Product Overview

UNS S30400 yog lub hauv paus austenitic stainless hlau nyob rau hauv 300 series, dav lees paub tias yog kev lag luam tus qauv rau ntau yam, tus nqi - zoo corrosion kuj thiab fabricability. Muab faib ua 18-8 stainless hlau (18% chromium, 8% npib tsib xee), nws tsim cov austenitic microstructure tag nrho ntawm chav tsev kub, xa cov khoom tsis yog- sib nqus thiab cov khoom tshwj xeeb. Qib no yog tsim los tiv thaiv atmospheric corrosion, raug dej tshiab, thiab ib puag ncig tshuaj lom neeg, ua rau nws haum rau huab hwm coj{11}}cov khoom tsim tawm thoob plaws cov neeg siv khoom thiab kev lag luam. Tsis zoo li cov alloys tshwj xeeb muaj kev ua tau zoo, S30400 ua qhov tseem ceeb ntawm kev ua haujlwm sib luag thiab kev pheej yig, nrog rau weldability zoo, formability, thiab polishability kom tau raws li kev xav tau ntau yam fabrication.

Chemical Composition (Mass Fraction, %)

C Tsawg dua lossis sib npaug 0.08, Cr: 18.00-20.00, Ni: 8.00-11.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.045, S Less dua lossis sib npaug 0.0130,

Mechanical Properties (Annealed Condition)

Tensile Strength Ntau dua lossis sib npaug ntawm 520 MPa; Yield zog ntau dua los yog sib npaug rau 205 MPa; Elongation Ntau dua lossis sib npaug li 40%; Hardness Tsawg dua los yog sib npaug rau 200 HB

Core Zoo

Unmatched versatility rau dav -cov ntaub ntawv siv hom phiaj; txhim khu kev qha corrosion kuj nyob rau hauv ib puag ncig me me; tsis yog- sib nqus ntawm chav tsev kub; tsis siv neeg tsim, vuam, thiab machining; tus nqi -ntau npaum rau loj- teev ntau lawm; superior nto tiav rau kev siv kho kom zoo nkauj.

Tej kev siv

Cov khoom siv hauv chav ua noj, cov khoom siv ua zaub mov, kev tsim vaj tsev, cov dej cia tank, tubing, fasteners, HVAC Cheebtsam, thiab cov khoom siv yuav tsum muaj kev tiv thaiv corrosion zoo ib yam.

Qib sib npaug

AISI 304, EN 1.4301, GB 06Cr19Ni10, SUS304

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.