Qhov twg zoo dua: Khoom noj khoom haus-Qib 304 Stainless Hlau lossis 316 Stainless Hlau?
Dec 17, 2025
Tso lus
Khoom noj khoom haus-Qib 304 thiab 316: Cov Cai Li Cas?
Khoom noj khoom haus-qib 304 stainless hlau yog austenitic 304, UNS S30400 thiab EN 1.4301, tsim los nrog kev tswj muaj pes tsawg leeg, huv si melting thiab ib tug haum nto tiav kom cov khoom raws li cov zaub mov- tiv tauj rau kev nyab xeeb xws li GB 4806.9 thiab FDA 21 CFR6 hais txog kev tso tawm ntawm UN{0} thiab EN 21 CFR6{0} 1.4401, yog molybdenum{11}}cov qib austenitic. Tsis muaj qib twg zoo dua: qhov kev xaiv raug yog nyob ntawm cov khoom noj, tshuaj ntxuav, cov tshuaj chloride load thiab cov cuab yeej siv nyiaj.
Chemical Composition piv
Cov lus hauv qab no piv cov qauv kev txwv tsis pub dhau ASTM A240 rau UNS S30400 thiab UNS S31600. Tus nqi yog qhov feem pua siab tshaj plaws tshwj tsis yog tias muaj ntau yam qhia.
| Element | 304 (S30400) | 316 (S31600) |
|---|---|---|
| C | 0.08 | 0.08 |
| Mn | 2.00 | 2.00 |
| P | 0.045 | 0.045 |
| S | 0.030 | 0.030 |
| Si | 0.75 | 0.75 |
| Cr | 17.5-19.5 | 16.0-18.0 |
| Ni | 8.0-10.5 | 10.0-14.0 |
| Mo | Tsis tau teev tseg, residual nkaus xwb | 2.0-3.0 |
Vim li cas molybdenum tseem ceeb hauv kev pabcuam zaub mov
Molybdenum txhawb nqa kev tiv thaiv rau pitting thiab crevice corrosion nyob rau hauv chloride-cov kabmob media. Cov khoom noj ib puag ncig xws li brines, sauces, txiv lws suav, kua txiv hmab txiv ntoo thiab cov tshuaj chlorine-raws li cov tshuaj tua kab mob raws nraim cov xov xwm uas 316 outlasts 304. Ob qib muaj zog tensile yam tsawg 515 MPa thiab yield zog 205 MPa ib ASTM A240, yog li qhov kev xaiv tshuab; ide qhov kev txiav txim siab yog purely txog corrosion load.
Kev nyab xeeb thiab kev tswj hwm keeb kwm yav dhau
GB 4806.9 yog lub teb chaws Suav zaub mov- tus qauv kev nyab xeeb rau cov khoom siv hlau thiab cov khoom npaj rau kev sib cuag zaub mov; nws txwv kev tsiv teb tsaws ntawm cov khoom xws li txhuas, cadmium, chromium thiab nickel. FDA 21 CFR txhais cov zaub mov-cov tshuaj tiv thaiv hauv Tebchaws Meskas. Ob leeg 304 thiab 316 nyob rau hauv daim ntawv ua tau zoo yog txais khoom noj-cov ntaub ntawv tiv tauj; Kev ua raws cai yog qhia los ntawm kev kuaj kev tsiv teb tsaws ntawm cov ntawv tiav, tsis yog los ntawm lub npe qib ib leeg. Qhov kev ua haujlwm tsis tu ncua ntawm ob qib siab tshaj qhov ntsuas kub tau mus txog hauv kev ua zaub mov, yog li thermal degradation ntawm cov hlau tsis yog qhov kev txhawj xeeb.
304 lossis 316: Yam Koj Yuav Tsum Tau Xaiv?
Xaiv 304 rau cov khoom noj khoom haus dav dav, cov txee chav ua noj thiab cov dab dej, cov tso tsheb hlau luam, brewing thiab cov khoom noj siv mis, cov tais diav thiab cov tais diav, thiab feem ntau cov khoom siv hauv chav ua noj.
