Feb 24, 2026
Tso lus



Cov khoom sib npaug ntawm 440 Stainless Hlau Phaj
440A Stainless hlau:
Sib npaug rau AISI 440A, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS 5634, 82 AMS, SAE J405 (51440A) UA
Cov qib zoo sib xws: 7Cr17, 7Cr17MoV, X70CrMo15
440B Stainless hlau:
Sib npaug rau AISI 440B, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS 5634, 82 AMS, SAE J405 (51440B)
Cov qib zoo sib xws: 9Cr18, 9Cr18Mo, X90CrMoV18
440C Stainless hlau:
AISI 440C, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5630, AMS 5880, MIL-S-862, 5 SAE J405 ()
Cov qib zoo sib xws: 9Cr18MoV, X105CrMo17
440 Stainless Hlau Phaj Chemical Composition (%)
| Qib | C | Si | Mn | S | P | Cr | Ni | Mo |
|---|---|---|---|---|---|---|---|---|
| 440A | 0.60~0.75 | Tsawg dua los yog sib npaug li 1 | Tsawg dua los yog sib npaug li 1 | Tsawg dua lossis sib npaug li 0.030 |
Tsawg dua lossis sib npaug li 0.040 |
16.00-18.00 | – | Tsawg dua lossis sib npaug li 0.75 |
| 440B | 0.85-0.95 | Tsawg dua los yog sib npaug li 1 | Tsawg dua los yog sib npaug li 1 | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 0.035 | 16.00-18.00 | Tsawg dua lossis sib npaug li 0.60 | Tsawg dua lossis sib npaug li 0.75 |
| 440C | 0.95 – 1.20 | Tsawg dua los yog sib npaug li 1 | Tsawg dua los yog sib npaug li 1 | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 0.040 | 16.00-18.00 | – | Tsawg dua lossis sib npaug li 0.75 |
Mechanical Properties
| Khoom | 440A | 440B | 440C |
|---|---|---|---|
| Hardness (Rockwell C) | 56-59 HRC | 57-60 HRC | 58-62 HRC |
| Tensile zog (MPa) | 760-820 | 760-840 | 760-820 |
| Tensile zog (MPa) | 450-600 | 450-600 | 450-600 |
| Elongation ntawm Break (%) | 20-25 | 15-20 | 10-15 |
| Modulus ntawm Elasticity (GPa) | 200 | 200 | 200 |
Lub cev muaj zog
| Khoom | 440A | 440B | 440C |
|---|---|---|---|
| Qhov ceev (g / cm³) | 7.65 | 7.75 | 7.75 |
| Thermal conductivity (W / m · K) | 24 | 24 | 24 |
| Lub peev xwm kub tshwj xeeb (J / kg·K) | 460 | 460 | 460 |
| Hluav taws xob tiv thaiv (μΩ·cm) | 60 | 60 | 60 |
| Coefficient ntawm Thermal Expansion (μm / m·K) | 10.4 | 10.4 | 10.4 |