UNS S43100 Martensitic Stainless Hlau - Siab -Lub zog Toughness Alloy
Feb 28, 2026
Tso lus
UNS S43100 Martensitic Stainless Hlau yog dab tsi?
Cov yam ntxwv tseem ceeb ntawm UNS S43100 Martensitic Stainless Hlau
Chemical Composition (wt%) ntawm UNS S43100 SS
|
C
|
Cr
|
Ni
|
Mn
|
Si
|
P
|
S
|
|---|---|---|---|---|---|---|
|
Tsawg dua los yog sib npaug li 0.20
|
15.00-17.00
|
1.25-2.50
|
Tsawg dua lossis sib npaug li 1.00
|
Tsawg dua lossis sib npaug li 1.00
|
Tsawg dua lossis sib npaug li 0.040
|
Tsawg dua lossis sib npaug li 0.030
|
Mechanical Properties ntawm UNS S43100 SS
|
Qhov xwm txheej
|
Tensile zog
|
Yield zog
|
Elongation
|
Hardness
|
|---|---|---|---|---|
|
Annealed
|
Ntau dua lossis sib npaug li 725 MPa
|
Ntau dua lossis sib npaug li 515 MPa
|
Ntau dua lossis sib npaug li 15%
|
Tsawg dua lossis sib npaug li 241 HB
|
|
Thaum tshav kub kub- kho
|
Ntau dua lossis sib npaug li 1000 MPa
|
Ntau tshaj lossis sib npaug li 700 MPa
|
Ntau dua lossis sib npaug li 10%
|
Ntau dua lossis sib npaug rau 285 HB
|
Qib sib npaug ntawm UNS S43100 SS
|
Txuj
|
Lub npe
|
|---|---|
|
AISI / SAE
|
431
|
|
EN
|
1.4057 (X17CrNi16-2)
|
|
GB
|
17Cr16Ni 2
|
|
JIS
|
SUS 431
|
UNS S43100 (AISI 431 / 1.4057) Martensitic Stainless Steel 2026 Export Reference Nqe
Kev siv ntawm UNS S43100 SS

S43100 Stainless Hlau Hydraulic Piston Qws
S43100 Stainless Hlau Marine Pump Ncej

S43100 Martensitic Stainless Hlau Siab -Txoj hlua khi
UNS S43100 SS Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

S43100 Stainless hlau kav

S43100 stainless hlau coils

S43100 stainless hlau phaj
Yog tias koj tab tom npaj ib qhov project, qhia rau kuv paub:
Yam khoom tshwj xeeb daim ntawvkoj xav tau (piv txwv li, round bar, ntawv, fasteners)
Qhov kev kho cua sov yuav tsum tau ualos yog mechanical zog lub hom phiaj
Kuv tuaj yeem pab muab cov lus qhia ntxiv los yog cov khoom siv ntxiv.
FAQ
Piv nrog rau qib 420: S43100 muaj npib tsib xee rau kev txhim kho toughness thiab corrosion kuj, zoo dua kev ua tau zoo tom qab quenching & tempering. Piv nrog 304: S43100 muab ntau zog thiab hardness, tab sis qis corrosion kuj. Nws yog hlau nplaum thiab yuav tsum tau kho cua sov rau lub zog nce.
Weldability tsis zoo, vuam tsis pom zoo. Yog tias vuam tsis tuaj yeem zam tau, tag nrho tom qab vuam kev kho cua sov yog qhov yuav tsum tau ua kom tsis txhob tawg. Forged los yog bar-stock machined qhov chaw yog nyiam
Tsis txhob ua kom tag nrho cov dej hiav txwv immersion, high-chloride ib puag ncig, muaj zog acid lossis alkali kev pabcuam. Qhov siab tshaj plaws kev pab cuam qhov kub thiab txias yog kwv yees li 400 degree.