Dab tsi yog 2205 stainless hlau kaum?

Apr 27, 2026

Tso lus

Dab tsi yog 2205 stainless hlau kaum?

2205 stainless hlau lub kaum sab xis yog cov khoom siv ntev steel, tshwj xeeb yog duplex (austenitic{1}}ferritic) stainless hlau, muaj 22% chromium, 5-6% nickel, 3% molybdenum, thiab nitrogen. Nws cov ntaub ntawv tseem ceeb suav nrog sib npaug - ceg thiab tsis sib npaug - ceg kaum. Cov khoom siv no ua ke nrog lub zog siab (muaj lub zog tawm los kwv yees li ob npaug ntawm 316L) nrog kev ua haujlwm zoo heev rau chloride kev nyuaj siab corrosion tawg, pitting, thiab crevice corrosion; nws yog feem ntau siv hauv cov khoom siv roj thiab roj, ntawv- ua tshuab, kev tiv thaiv ib puag ncig, thiab siab - lub zog ntawm cov khoom siv.

 

2205 Stainless Steel Angle Supplier

GNEE yog tus kws tshaj lij duplex stainless hlau chaw tsim tshuaj paus nrog ntau tshaj 20 xyoo ntawm kev paub, nplooj siab rau exporting Alloy 2205 (UNS S32205 / 1.4462) duplex stainless hlau kaum bar rau ntau tshaj 70 lub teb chaws thoob ntiaj teb. Peb tau muab cov kev qhia tshwj xeeb zoo ib yam rau Middle East desalination nroj tsuag thiab offshore roj platforms, nrog rau cov khoom pov thawj los ntawm thib peb - tog soj ntsuam xws li SGS, BV, thiab ABS faib pawg neeg pov thawj.

 

EN 10204 3.1 Mill Test Certificate (MTC)

EN 10204 3.1 Mill Test Certificate (MTC)

 

Lub pitting thiab tawg corrosion kuj ntawm GNEE 2205 sib npaug lub kaum sab xis yog 3-5 npaug siab dua li ntawm 316L stainless hlau, ua rau nws tshwj xeeb tshaj yog haum rau chloride - muaj ib puag ncig thiab muaj txiaj ntsig txuas ntxiv kev pab cuam lub neej ntev li ob zaug. Lub zog tawm ntawm 2205 stainless hlau lub kaum sab xis yog ntau dua lossis sib npaug rau 450 MPa (kwv yees li ob zaug ntawm 316L), nrog lub zog tensile Ntau dua lossis sib npaug rau 620 MPa, hardness Tsawg dua lossis sib npaug rau 290 HBW, thiab cuam tshuam toughness Ntau dua lossis sib npaug rau 40J ntawm -40℃Siv cov khoom no tso cai rau 20% -30% txo qhov hnyav ntawm cov qauv thaum tswj kev ua haujlwm.

 

Peb 2205 lub kaum ntse ntse bar specifications muaj li ntawm 20 × 20 × 3 hli mus rau 200 × 200 × 20 hli, muaj nyob rau hauv ob qho tib si sib npaug thiab tsis sib npaug. Nto tiav suav nrog kub - dov thiab pickled xaiv. Peb kuj muab qhov loj me, txiav, drilling, kos duab-raws li fabrication, thiab me me{11}}batch qauv kev pab cuam, suav nrog precision txiav raws li engineering kos duab.

 

2205 Stainless Steel Angle

 

2205 Stainless hlau kaum Specifications

Hom

vaj huam sib luag steel, tsis sib npaug lub kaum steel

Thickness

3-24 hli

Ntev

1-12 m, los yog raws li xav tau

Equal Angle

Loj

20-200 hli

Qhov hnyav

0.597-71.168kg / m

Lub kaum sab xis

Loj

25 * 16-200 * 125mm

Ntev Sab

20-200 hli

Sab Qab Teb

16-125 hli

Qhov hnyav

1.687-43.588kg / m

Kev kho saum npoo

roj, dub, galvanized, pleev xim rau

Cov txheej txheem

Kub dov / txias dov / galvnized

Ntim

nrog pob, raws li tus qauv seaworthy pob lossis raws li cov neeg siv khoom xav tau

 

Chemical Composition (Tswj %)

Element Cov pa roj carbon (C) Manganese (Mn) Silicon (Si) Chromium (Cr) Nickel (Ni) Molybdenum (hli) Nitrogen (N)
Tus nqi Tsawg dua lossis sib npaug li 0.030 Tsawg dua lossis sib npaug li 2.00 Tsawg dua lossis sib npaug li 1.00 22.0 - 23.0 4.5 - 6.5 3.0 - 3.5 0.14 - 0.20

