Yam khoom twg yog 1.4878 sib npaug rau?
Nov 10, 2025
Tso lus
Dab tsi yog 1.4878 khoom?
1.4878 yog European (EN) cov khoom naj npawb ntawm X8CrNiTi18-10, titanium-stabilized, tshav kub-resistant austenitic stainless hlau. Cov muaj pes tsawg leeg yog tsim los ntawm 18-8 chromium-nickel puag nrog txhob txwm siab dua cov pa roj carbon ntau ntawm 0.04-0.10%, ua ke nrog titanium ntxiv ntawm tsawg kawg plaub npaug ntawm cov ntsiab lus carbon. Cov pa roj carbon ntau dua ua rau lub zog thiab nkag siab ntawm qhov kub siab, thiab cov titanium xauv cov pa roj carbon monoxide rau hauv cov carbides ruaj khov kom cov khoom tsis hnov tsw thaum tuav hauv lossis rov ua dua los ntawm 425-900℃ntau.
Hauv North America cov khoom siv tib yam hu ua AISI 321H, nrog UNS tus lej S32109; Nyob rau hauv Nyiv nws yog SUS321H nyob rau hauv JIS G4312. H qhia txog qhov siab -carbon, siab- kub hloov pauv ntawm tus qauv stabilized qib 321 (UNS S32100, EN 1.4541).
1.4878 stainless hlau sib npaug khoom
| Qhov system | Lub npe |
|---|---|
| EN | 1.4878 / X8CrNiTi18-10 |
| ASTM | 321H / S32109 |
| JIS | SUS 321 H |
| AFNOR | Z6CNT18-10 |
| BS | 321S51 |
| ISO | X7CrNiTi18-10 tsev neeg |
| GOST | 12 KH18N10T |
Cov tshuaj muaj pes tsawg leeg rau EN 10088 / EN 10095
| Element | 1.4878 (AISI 321H) wt. % |
|---|---|
| C | 0.04–0.10 |
| Si | Tsawg dua lossis sib npaug li 1.00 |
| Mn | Tsawg dua lossis sib npaug li 2.00 |
| P | Tsawg dua lossis sib npaug li 0.045 |
| S | Tsawg dua lossis sib npaug li 0.015 |
| Cr | 17.0–19.0 |
| Ni | 9.0–12.0 |
| Ti | Ntau dua lossis sib npaug li 4 × C, Tsawg dua lossis sib npaug rau 0.70 |
Mechanical Properties ntawm Chav Kub
| Khoom | 1.4878 (AISI 321H) |
|---|---|
| Tensile zog (Rm) | 520-750 MPa |
| Yield zog (Rp0.2) | Ntau dua lossis sib npaug li 210 MPa |
| Elongation (A5) | Ntau dua lossis sib npaug li 35% |
| Hardness | Tsawg dua lossis sib npaug li 217 HB |
Thaum tshav kub kub Resistance thiab siab -Tub kub Service
1.4878 muaj qhov zoo oxidation tsis kam mus txog 900℃hauv kev pabcuam cuam tshuam thiab 925℃hauv kev pabcuam txuas ntxiv. Nws lub zog tsim yog siv nyob rau hauv 425-900℃band, qhov twg cov pa roj carbon ntau dua thiab titanium stabilization muab kev coj tus cwj pwm zoo dua li tus qauv stabilized qib 1.4541. Qhov no yog vim li cas 1.4878 tau teev tseg rau lub zog los yog thauj khoom-cov kabmob hauv cov khoom siv rau hauv lub cub tawg, lub tshuab tso pa, thermal oxidizers thiab cov khoom siv hluav taws xob, thaum 1.4541 npog dav dav -lub hom phiaj kev pabcuam ntawm qhov kub thiab txias.
Nyob rau hauv lub annealed mob nws corrosion kuj yog piv rau 304 tsev neeg, nrog rau qhov zoo ntawm weldments thiab kev pab cuam -tawm qhov chaw tsis poob intergranular corrosion kuj nyob rau hauv lub rhiab heev ntau yam. Zoo li txhua qib austenitic nws tseem muaj kev cuam tshuam rau pitting thiab crevice corrosion nyob rau hauv sov chloride ib puag ncig thiab chloride kev nyuaj siab corrosion tawg saum toj li 60 degree.
