Dab tsi yog qhov txawv ntawm 1.4301 thiab 1.4310 stainless hlau?
Sep 21, 2026
Tso lus
Yog tias koj tab tom nrhiav High-Strength Springs, Railway Panels, Los Txias-Formed Structural Parts, 1.4310 (AISI 301) yog koj qib. Yog tias koj xav tau Corrosion Resistance, Weldability, Thiab General-Lub Hom Phiaj Fabrication rau cov khoom noj, tshuaj, lossis kev siv vaj tse, 1.4301 (AISI 304) yog qhov kev lag luam default. Ob leeg yog austenitic chromium-nickel stainless hlau, tab sis lawv cov ntsiab lus carbon thiab npib tsib xee tsim muaj zog sib txawv, corrosion, thiab cov nqi profile. Phau ntawv qhia no muab cov ntaub ntawv rau koj los txiav txim siab yuav khoom zoo.
Stainless hlau qib 1.4301 yog dab tsi?
Qib 1.4301 (X5CrNi18-10, EN 10088) yog European tus qauv austenitic stainless hlau sib npaug rau AISI 304 / UNS S30400 thiab JIS SUS304. Nws muaj 17.5%–19.5% chromium (Cr) thiab 8.0%–10.5% npib tsib xee (Ni) (nrog cov ntsiab lus carbon C tsawg dua lossis sib npaug li 0.07%); Nws muaj qhov ceev ntawm 7.9 g / cm³, lub zog tawm los ntawm tsawg kawg yog 210 MPa, lub zog tensile ntawm 520 thiab 720 MPa, thiab Pitting Resistance Equivalent Number (PREN) ntawm kwv yees li 18-20. Renowned rau nws zoo heev formability, weldability, thiab zoo corrosion kuj, nws yog dav siv nyob rau hauv sectors xws li tshuaj lom neeg kev lag luam, zaub mov ua, thiab kev tsim kho.
Dab tsi yog 1.4310 stainless hlau sib npaug?
Qib 1.4310 (X10CrNi18-8, EN 10088) yog siab-lub zog, caij nplooj ntoos hlav{20}}qib austenitic stainless hlau sib npaug rau AISI 301 / UNS S30100, JIS SUS301, thiab 7 GBNi2 Muaj 16.0%–18.0% chromium (Cr) thiab 6.0%–9.0% npib tsib xee (Ni) (nrog cov ntsiab lus carbon ntawm 0.05%–0.15%), qib no tau ua haujlwm tseem ceeb thaum lub caij txias deformation; qhov no nce nws lub zog tensile los ntawm 600-800 MPa hauv cov tshuaj -annealed xeev mus rau 2000 MPa nyob rau hauv lub caij nplooj ntoos hlav-hardened xeev, ua rau nws yog ib tug zoo tagnrho cov khoom rau manufacturing precision springs, fasteners, thiab high-lub zog Cheebtsam.
1.4301 vs . 1.4310 Stainless hlau: Qhov txawv ntawm qhov tseem ceeb
| 1.4301 | 1.4310 | |
| EN npe | X5CrNi18-10 | X10CrNi18-8 |
| US sib npaug | AISI 304 / UNS S30400 | AISI 301 / UNS S30100 |
| Cov pa roj carbon | Tsawg dua lossis sib npaug li 0.07% | 0.05 – 0.15 % |
| Nickel | 8.0 – 10.5 % | 6.0 – 8.0 % |
| Thawj Lub Zog Mechanism | Alloying | Txias ua hauj lwm hardening |
| Zoo tshaj rau | Vuam, corrosion, khoom noj khoom haus | Springs, siab - zog tsim |
| 2026 Indicative Nqe | $2.20 - $3.50 / kg | $0.99 – $3.50 / kg |
1.4301 vs . 1.4310 Stainless hlau: Tshuaj muaj pes tsawg leeg
| Element | 1.4310 (EN 10088-1) | 1.4301 (EN 10088-1) |
| C | 0.05 – 0.15 | Tsawg dua los yog sib npaug li 0.07 |
| Cr | 16.0 – 18.0 | 17.5 – 19.5 |
| Ni | 6.0 – 8.0 | 8.0 – 10.5 |
| Mn | Tsawg dua los yog sib npaug rau 2.0 | Tsawg dua los yog sib npaug rau 2.0 |
| Si | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug rau 1.0 |
| P | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.045 |
| S | Tsawg dua lossis sib npaug li 0.015 | Tsawg dua lossis sib npaug li 0.015 |
| N | Tsawg dua lossis sib npaug li 0.10 | Tsawg dua lossis sib npaug li 0.11 |
| Mo | – | – |
1.4301 vs . 1.4310 Stainless hlau: Mechanical Properties
Lub caij txias - ua haujlwm 1.4310 caij nplooj ntoos hlav tuaj yeem ua tau zoo tshaj qhov kev sib koom ua ke ntawm 1.4301 tus tswv cuab los ntawm 40-60 % hauv cov khoom muaj zog thaum khaws cov ductility txaus rau kev thauj khoom cyclic.
