316 Stainless hlau vs 17-4 PH: Kev sib xyaw, Lub zog thiab Corrosion
Aug 01, 2025
Tso lus
Ob Tsev Neeg Stainless Hlau sib txawv
316 stainless hlau thiab 17-4 PH stainless hlau ob qho tib si cia siab rau chromium rau corrosion kuj, tab sis lawv yog cov tsev neeg metallurgical sib txawv thiab tau teev tseg rau cov dej num sib txawv kiag li. 316 yog molybdenum-bearing qib austenitic: nws tsis yog - sib nqus nyob rau hauv lub annealed mob, tsis tuaj yeem ua rau kev kho cua sov, thiab tsis tuaj yeem ua kom tawv nqaij, thiab tsis tuaj yeem ua kom tawv nqaij. corrosion nyob rau hauv ib puag ncig chloride-cov kabmob.
17-4 PH yog martensitic nag lossis daus- qib hardening, kuj tau xaiv AISI 630 lossis DIN 1.4542. Nws nqa cov tooj liab ua ke nrog niobium ntxiv rau tantalum, thiab cov ntsiab lus no tsim cov dej nag zoo thaum lub sij hawm qis -kub kev laus, nce lub zog mus rau qib uas tsis muaj qib austenitic tuaj yeem ncav cuag. Kev lag luam tawm yog ib qho leaner npib tsib xee thiab molybdenum cov ntsiab lus, thiab yog li qis dua kev tiv thaiv corrosion.
Txoj cai xaiv luv luv: xaiv 316 thaum ib puag ncig yog qhov teeb meem ntawm kev tswj hwm, thiab xaiv 17-4 PH thaum lub tshuab thauj khoom yog qhov teeb meem tswj hwm thiab ib puag ncig tsuas yog me me lossis nruab nrab corrosive.
Chemical Composition piv (wt%)
Qhov sib txawv ntawm qhov sib txawv yog molybdenum: 316 muaj 2.0 txog 3.0% Mo, thaum 17-4 PH tsis muaj. Hauv kev sib pauv, 17-4 PH nqa 3.0 txog 5.0% tooj liab thiab 0.15 txog 0.45% niobium ntxiv rau tantalum, cov ntsiab lus muaj lub luag haujlwm rau nag lossis daus hardening.
| Element | 316 Stainless hlau | 17-4 PH Stainless hlau |
|---|---|---|
| Chromium (Cr) | 16.0 - 18.0 | 15.0 - 17.5 |
| Nickel (Ni) | 10.0 - 14.0 | 3.0 - 5.0 |
| Molybdenum (hli) | 2.0 - 3.0 | - |
| Cov pa roj carbon (C) | Tsawg dua los yog sib npaug li 0.08 | Tsawg dua lossis sib npaug li 0.07 |
| Manganese (Mn) | Tsawg dua lossis sib npaug li 2.00 | Tsawg dua lossis sib npaug li 1.00 |
| Silicon (Si) | Tsawg dua lossis sib npaug li 1.00 | Tsawg dua lossis sib npaug li 1.00 |
| Phosphorus (P) | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.040 |
| Sulfur (S) | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 0.030 |
| Copper (Cu) | - | 3.0 - 5.0 |
| Niobium + Tantalum (Nb + Ta) | - | 0.15 - 0.45 |
Mechanical Properties muab piv
Tus nqi rau 17-4 PH yog hais rau H900 nag lossis daus-tawv tawv, uas yog tom qab kev laus ntawm 480℃(900℃F). 316 qhov tseem ceeb yog qhov tsawg kawg nkaus uas yuav tsum tau muaj rau cov khoom annealed.
| Khoom | 316 Stainless hlau | 17-4 PH Stainless hlau (H900) |
|---|---|---|
| Tensile zog | Ntau dua lossis sib npaug rau 515 MPa (75 ksi) | Ntau dua lossis sib npaug rau 1170 MPa (170 ksi) |
| Yield zog, 0.2% offset | Ntau dua lossis sib npaug rau 205 MPa (30 ksi) | Ntau dua lossis sib npaug rau 1030 MPa (150 ksi) |
| Elongation nyob rau hauv 50 mm | Ntau dua lossis sib npaug li 40% | Ntau dua lossis sib npaug li 10% |
| Hardness, Rockwell C | Tsawg dua lossis sib npaug li 22 HRC | 40 - 45 HRC |
| Modulus ntawm elasticity | ~ 193 GPa (28 × 106psi) | ~ 200 GPa (29 × 106psi) |
Lub zog sib txawv yog kwv yees li ib feem ntawm ob ntawm lub zog tensile thiab ib qho ntawm tsib hauv lub zog tawm los. Qhov tseem ceeb sib npaug, 17-4 PH poob ductility: yam tsawg kawg nkaus elongation poob los ntawm 40% hauv 316 txog 10% hauv H900 mob.