1.4878 vs 1.4541: Qhov txawv yog dab tsi?
Ob yam khoom muaj feem xyuam zoo sib xws. 1.4541 (X6CrNiTi18-10, AISI 321, UNS S32100, JIS SUS321) muaj cov pa roj carbon txwv ntawm 0.08% thiab yog qib qib ruaj khov rau qhov dav dav thiab siab me me {{14{14}{}} qhov kub thiab txias (X8CrNiTi18-10, AISI 321H) nqa 0.04–0.10% carbon, uas nce lub sij hawm luv luv thiab creep zog ntawm qhov kub thiab txias. Qhov twg tus qauv tsim kub siab tshaj li 500-600℃los yog cov khoom yog load-bearing ntawm qhov kub thiab txias, 1.4878 yog xaiv; hauv qab no, 1.4541 muaj lub zog txaus nrog kev lag luam zoo dua thiab yooj yim dua vuam me ntsis.
1.4878 stainless hlau daim ntaub ntawv
Rauv qhov chaw, radiant raj thiab burner Cheebtsam
Automotive thiab industrial pa system thiab silencers
Superheater raj thiab boiler internals
Thermal oxidizers thiab incinerator liners
Thaum tshav kub kub exchangers thiab expansion pob qij txha nyob rau hauv cov pa kub kev pab cuam
FAQ
Puas yog 1.4878 tib yam li 321?
Tsis raws nraim . 1.4878 yog lub tshav kub- tiv taus siab -carbon variant 321H, thaum 321 (EN 1.4541) yog tus qauv stabilized qib. Lawv yog tib tsev neeg cov khoom siv nrog tib titanium stabilization, tab sis 1.4878 muaj cov pa roj carbon ntau dua rau kev nkag siab zoo dua ntawm qhov kub siab.
Dab tsi yog 1.4878 sib npaug hauv JIS?
Qhov sib npaug JIS yog SUS321H, siab -cov pa roj carbon cua sov- qib tiv thaiv tau teev tseg hauv JIS G4312 rau cua sov- cov phaj hlau, ntawv thiab sawb.
Qhov txawv ntawm 1.4541 thiab 1.4878 yog dab tsi?
1.4541 yog AISI 321 nrog carbon txog 0.08%; 1.4878 yog AISI 321H nrog carbon 0.04-0.10%. Cov pa roj carbon ntau dua muab 1.4878 lub zog siab dua thiab nkag siab ua haujlwm siab tshaj li ntawm 500 degree, ntawm tus nqi qis me ntsis weldability, uas yog vim li cas nws thiaj li nyiam rau siab - qhov kub ntawm cov qauv thiab cov khoom siv siab.
Vim li cas titanium ntxiv rau 1.4878?
Titanium sib xyaw ua ke nyiam nrog cov pa roj carbon, tiv thaiv chromium carbide nag lossis daus ntawm cov ciam teb hauv thaj tsam 425-900 degree. Qhov no tiv thaiv corrosion tsis kam tom qab vuam thiab thaum lub sij hawm siab - qhov kub thiab txias kev pab cuam, uas tsis ruaj khov qib yuav poob los ntawm rhiab heev.
Qhov siab tshaj plaws ua haujlwm kub ntawm 1.4878 yog dab tsi?
Oxidation kuj tuav mus txog 900℃hauv kev pabcuam cuam tshuam thiab 925℃hauv kev pabcuam txuas ntxiv. Rau kev thauj khoom-cov kabmob, qhov tso cai rau kev ntxhov siab ntawm qhov kub thiab txias yuav tsum raug coj los ntawm EN tsim qauv code tsis yog qhov txwv oxidation.
Yog 1.4878 weldable?
Yog lawm. Siv stabilized los yog txuam muab tub lim, feem ntau ntawm 321H los yog 347 tsev neeg, nrog rau ib txwm austenitic welding tsis. Tsis muaj kev tshaj tawm -weld cua sov yuav tsum tau kho, txawm hais tias lub welded tivthaiv qhov kev pab cuam kub thiab load yuav tsum tau txiav txim siab nyob rau hauv tsim.