| Khoom | 1.4310 Nws | 1.4310 Txias-Ua haujlwm (H) | 1.4301 Ib |
| Tensile zog (MPa) | 600 – 950 | 950 – 1,200 | 500 – 700 |
| Yield zog (MPa) | 240 – 350 | 700 – 1,000+ | 210 – 310 |
| Elongation (%) | 40 – 50 | 15 – 25 | 45 – 55 |
| Hardness (HV) | Tsawg dua los yog sib npaug li 220 | 300 – 400+ | Tsawg dua los yog sib npaug li 200 |
| Modulus ntawm Elasticity (GPa) | ~193 | ~193 | ~193 |
| Qhov ceev (g / cm³) | 7.9 | 7.9 | 7.9 |
1.4310 vs . 1.4301 stainless hlau: Corrosion Resistance
Ob qib tiv thaiv atmospheric, dej tshiab, thiab qaug zog acid/alkali ib puag ncig. Qhov sib txawv widens nyob rau hauv peb scenarios:
| Scenario | 1.4310 (301) | 1.4301 (304) |
| Sab nraum zoov / ntub | Zoo, tej zaum yuav qhia nto staining ntau xyoo | Zoo heev, ntev - lub sij hawm ruaj khov |
| Welded pob qij txha (HAZ) | Kev pheej hmoo siab ntawm intergranular corrosion(C> 0.1% sensitizes Cr carbides) | Kev pheej hmoo tsawg (C Tsawg dua lossis sib npaug li 0.07%) |
| Chloride / dej hiav txwv | Ncaj ncees - tsis pom zoo | Zoo – tseem tsis marine -qib (siv 316) |
| High-temperature (>400 degree) | Oxidation kuj degrades sai dua | ruaj khov mus txog ~ 870 degree |
1.4310 vs . 1.4301 stainless hlau: Vuam xav txog
| Qhov xwm txheej | 1.4310 | 1.4301 |
| Weldability | Zoo, tab sis tom qab -weld annealing (1010-1100 degree) pom zoo kom rov qab ua kom corrosion | Zoo heev, tsis muaj PWHT xav tau rau kev pabcuam feem ntau |
| Txaus ntshai | Intergranular corrosion ntawm HAZ (C rhiab heev) | Tsawg kawg |
| Pom zoo muab tub lim | 1.4307 (304L) lossis 1.4316 (316L) | 1.4301 / 1.4307 |
| Ua ntej - cua sov | Tsis xav tau | Tsis xav tau |
Qhov txawv ntawm 1.4301 thiab 1.4305 yog dab tsi?
1.4301 (AISI 304) yog tus qauv austenitic stainless hlau (sulfur ntsiab lus S < 0.030%), whereas 1.4305 (AISI 303) yog dawb- qib machining tsim los ntawm kev txhob txwm ntxiv ntawm sulfur (S cov ntsiab lus 0.15–0.35%). Ob leeg muaj kwv yees li 17.5-19.5% chromium (Cr) thiab 8.0-10.5% nickel (Ni). Txawm hais tias 1.4305 muab cov nti zoo dua qub-cov yam ntxwv tawg thiab kev ua haujlwm nrawm thaum lub sijhawm CNC tig, nws cov ntsiab lus sulfur ntau dua txo cov ductility, weldability, thiab pitting corrosion kuj (PREN yog kwv yees li 17, piv rau 18-20 rau 1.4301).
Qhov txawv ntawm 1.4301 thiab 1.4307 yog dab tsi?
