316L Stainless hlau yog dab tsi?

316L yog qhov qis-carbon, molybdenum-cov kabmob austenitic stainless hlau qauv raws li UNS S31603 thiab raws li EN 1.4404, X2CrNiMo17-12-2. Nws cov qauv yog lub ntsej muag-centred cubic austenite: tsis yog{12}}sib nqus nyob rau hauv cov mob annealed, tsis hardenable los ntawm kev kho cua sov, thiab ntxiv dag zog los ntawm txias ua hauj lwm. Qhov 2-3% molybdenum ntxiv yog dab tsi lifts tsis kam rau pitting thiab crevice corrosion nyob rau hauv chloride-cov kabmob xov xwm saum toj no theem ntawm unalloyed-molybdenum 18/8 steels xws li 304.

Stainless hlau raws li ib tsev neeg yog txhais los ntawm chemical stability nyob rau hauv huab cua, dej, kua qaub, alkali thiab ntsev ib puag ncig, thiab chromium khoom uas stability los ntawm kev ua ib tug passive oxide zaj duab xis uas re- cov ntaub ntawv tom qab deg puas tsuaj. Cov ntsiab lus chromium siab dua nce ob qho tib si stain resistance thiab corrosion resistance. 316L khub 16-18% chromium nrog molybdenum thiab 10-14% npib tsib xee, uas nthuav dav ntau yam ntawm cov xov xwm qib tuaj yeem tswj tau thiab ua rau nws haum rau cov khoom siv siab.

Tshuaj muaj pes tsawg leeg thiab cov qauv siv tau

Element ASTM A 240 316 (S31600) ASTM A 240 316L (S31603) TS EN 1.4404
Cov pa roj carbon (C) 0.08 max 0.030 max 0.030 max
Silicon (Si) 0.75 max 0.75 max 0.75 max
Manganese (Mn) max 2.00 Nws max 2.00 Nws max 2.00 Nws
Phosphorus (P) 0.045 max 0.045 max 0.045 max
Sulfur (S) 0.030 max 0.030 max 0.015 max
Chromium (Cr) 16.0-18.0 16.0-18.0 16.5-18.5
Nickel (Ni) 10.0-14.0 10.0-14.0 10.0-13.0
Molybdenum (hli) 2.00-3.00 2.00-3.00 2.00-2.50
Nitrogen (N) 0.10 max 0.10 max 0.10 max

Tus nqi yog feem pua ​​ntawm pawg. Rau kev siv tshuaj, bioprocessing thiab siab -purity dej kev pab cuam, EN 1.4435, X2CrNiMo18-14-3, feem ntau teev es tsis txhob: nws belongs rau tib chemistry tsev neeg nrog nruj txwv nyob rau hauv cov ntsiab lus ferrite ntawm cov weld thiab, nyob rau hauv qis-ferrite zeb versions, ib theem siab dua.

Mechanical Properties

Khoom Yam nqi
Tensile zog, annealed 485 MPa min
0.2% pov thawj muaj zog 170 MPa min
Elongation nyob rau hauv 50 mm 40% min
Qhov ntom 8.00 g / cm3
Modulus ntawm elasticity 193-200 GPa
Pitting kuj sib npaug tus lej txog 24 rau chemistry ib txwm
Nruam kev pabcuam qab nthab cav 425c

Tus lej sib npaug ntawm pitting yog suav tias yog chromium ntxiv rau 3.3 npaug ntawm molybdenum ntxiv rau 16 npaug ntawm nitrogen. Rau 316L uas tsaws ze rau 24, uas yog txaus rau ntug hiav txwv cua, txheej txheem dej thiab dilute chlorides tab sis tsis yog rau kub concentrated chloride brines.

Yog vim li cas cov ntsiab lus qis Carbon tseem ceeb

Kev tswj hwm kev xav.Chromium carbides precipitate raws cov ciam teb nyob rau hauv 425-815 C ntau yam, stripping chromium los ntawm cov hlau uas nyob ib sab. 0.030% carbon qab nthab ntawm 316L suppresses nag lossis daus.

Tshaj tawm -weld condition.Welded assemblies feem ntau tuaj yeem muab tso ncaj qha rau hauv kev pabcuam yam tsis muaj kev daws teebmeem, uas tseem ceeb rau tuab -section hlab ntsha thiab teb welds.