 

Mechanical Properties (Nyob ntawm Chav Kub)

Khoom Metric nqi Imperial nqi
Tensile zog (min) 620 MPa rau 90 ksg
Yield zog (0.2% Offset, min) 450 MPa 65 ksg
Elongation (% hauv 50mm, min) 25% 25%
Hardness (Brinell, max) 293 HWB -
Hardness (Rockwell C, max) 31 HRC -

 

Lub cev muaj zog

Khoom Tus nqi Chav tsev
Qhov ntom 7,800 kg/m³ (0.28 lb/in³)
Modulus ntawm Elasticity 200 GPa
Thermal conductivity (ntawm 100 degree) 19.0 W/m·K
Tshwj xeeb kub 450 J/kg · K
Hluav taws xob Resistivity 0.80 μΩ·m
PREN (Pitting Resistance Equiv. No.) 33 - 35

Cr+3.3Mo+16NCr+3.3Mo+16N

 

SS 2205 Lub kaum ntse ntse Bar Dimensions & Nyhav

Lub kaum sab xis feem ntau yog Kub Rolled lossis Laser Fused.

Loj (Peg A x Leg B) Thickness (t) Qhov hnyav (kg / m) Qhov hnyav (lb / ft)
25 x 25 mm (1" x 1") 3.0mm ib 1.12 kg / m 0.75 lb / ft
40 x 40 hli (1.5 "x 1.5") 4.0mm ib 2.42 kg / m 1.63 lb / ft
50 x 50 mm (2" x 2") 5.0mm ib 3.77 kg / m 2.53 lb / ft
50 x 50 mm (2" x 2") 6.0mm ib 4.47 kg / m 3.00 Ib/ft
75 x 75 mm (3 "x 3") 6.0mm ib 6.85kg / m 4.60 Ib/ft
75 x 75 mm (3 "x 3") 10.0 hli 11.00 Kg / m 7.39 lb / ft
100 x 100 hli (4 "x 4") 10.0 hli 15.00 Kg / m 10.08 lb / ft
100 x 100 hli (4 "x 4") 12.0mm 3 17.80 Kg / m 11.96 lb / ft

 

Dab tsi yog cov ntawv thov rau 2205 lub kaum ntse ntse?

Brackets rau offshore roj platforms.
Txhawb nqa hauv chemical processing tanks.
Cov khoom siv rau cov nroj tsuag desalination.
Cov choj thiab chaw nres nkoj infrastructure hauv thaj chaw ntug hiav txwv.

Applications For 2205 Angles

 

Raws li 2205 yog qib tshwj xeeb stainless hlau, ntau tus tub luam me tsis tuav cov khoom ntawm tes. Gnee, txawm li cas los xij, feem ntau tswj xyuas cov khoom lag luam tseem ceeb, ua rau kev xa khoom sai thiab pab txo cov sijhawm ua haujlwm.
Gnee tuav lub sijhawm ntev - kev koom tes nrog kev koom tes nrog cov tuam txhab hlau thoob ntiaj teb - xws li TISCO, Baosteel, thiab Tsingshan- yog li lav qhov tseeb ntawm peb cov ntaub ntawv raw. Muab hais tias 2205 yog ib qho tshwj xeeb stainless hlau, kev cai ntau lawm voj voog yuav siv sij hawm ntev li 45 mus rau 60 hnub; Txawm li cas los xij, Gnee feem ntau khaws cov khoom lag luam loj tuaj yeem muaj, ua kom yooj yim xa khoom sai thiab txo qhov project ntev.

 

Tus nqi - ntxiv cov kev pabcuam ua haujlwm

Precision txiav: Laser txiav, waterjet txiav, los yog txiav txiav.
Kev kho deg: polishing (raws li thov), sandblasting, lossis passivation.
Punching & dabtsi yog khoov: Ua ntej- ua tiav raws li engineering kos duab.

Value-Added Processing Services

Export Ntim

Gnee ntiav peb - txheej txheej ntim cov txheej txheem uas txo tus nqi ntawm kev puas tsuaj mus rau qis dua 0.3%. Peb siv cov cua sov- kho ntoo crates raws li ISPM15 cov qauv, ntxiv los ntawm VCI los tiv thaiv-corrosion puab ntim, yog li ua tiav txog li 99.9% kev tiv thaiv noo noo thaum lub sij hawm ntev - thauj hiav txwv. Txhua qhov khoom xa tuaj tau txhawb nqa nrog siab - lub zog steel hlua khi thiab haum nrog cov kev tiv thaiv ywj pheej los tiv thaiv qhov khawb ntawm qhov chaw thiab cov pa roj carbon monoxide.