS316's 36% (xws li 1212 carbon steel). Txawm hais tias ob qho tib si yog austenitic stainless hlau uas ua haujlwm- tawv sai sai thiab ua kom muaj cua sov, SUS316 yog qhov pom tseeb thiab tawv dua vim nws cov ntsiab lus molybdenum.

 

SUS304 vs SUS316: Nqe

Metric / Format SUS304 Nqe Ntau SUS316 Nqe Ntau Tus nqi hwm rau SUS316
Ntiaj teb Raw Material (ib KG) $3.50 – $5.00 $4.50 – $6.50 ~ 20% - 30% siab dua
B2B Slabs / Ntawv (ib KG) $2.50 – $3.50 $3.50 – $5.00 ~ 30% - 50% siab dua
Teb Chaws Asmeskas Tshuag / Daim Ntawv (ib LB) $1.45 – $2.06 $2.50 – $2.80 ~ 35% - 70% siab dua
Scrap Hlau Tus Nqi (ib LB) ~$0.56 ~$0.78 ~ 40% siab dua

 

 

SUS304 vs SUS316 Stainless hlau: Yuav xaiv li cas?

1. Xaiv SUS304 kom txuag Upfront peev yog:
Qhov chaw nyob sab hauv tsev, huab cua- tswj tau, lossis qhuav.
Daim ntawv thov no suav nrog dej tshiab lossis tsis yog - cov tshuaj corrosive.
Koj tab tom tsim cov khoom siv hauv chav ua noj, cov cuab yeej npaj zaub mov (tsis muaj ntsev), lossis cov khoom siv hauv tsev.

2. Them SUS316 Hwm kom qis dua -Cov Nqi Them Nqi yog:
Ib puag ncig cuam tshuam ncaj qha dej hiav txwv, dej ntsev, lossis huab cua hauv hiav txwv.
Lub tshuab ua cov khoom noj uas muaj kua qaub (brining kab) los yog cov tshuaj lom neeg muaj zog.

Yog tias koj tab tom nrhiav cov ntaub ntawv rau ib qhov project, qhia rau kuv paub koj hom kev lag luam (xws li marine, zaub mov, kev tsim kho) thiab kev khiav hauj lwm ib puag ncig yog li kuv tuaj yeem xam seb qhov kev kho dua tshiab rau SUS316 yuav txuag koj nyiaj li cas.

Hu rau tam sim no

 

GNEE Stainless Hlau yog ib qho khoom lag luam ywj pheej thiab cov txheej txheem ntawm SUS 304/316 stainless hlau. Nrog rau cov khoom lag luam loj thiab muaj peev xwm ua tau zoo, peb tuaj yeem ua tau raws li cov kev xav tau ntawm feem ntau cov haujlwm, txawm tias cov khoom lag luam lossis cov kev cai txiav txim. Peb muab: Tshuag loj ntawm daim ntawv thiab phaj, Tshuag ntev ntawm puag ncig bar, ruaj - ntev daim ntawv thiab phaj, tsau-ntev round bar, txias sib sau ntawm daim ntawv thiab phaj thiab puag ncig bar, thiab lwm yam kev pab cuam tsim nyog. Yog xav paub ntxiv, thov Email:sales@gneestainless.com.

SUS 304 stainless steel plate
SUS 304 stainless hlau phaj
ASTM A276 304 stainless steel bar
ASTM A 276 304 stainless hlau bar
ASTM A276 316L stainless steel bar
ASTM A 276 316L stainless hlau bar