Dab tsi yog 347 stainless hlau siv rau?
Jul 07, 2025
Tso lus
Dab tsi yog 347 stainless hlau?
347 Stainless HlauYog ib qho ruaj khov rau cov roj stainless hlau tau sib cais nrog Niobium (Columbium), uas txhim kho nws qhov chaw kub (siab tshaj 800 Qib F \/ 425 Degree). Nws yog tshuaj zoo ib yam li 304 tab sis muab tau zoo dua qhov kev kub ntxhov siab, ua rau nws zoo tagnrho rau kev kho cua sov, ib qho chaw ua haujlwm, thiab tshuaj xyuas ib puag ncig.
Tus lej tsis yog: S34700
Sib npaug rau: 1.4550 (EN), X6CrNiNb18-10 (DIN), ASTM A240 \/ A213 \/ A182
Dab tsi yog 347 stainless hlau siv rau?
347 Stainless hlau tau siv dav hauv kev lag luam uas yuav tsum muaj lub zog kub, xeb tsis kam, thiab weldability heev. Cov ntawv thov feem muaj xws li:

Muaj & Kev Kub Ntxov Kub:
Kev hloov pauv kub thiab cov superheaters
Boiles Tubes
Cov khoom siv hluav taws xob
Qhov Chaw Ua Si Thiab Radiant Tube
Tshuaj Yeeb Nkab Piping
Aerospace & aviation:
Dav hlau cav Cheebtsam
Tso manifolds
Airccraft pa taws


Lub zog tiam & roj \/ roj:
Kev ntsuas cov cheeb tsam
Reformer Tube
Cov hlab ntsha thiab reactors
Siv Welded Welded Qauv:
Welded Tso Tsheb Hlau Luam Thiab Cov Piping Tshuab
Cov pob qij txha nthuav dav
Flanges thiab fittingsNyob rau hauv cov kev pab kub-kub

Tshuaj Muaj Tshuaj
| Tshuaj lom neeg siv tshuaj lom neeg txwv | ||||||||||||
| Nyhav%% | C | P | Si | Ni | Mn | S | Cr | CB + TA | Zaum fe | Co las | Mo | CU |
| 347 | 0. 08 Max | 0. 040 Max | 1. {00 max | 9-12 | 2. {0 max | {{0 {}}. 030 Max | 17-19 | 10 x c min | Tus liab | 1. {00 max Tsuas yog Ams 5646 |
0. 75 max | 0. 75 max |
| 347H | 0.04-0.10 | 0. 040 Max | 1. {00 max | 9-12 | 2. {0 max | {{0 {}}. 030 Max | 17-19 | 10 x c min | Tus liab | |||
Cov Khoom Siv Neeg Kho Tshuab
| Khoom | Paib muaj zog (ksi) | Tensile lub zog (ksi) | % Elongation% | Hardness Hb |
| Alloy 347 Ntawv (Sol Trtd) Ams 5512 |
25 | 70-105 | 40 | - |
| Alloy 347 Bar (sol trtd) Ams 5646 |
- | - | - | 255 Max |
Kev Zoo Tshaj Plaws ntawm 347 Stainless Hlau
| Ntiag tug | Kev piav txog |
|---|---|
| Kub-Kub Kuj | Muaj lub zog ntawm lub zog ntawm 870 degree (1600 degree f) |
| Ruaj khov tawm tsam carbide tsim | Niobium tiv thaiv intergranular corrosion tom qab vuam |
| ZOO TXHUA YAM KEV PAB HEEV | Piv rau 304 tab sis zoo dua thaum nce siab Temps |
| Zoo heev Weldability | Haum rau kev siv hauv cov ntaub thaiv tuab los yog cov hlab ntsha siab |
| Corrosion Kuj | Zoo tsis kam rau cov kua qaub thiab atmospheric corrosion |
Xav tau 347 stainless hlau rau koj qhov project siab?
Peb muab347 stainless hlau los xij, hlab, tuav, thiab cov yeeb nkab fittingsNrog: Daim Ntawv Qhia Txog Mill Cov Ntawv Qhia Txog Kev Ntsuas Ntau Lawm (MSTS), txiav-rau-loj thiab kev cai machining
Kev them nyiaj thoob ntiaj teb thiab kev txhawb nqa!
Cov qauv khoom ntawm 347 stainless hlau
Seamless thiab welded kav (Astm A312 \/ A213)
Cov ntawv thiab daim hlau (ASTM A240)
Cov tuav thiab kev lom zem (Astm A182)
Hlau thiab cov tub lim hlau (AWS ER347 rau VUAM)
Flanges, fittings, luj tshib, tees, reducers
Hu rau peb pab neegNiaj hnub no los thov cov lus hais lossis hais lus nrog tus kws ua choj.