Kev lag luam muaj zog -tawm.Cov pa roj carbon tsawg txo qis qhov pov thawj tsawg kawg nkaus rau txog 170 MPa tiv thaiv 205 MPa rau tus qauv 316, yog li cov neeg tsim qauv yuav tsum tso cai rau qhov sib txawv ntawm nyias - phab ntsa siab qhov chaw.

Dual ntawv pov thawj.Cov cua sov ua tau raws li kev sib tw nruj dua yog niaj hnub lees paub raws li 316/316L, tso cai rau ib qho cua sov kom txaus siab rau ob qho kev qhia tshwj xeeb.

Daim Ntawv Thov thiab Kev Pabcuam txwv

Cov kev siv ib txwm muaj xws li:

Petrochemical thiab refinery piping, kab, reactors thiab tshav kub exchangers.

Fertilizer thiab urea cog cov cuab yeej tuav ammonia thiab carbamate daws.

Pulp thiab ntawv digesters, bleach kab thiab chlorine dioxide kev pab cuam.

Dyeing, luam ntawv thiab textile machinery raug rau dye cawv thiab chav.

Khoom noj khoom haus, mis nyuj thiab brewery cog, nrog rau cov twj tso kua mis, li qub thiab tu tubing.

Pharmaceutical thiab bioprocessing skids ua kom siab -purity tiav cov cai.

Marine thiab offshore hardware, ntug hiav txwv fixings thiab architectural Cheebtsam.

Cov hniav nyiaj hniav kub thiab saib cov rooj plaub, qhov twg tarnish kuj thiab tsis tshua muaj teeb meem allergenicity.

Tshaj li kwv yees li 425 C hauv kev pabcuam txuas ntxiv, nkag thiab oxidation dhau los ua kev txwv, yog li siab dua - kub lub luag haujlwm yuav tsum raug xa mus rau qib ruaj khov lossis siab -nickel austenitic qib. Qhov twg cov khoom purity thiab corrosion kuj yuav tsum tau maximised, qhov tsawg -ferrite variants ntawm tib tsev neeg yog cov ib txwm specification.

FAQ

Q: Dab tsi ntawm stainless hlau yog 316L?
316L yog austenitic stainless hlau nrog lub ntsej muag -cented cubic qauv. Nws tsis yog-sib nqus hlau nplaum thaum annealed, tsis tuaj yeem hardened los ntawm kev kho cua sov, thiab ntxiv dag zog rau kev ua haujlwm txias.

Q: Puas yog 316L stainless hlau zoo rau cov hniav nyiaj hniav kub?
Yog lawm. Qib resists xeb, tarnishing thiab discoloration zoo dua 304, thiab nws yog feem ntau tolerated nyob rau hauv daim tawv nqaij daim ntaub ntawv. Qhov ntawd ua rau nws yog qhov kev xaiv zoo tshaj plaws rau cov nplhaib, caj dab thiab saib cov khoom.

Q: Qhov twg zoo dua, 304 lossis 316L stainless hlau?
316L muaj tsawg kawg yog 2.0% molybdenum, muab nws siab dua pitting thiab crevice corrosion tsis kam tshaj 304, tshwj xeeb tshaj yog nyob rau hauv chloride thiab acidic kev pab cuam . 304 tseem yog qhov kev xaiv pheej yig dua rau me me corrosive sab hauv lub luag hauj lwm.

Q: Puas yog 316L kim dua 316?
Cov nqi feem ntau yog nyob ze. Ntau qhov ntau lawm yog ob daim ntawv pov thawj raws li 316/316L, yog li ob qib feem ntau los ntawm tib lub tshav kub thiab tus nqi rau qhov qis -carbon lav yog me me.

Q: Puas yog 316L stainless hlau sib nqus?
Annealed 316L yog qhov zoo uas tsis yog-magnetic. Vuam, dabtsi yog khoov lossis kos duab txias tuaj yeem ua rau me me ntawm strain-induced martensite thiab cov lus teb me ntsis sib nqus, uas tsis qhia txog cov khoom siv tsis raug.

Q: Dab tsi yog qhov kev pabcuam siab tshaj plaws rau 316L?
Kev pabcuam txuas ntxiv yog ib txwm txwv rau kwv yees li 425 C, saum toj no uas nkag thiab oxidation ua qhov tseem ceeb. Siab dua - kub lub luag hauj lwm yuav tsum siv lub stabilized los yog siab -nickel austenitic qib hloov.