Yog tias koj tab tom nrhiav qhov siab -kub stainless hlau piping, nkag siab qhovCov qib sib npaug ntawm EN 1.4845 stainless hlau yeeb nkabyog qhov tseem ceeb. Txawm hais tias koj tab tom muab cov qauv thoob ntiaj teb sib piv, ntsuas cov khoom hloov pauv, lossis tswj kev yuav khoom thoob ntiaj teb, kev paub txog qhov sib npaug tuaj yeem pab kom tsis txhob dhau -cov lus qhia tshwj xeeb, txuag nqi, thiab kev txiav txim siab ntawm cov saw hlau.

 

1.4845 Stainless Hlau Tube Cov Ntaub Ntawv Cov Ntaub Ntawv Download

 

1.4845 Stainless hlau yog dab tsi?

TS EN 1.4845, tseem hu ua X8CrNi25-21, yog siab -Tub kub Austenitic Stainless hlau uas muaj kwv yees li 25% Chromium thiab 20% Nickel, tsim los rau Oxidation Resistance zoo heev txog 1100-1150 degree. Nws yog feem ntau siv nyob rau hauv: Rauv qhov chaw, Thaum tshav kub kub exchangers, Radiant raj, High-temperature ducts thiab headers.
Nws Cov Ntsiab Cai Tsawg (max 0.04%) txhim kho weldability thiab txo qhov kev pheej hmoo ntawm carbide nag lossis daus piv rau cov qib zoo sib xws xws li 1.4841 (310).

Qib sib npaug ntawm 1.4845 Stainless Yeeb Nkab (Los ntawm Tus Qauv)

Txuj Qib sib npaug
ASTM / AISI 310S (UNS S31008)
DIN X8CrNi25-21
JIS SUS 310 S
GB (Tuam Tshoj) 0Cr25Ni20/310S
ISO / EU 1.4845

Tshuaj muaj pes tsawg leeg ntawm 1.4845 Stainless hlau yeeb nkab

Element Cim Cov ntsiab lus (%)
Chromium Cr 24.0 – 26.0
Nickel Ni 19.0 – 22.0
Cov pa roj carbon C Tsawg dua los yog sib npaug li 0.08
Silicon Si 1.00 – 1.50
Manganese Mn Tsawg dua lossis sib npaug li 2.00
Phosphorus P Tsawg dua lossis sib npaug li 0.045
Sulfur S Tsawg dua lossis sib npaug li 0.030
Hlau Fe Tshuav

Mechanical zog ntawm 1.4845 / 310S Stainless hlau yeeb nkab

Khoom Tus nqi
Tensile zog Ntau dua lossis sib npaug li 520 MPa
Lub zog muaj zog (0.2%) Ntau dua lossis sib npaug li 205 MPa
Elongation Ntau dua lossis sib npaug li 40%
Max ua haujlwm kub 1100-1150℃(Oxidizing ib puag ncig)

Creep Strength ntawm 1.4845 Stainless Hlau Yeeb Nkab (Hloov Zoo)

Kub (degree) Kev ntxhov siab rau 1% Creep hauv 10,000 h (MPa) Kev ntxhov siab rau Rupture hauv 100,000 h (MPa)
600 degree ~90 ~70
700 degree ~50 ~35
800 degree ~30 ~20
900 degree <20 <10

 

Cov ntsiab lus tseem ceeb rau cov neeg yuav khoom

Paub meej qhov ntev thiab phab ntsa thickness kam rau ua (ib ASTM A312 / EN 10216).

Yog tias welding, xyuas kom haum cov khoom siv hlau (ER310 lossis zoo sib xws) siv.

 

Peb muab1.4845 stainless hlau yeeb nkabthiab nws qhov sib npaug (310S, SUS310S) nrogntawv pov thawj, kev cai txiav lengths, thiabkev txhawb nqarau cov neeg yuav khoom thoob ntiaj teb. Cia peb pab koj xaiv cov qib zoo rau kojhigh -kub piping project.