Lub cev muaj zog piv
| Khoom | 316 Stainless hlau | 17-4 PH Stainless hlau |
|---|---|---|
| Qhov ntom | 8.0 g / cm33 | 7.75 g / cm33 |
| Melting point | 1370 - 1398℃(2500 - 2550℃F) | 1427 - 1538℃(2600 - 2800℃F) |
| Thermal conductivity ntawm 20 degree | 16.2 W/(m·K) | 15.1 W/(m·K) |
| Tshwj xeeb kub muaj peev xwm ntawm 20 degree | 0.50 J/(g·K) | 0.46 J/(g·K) |
| Coefficient ntawm thermal expansion, 20 - 100 degree | 16.0 × 10-6/ degree | 10.8 × 10-6/ degree |
| Hluav taws xob resistivity | 74 × 10-8 Ω·m | 80 × 10-8 Ω·m |
Qhov qis dua thermal expansion ntawm 17-4 PH yog qhov zoo dua nyob rau hauv kev sib dhos precision, thaum qhov kev nthuav dav ntau dua ntawm 316 yuav tsum tau tso cai rau thaum cov khoom siv austenitic tau koom nrog cov hlau ntawm qhov kub siab.
Corrosion Resistance, Thaum tshav kub kub kev kho mob thiab tej yam kev siv
Vim tias 17-4 PH tsis yog alloyed nrog molybdenum thiab nqa cov nickel tsawg dua, nws cov corrosion kuj yog qis dua li ntawm 316, thiab kom meej meej qis dua li cov pa roj carbon tsawg 316L. 17-4 PH tseem tuaj yeem ua haujlwm me me mus rau nruab nrab corrosive ib puag ncig, tab sis aggressive chloride los yog cov kev pab cuam ntxiv rau cov kua qaub.
Kev kho cua sov yog qhov kev txiav txim siab thib ob . 316 yog muab los ntawm annealed, tsis tuaj yeem ua kom tawv nqaij los ntawm kev kho cua sov, thiab tsuas yog tuaj yeem ntxiv dag zog los ntawm kev ua haujlwm txias . 17-4 PH yog cov tshuaj annealed thiab tom qab laus laus, thiab qhov kub ntawm qhov kev laus teeb tsa lub zog thiab toughness sib npaug: H900 muab lub zog siab tshaj plaws, thaum muaj kev kub ntxhov siab xws li H102 thiab H102.
316 stainless hlau: cov khoom siv tshuaj, cov khoom siv hauv hiav txwv thiab sab nrauv, cov khoom noj thiab dej haus, cov kav dej tshuaj, cov vaj tsev vaj tsev.
17-4 PH stainless hlau: aircraft thiab aerospace Cheebtsam, siab- lub zog ncej thiab lub zog, valve stems thiab trim, twj tso kua mis qhov chaw, precision industrial khoom, high-strength fasteners.
Cov ntaub ntawv khoom kuj txawv . 316 yog muaj xws li phaj, ntawv, coil, bar, raj thiab yeeb nkab nyob rau hauv ib tug dav loj ntau yam, thaum 17-4 PH yog ib txwm muab raws li phaj, bar thiab forging Tshuag, nrog phaj thickness feem ntau khiav ntawm li 3 hli mus rau 100 hli.
Cov lus nug nquag
Q: Qib twg muaj zog dua, 316 lossis 17-4 PH?
17-4 PH muaj zog dua. Nyob rau hauv cov xwm txheej H900 nws yuav tsum muaj qhov tsawg kawg nkaus tensile lub zog ntawm 1170 MPa thiab qhov tsawg kawg nkaus yield zog ntawm 1030 MPa, tiv thaiv 515 MPa thiab 205 MPa rau annealed 316 stainless hlau.
Q: Puas yog 17-4 PH ntau dua corrosion resistant dua 316?
Tsis yog. Tsis muaj molybdenum thiab nrog ntau cov npib tsib xee qis, 17-4 PH muaj kev tiv thaiv corrosion tsawg dua 316 thiab 316L. Nws ua tau zoo tsuas yog nyob rau hauv me me los yog nruab nrab corrosive tej yam kev mob.
Q: Dab tsi yog qhov sib npaug ntawm 17-4 PH stainless hlau?
Qhov sib npaug siv dav tshaj plaws yog AISI 630 thiab DIN 1.4542, ob qho tib si piav qhia txog nag lossis daus -hardening chromium-nickel- tooj liab stainless hlau nrog cov khoom sib piv.
Q: 316 stainless hlau puas tuaj yeem ua kom tawv los ntawm kev kho cua sov?
Tsis yog . 316 yog austenitic thiab tsis tuaj yeem hardened los ntawm kev kho cua sov; nws tsuas tuaj yeem muaj zog los ntawm kev ua haujlwm txias, uas kuj ua rau nws sib nqus me ntsis.
Q: Ua li cas qhov kev laus kub hloov 17-4 PH zog?
Kev kub siab kev laus txo lub zog thiab hardness thaum nce ductility thiab cuam tshuam toughness. H900 muab lub zog siab tshaj plaws, thaum H1025 thiab H1150 raug xaiv thaum muaj zog lossis kev ntxhov siab- tus cwj pwm corrosion tseem ceeb dua.
Q: Ua li cas 17-4 PH piv nrog 410 stainless hlau?
17-4 PH muaj ntau cov chromium thiab ntau npib tsib xee dua li 410 stainless hlau, yog li nws muaj kev tiv thaiv corrosion zoo dua thiab muaj zog ntau dua thiab hardness tom qab laus.
Xa kev nug