1.4301 (AISI 304) muaj tus qauv carbon cov ntsiab lus (C < 0.07%), thaum 1.4307 (AISI 304L) yog nws qis -carbon variant (C Tsawg dua lossis sib npaug li 0.030%). Ob leeg sib koom ua ke tib lub zog (lub zog tensile Rm ntawm 520-720 MPa) thiab dav corrosion kuj (Cr 17.5-19.5%, Ni 8.0-10.5%). Cov pa roj carbon tsawg hauv 1.4307 tiv thaiv chromium carbide nag lossis daus thaum lub sijhawm vuam, yog li tshem tawm cov kev nyiam rau intergranular corrosion nyob rau hauv tshav kub- cuam tshuam cheeb tsam (HAZ) thiab tshem tawm qhov xav tau tom qab-weld tov annealing.
Qhov txawv ntawm 1.4301 thiab 1.4016 yog dab tsi?
1.4301 (AISI 304) yog cov hlau tsis muaj - hlau nplaum austenitic nrog lub zog tawm los tshaj 210 MPa, thaum 1.4016 (AISI 430) yog npib tsib xee-cov hlau tsis muaj ferritic uas yog ib txwm muaj ferromagnetic thiab muaj 60 MPa zog tshaj 2. Vim tias tsis muaj npib tsib xee, 1.4016 tus nqi kwv yees li 25% -35% tsawg dua thiab tiv thaiv chloride kev nyuaj siab corrosion tawg; Txawm li cas los xij, nws yog qhov qis dua rau 1.4301 nyob rau hauv cov nqe lus ntawm kev sib sib zog nqus- kos duab, weldability, thiab pitting corrosion kuj.
Qhov txawv ntawm 1.4310 thiab 1.4311 yog dab tsi?
1.4311 (AISI 301L) yog qhov qis -carbon variant ntawm 1.4310 (C Tsawg dua lossis sib npaug rau 0.035 %). Nws muaj lub zog qis dua tab sis zoo dua weldability thiab corrosion kuj dua li tus qauv 1.4310. Yog tias koj xav tau 301's formability nrog 304-zoo li weldability, qhia 1.4311.
1.4310 vs . 1.4301 Stainless hlau: Daim ntawv thov
1.4301 (AISI 304): Cov khoom siv ua zaub mov, vaj huam sib luag vaj huam sib luag, chemical cia tanks, chav ua noj, thiab dav dav - lub hom phiaj kav.
1.4310 (AISI 301): Mechanical springs, retaining rings, clips, precision stamped parts, and structural components that need high yield strength.
1.4310 vs . 1.4301 stainless hlau: Nqe (2026 Indicative, FOB Tuam Tshoj)
| Qib | Daim ntawv | Tus nqi ntau (USD / kg) | Sau ntawv |
| 1.4310 | Kub-rolled phaj | $2.10 – $3.40 | 3-50 hli, No.1 tiav |
| 1.4310 | Txias- yob daim ntawv | $2.50 – $4.20 | 0.3-6 hli, 2B |
| 1.4310 | Daim iav / BA | $3.00 – $6.50 | 8K lossis Bright Annealed |
| 1.4301 | Kub-rolled phaj | $2.20 – $2.60 | 6-20 hli feem ntau yig |
| 1.4301 | Txias- yob daim ntawv | $2.50 – $3.00 | 2B tiav |
| 1.4301 | Txiav daim ntawv (me me) | $2.80 – $3.50 | Service center nqi |
301 feem ntau yog15-20% pheej yig duatshaj 304 vim qis Ni cov ntsiab lus. Cov nqi hloov pauv nrog LME npib tsib xee. Thov tam sim no quotes rau ntim xaj.
GNEE Cov Qauv Khoom: 1.4301 (304) 1.4310 (301) specification
| Yam khoom | 1.4301 (304) | 1.4310 (301) |
| Cov khoom lag luam | Ntawv, phaj, coils, strips | Daim kab xev (Cold Rolled), Daim Ntawv |
| Cov khoom siv ntev | Round Bars, Flat Bars, Angles | Caij nplooj ntoos hlav hlau, tshwj xeeb tuav |
| Tube & Tubes | Seamless & Welded Yeeb Nkab | Tsis tshua siv (tsis txheem) |
| Mechanical Parts | Flanges, Fittings, Fasteners | Springs, Clips, Washers |
| Cov khoom siv hlau | Vuam Hlau | High-Tensile Caij Nplooj Hlav Hlau |