Xaiv 316 rau siab -cov khoom siv ntsev thiab kua qaub, kev ua zaub mov hauv hiav txwv thiab dej hiav txwv, tshuaj- qib kev sib cuag, thiab cov txheej txheem ntxuav nrog cov tshuaj chlorine muaj zog- raws li cov tshuaj tua kab mob.
316 tus nqi ntau dua vim nws cov molybdenum thiab cov ntsiab lus nickel ntau dua, yog li qhov tshwj xeeb yuav tsum tau ua raws li qhov tseeb corrosion load es tsis yog rau ib qho kev nyiam rau ib qib.
Cov ntawv thov hauv Kev Lag Luam Khoom Noj
304 stainless hlau ntawv yog dav siv rau cov khoom siv ua noj, cov rooj ua haujlwm, cov thawv ntim khoom noj thiab dej haus, cov khoom siv tub yees thiab cov tshuab ua haujlwm. 316 stainless hlau tau teev tseg rau cov chaw ua zaub mov hauv hiav txwv, khaws cov khoom noj acidic thiab dej haus xws li cov txiv lws suav thiab kua txiv qaub, siab - salinity coastal nroj tsuag, thiab cov tshuaj tiv thaiv kab mob {3} kev siv tshuaj.
Cov lus nug nquag
Q1: Puas yog 316 muaj kev nyab xeeb rau kev sib cuag zaub mov?
A1: Yog lawm. 316 yog cov khoom noj uas tau txais-hu rau qib austenitic nrog muaj zog tiv thaiv alkalis, acids thiab chlorides, thiab nws qhov kev khiav hauj lwm tsis tu ncua yog nyob deb tshaj qhov ntsuas kub tau mus txog hauv kev ua zaub mov.
Q2: Puas yuav 304 xeb hauv kev pabcuam zaub mov?
A2: Nyob rau hauv huv si, zoo -drained ib puag ncig 304 ua tau zoo heev. Nyob rau hauv kev sib cuag nrog ntsev, brine los yog chlorine -raws li cov tshuaj tua kab mob nws tuaj yeem txhim kho pitting corrosion, uas yog lub hauv paus tseem ceeb rau xaiv 316 rau cov kev pabcuam zoo li no.
Q3: Cov zaub mov - qib txhais li cas hauv kev xyaum?
A3: Khoom noj khoom haus- qib txhais tau hais tias cov khoom siv thiab cov ntawv ua tiav txaus siab rau cov zaub mov- tiv tauj cov kev txwv kev tsiv teb tsaws uas tau teev tseg los ntawm cov qauv xws li GB 4806.9 thiab FDA 21 CFR, txheeb xyuas los ntawm kev sim ntawm cov kab lus tseeb.
Q4: Puas yog 316 tsim nyog tus nqi ntxiv?
A4: Nws nyob ntawm ib puag ncig. Nyob rau hauv siab - ntsev, acidic los yog marine ua zaub mov, 316 zam pitting thiab ncua lub neej ntawm cov cuab yeej, uas feem ntau justifies tus nqi. Rau chav ua noj dav dav, 304 txaus.
Q5: Cov qauv twg txhais cov zaub mov- tiv tauj stainless hlau?
A5: Cov ntaub ntawv tseem ceeb yog GB 4806.9 hauv Suav teb thiab FDA 21 CFR hauv Tebchaws Meskas, txhawb nqa los ntawm cov qauv khoom xws li ASTM A240 rau lub hauv paus hlau muaj pes tsawg leeg.
Q6: Puas yog 304 thiab 316 sib txawv ntawm lub zog txhua yam?
A6: Tsis muaj qhov sib txawv ntawm qhov tsim qauv: ob qho tib si muaj lub zog tensile yam tsawg 515 MPa thiab tawm lub zog 205 MPa rau ASTM A240.