316L UG stainless hlau yog dab tsi?
May 09, 2026
Tso lus
316L UG stainless hlau yog dab tsi?
316L UG (Urea Qib) yog ib qho tshwj xeeb, qis -carbon "hloov" variant ntawm 316L stainless hlau, tshwj xeeb yog tsim los rau urea ntau lawm ib puag ncig (ie, urea-carbamate tov ib puag ncig). Nws feem ntau tswj hwm lub microstructure tag nrho austenitic nrog cov ntsiab lus ferrite tsawg heev (tsawg dua lossis sib npaug li 0.5% - 0.6%) kom tiv thaiv kev cuam tshuam intergranular. Nws yog tsim tshwj xeeb rau cov cuab yeej tseem ceeb hauv urea ntau lawm cov nroj tsuag (xws li siab -siab strippers thiab kub exchangers).
Dab tsi yog cov khoom sib npaug rau SS 316L UG?
316L Urea Qib (UG) stainless hlau (feem ntau hu ua 316LUG lossis 316LMod) yog tsim tshwj xeeb los muab kev tiv thaiv corrosion siab hauv urea - carbonate ib puag ncig. Nws qhov sib npaug ze tshaj plaws yog EN 1.4435 tseem hu ua hloov kho 316L UG steel thiab hauv cov ntawv thov tshwj xeeb, cov khoom siv no ua tau zoo tshaj tus qauv 316L stainless hlau.
Puas yog 1.4435 thiab 316L UG tib yam?
1.4435 yog qib stainless hlau txhais raws li European Standards (EN). Txawm hais tias nws cov tshuaj muaj pes tsawg leeg zoo sib xws nrog cov kev cai rau Urea Qib (UG) daim ntawv thov tshaj li tus qauv 316L (1.4404), tsis yog tag nrho cov khoom siv 1.4435 tuaj yeem raug xaiv los ua 316L UG.
SS 316L UG Chemical Composition
| Lub ntsiab | 316L UG (Typical wt.%) |
| Cov pa roj carbon (C) | Tsawg dua los yog sib npaug rau 0.020 |
| Manganese (Mn) | Tsawg dua lossis sib npaug li 2.00 |
| Silicon (Si) | Tsawg dua lossis sib npaug li 0.40 |
| Phosphorus (P) | Tsawg dua los yog sib npaug rau 0.020 |
| Sulfur (S) | Tsawg dua lossis sib npaug li 0.010 |
| Chromium (Cr) | 17.0 – 18.5 |
| Nickel (Ni) | 13.0 – 15.0 |
| Molybdenum (hli) | 2.20 – 3.00 |
| Nitrogen (N) | 0.10 – 0.16 |
| Hlau (Fe) | Tshuav |
Mechanical Properties (ntawm chav tsev kub)
| Khoom | Metric nqi | Imperial nqi |
| Tensile zog, min. | 485 MPa ua | 70 ksg |
| Yield zog (0.2%), min. | 190 MPa rau | 27, 5 tzs |
| Elongation (L0=50mm), min. | 40% | 40% |
| Hardness (Brinell), max. | 190 HWB | - |
| Hardness (Rockwell B), max. | 90 PAB | - |
Corrosion Resistance ntawm 316L UG Stainless hlau
Lub corrosion kuj ntawm 316L UG (Urea Qib) stainless hlau yog tshwj xeeb engineered nrog nruj me ntsis tswj cov ntsiab lus ferrite tuav nyob rau hauv ib theem ntawm tsawg tshaj li los yog sib npaug rau 0.6% (feem ntau tsawg tshaj li los yog sib npaug rau 0.5%) yog li xyuas kom muaj ib tug tag nrho austenitic microstructure uas zoo tiv thaiv corrosion. Nws yog tsim los tiv thaiv cov kev khiav hauj lwm hnyav heev uas tau ntsib thaum lub sij hawm urea ntau lawm, ib puag ncig uas tus qauv 316L stainless hlau feem ntau yuav ua tsis tau.
