Dab tsi yog qhov sib txawv ntawm 304 thiab 1.4401?

Aug 04, 2025

Tso lus

Dab tsi qib yog 1.4401 cov khoom siv?

Rau 1.4401 qib 316 Chromium Hlau (16% Chromium, 10% Molybdenum thiab ntau dua Codrosion tsis kam muab piv rau 304.

Cov khoom siv twg yog sib npaug rau 304?

Hom stainless hom 1.4301 thiab 1.4307 tseem hu ua qib 304 thiab 304L feem. Hom 304 yog qhov ntau tshaj plaws thiab dav siv stainless hlau.

Key Differences Between 304 And 1.4401

 

Qhov sib txawv ntawm 304 thiab 1.4401

Tshuaj Muaj Tshuaj

Lub ntsiab 304 (ASTM) 1.4401 (en)
Chromium (cr) 18.0–20.0% 16.0–18.0%
Npib tsib caug (ni) 8.0–10.5% 10.0–14.0%
Carbon (c) Tsawg dua los yog sib npaug rau 0.08% Tsawg dua los yog sib npaug rau 0.07%
Manganese (mn) Tsawg dua los yog sib npaug rau 2.0% Tsawg dua los yog sib npaug rau 2.0%
Silicon (si) Tsawg dua los yog sib npaug rau 0.75% Tsawg dua los yog sib npaug rau 1.0%
Molybdenum (mo) 0% (tsis tas yuav tsum) 2.0–3.0%

Cov Khoom Siv Neeg Kho Tshuab

Ntiag tug 304 (ASTM) 1.4401 (en)
Lub zog tensile Ntau dua los yog sib npaug rau 515 MPa Ntau dua los yog sib npaug rau 520 mpa
Paib lub zog Ntau dua los yog sib npaug rau 205 MPa Ntau dua los yog sib npaug rau 200 MPa
Elongation Ntau dua los yog sib npaug rau 40% Ntau dua los yog sib npaug rau 40%
Hardness (HBW) Tsawg dua los yog sib npaug rau 201 Tsawg dua los yog sib npaug rau 210

 

Corrosion Kuj
304 Stainless hlau muaj kev tiv thaiv zoo heev rau atmospheric corrosion, thiab cov tshuaj tsis huv (xws li cov acids me me). Txawm li cas los xij, nws tuaj yeem sau lossis corrosion hauv siab- cov chaw dej hiav txwv, pas dej hiav txwv, lossis chlorinated Industers tshuaj ntxuav).
1.4401 Stainless hlau, vim nws cov ntsiab lus molybdenum, muaj cov ntsiab lus tseem ua rau chloride corrosion, pitting, thiab cov nyom corrosion. Nws ua tshwj xeeb hauv cov av marine chaw, siv tshuaj lom neeg, lossis ib daim ntawv thov nrog ntsev, brine, lossis cov neeg sawv cev tawv nqaij tawv.

 

Yog 1.4301 stainless hlau sib nqus?
304 Austenic cov qauv hlau, tseem hu ua "AISI 304 hlau" lossis 1.4301, feem ntau tsis- sib nqus.

 

Yog 1.4401 sib nqus?

Cov 1.4401 (X5Cnimo17 - 12-2) steel yog qhov zoo tagnrho, ua tsaug rau nws cov kev ua kom kub siab, thiab cov yam ntxwv tsis tshua muaj zog.

 

Yog 1.4401 tib yam li 316?
Yog lawm, 1.4401 yog qhov ua tau zoo sib npaug ntawm Astm 316. Ob leeg muaj Molybdenum thiab muaj kev ua tau zoo sib xws.


Tau 304 thiab 1.4401 tau welded ua ke?
Yog lawm, tab sis siv cov tub rog sib zog sib xws nrog ob qho tib si (piv txwv li, ER316L) kom tswj hwm corrosion tsis kam nyob hauv Weld.


Qhov twg zoo dua rau kev siv sab nraum zoov?
Nws nyob ntawm qhov chaw . 304 ua haujlwm hauv cov chaw qhuav, hauv thaj chaw; 1.4401 yog qhov zoo dua rau cov cheeb tsam ntug hiav txwv muaj kev nyab xeeb nrog cov pa phem.

 

Dab tsi yog qhov sib txawv ntawm 1.440 thiab 1.4404?

En 1.4401 (316) piv rau txhua 1.440 (316L)
Lub ntsiab sib txawv ntawm ob qib no nyob hauv lawv cov ntsiab lus carbon. Rau 1.4401 muaj ntau dua cov pa roj carbon ntau dua, ua rau nws pheej yig dua rau kev pheej hmoo ntawm kev kub ntxhov, thaum en 1.4404 muaj zoo dua vuam cov ntsiab lus vim nws cov ntsiab lus muaj roj carbon ntau zoo dua.