Dab tsi yog qhov txawv ntawm 316L thiab 316L urea qib?
316L Urea Qib (316L UG / 316Lmod) yog ib qho tshwj xeeb, "kev cai- hloov kho dua tshiab" txawv ntawm tus qauv 316L stainless hlau, tsim tshwj xeeb kom ua tau raws li qhov xav tau ntawm huab cua corrosion kuj ntawm urea ntau lawm ib puag ncig. Nws txawv ntawm tus qauv 316L los ntawm cov ntsiab lus ntawm silicon qis (< 0.5%), a higher molybdenum content (>2.5%), thiab cov ntsiab lus ferrite tsis tshua muaj thiab nruj heev (< 0.5%), all designed to effectively prevent urea-carbonate corrosion.
Dab tsi yuav tsum tau ceev faj thaum vuam 316L UG?
Nws yog ib qho tseem ceeb uas yuav tsum xaiv cov urea sib xws - qib vuam khoom siv (xws li hloov kho ER316L lossis tshwj xeeb urea- qib vuam electrodes) kom ntseeg tau tias cov ntsiab lus ferrite ntawm cov hlau vuam zoo sib xws. Thaum tshav kub kub input yuav tsum tau nruj me ntsis tswj kom tsis txhob muaj nag lossis daus ntawm intermetallic theem (xws li Sigma theem), yog li tsis txhob muaj kev txo qis hauv corrosion kuj.
Dab tsi yog cov khoom siv siv rau 316L UG?
High-Pressure Systems (HP Loop) tshwj xeeb tsim los rau kev lag luam urea:
Cov ntaub ntawv rau Urea Reactors.
Siab -Pressure Condensers.
Siab -Nias Strippers.
Siab -Nias Scrubbers.
316LUG Stainless hlau yeeb nkab Supplier
GNEE muab 316L UG (Urea Grade) stainless hlau kav uas ua tau raws li cov qauv thoob ntiaj teb, suav nrog ASTM A312 (rau cov kav dej seamless), ASTM A213 (rau cov raj xa hluav taws xob), thiab EN 10216-5. Peb muab tag nrho traceability nrog EN 10204 3.1 lossis 3.2 daim ntawv pov thawj, suav nrog kev tshuaj xyuas thib peb los ntawm cov chaw muaj npe nrov xws li BV, TUV, thiab Lloyd's.
| Yam khoom | Specification / Txuj | Size Range (Tswj) |
| Instrumentation Tubing | ASTM A269 / EN 10216-5 | OD: 6.0 - 25.4 hli; WT: 0.5 - 2.11 mm |
| Thaum tshav kub kub Exchanger Tubes | ASTM A213 / ASME SA213 | OD: 12.7 - 38.1 hli; WT: 1.0 - 3.5 mm |
| Txheej Txheem Piping (Seamless) | ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASTM A312 / ASME SA312) | NPS: 1/2" - 12"; Teem sijhawm: 10S, 40S, 80S, XXS |
| Cov kav dej siab | Tus Qauv Tsim Qauv | OD: Txog li 250 hli; WT: Mus txog 40 mm |
Peb cov khoom

ASTM A312 316LUG High Pressure Pipes

ASTM A213 316LUG Heat Exchanger Tubes

ASTM A269 316LUG Instrumentation Tubing
Ntxiv rau cov txheej txheem phab ntsa tuab seamless kav, GNEE muaj nyias -walled heat exchanger/instrumentation tubing nrog rau loj -diameter hnyav- phab ntsa kav. Tsis tas li ntawd, peb muab 'ib- nres' kev daws teeb meem los ntawm kev muab kev sib txuam 316L UG lub luj tshib, tees, flanges, thiab vuam siv tau zoo, tshem tawm cov kev pheej hmoo ntawm cov khoom tsis sib haum ntawm cov khoom sib txawv.