Thermal conductivity ntawm SUS316 Stainless hlau yeeb nkab

Dec 03, 2025

Tso lus

Thermal conductivity ntawm SUS316

SUS316, kuj tau xaiv 316, 1.4401, lossis X5CrNiMo17-12-2, yog austenitic stainless hlau dav siv hauv kev ua tshuaj, khoom noj thiab dej haus, marine, thiab cov khoom siv tshuaj. Nws thermal conductivity yog tsawg piv nrog carbon steel, aluminium, los yog tooj liab vim nws cov austenitic siv lead ua qauv thiab cov alloying ntsiab chromium, npib tsib xee, thiab molybdenum uas tawg lattice vibrations.

Yam khoom muaj nqis

Nyob rau ntawm 20 degrees C lub thermal conductivity ntawm SUS316 yog hais txog 16.2 W ib meter ib Kelvin, nce maj mam nrog kub: kwv yees li 16.3 W ib meter ib Kelvin ntawm 100 degrees C thiab 21.5 W ib meter ib Kelvin ntawm 500 degrees C. Rau kev sib piv, cov conductivity ntawm SUS301 ib ncig ntawm 6. 100 ° C, thaum carbon steel yog kwv yees li plaub zaug siab dua thiab tooj liab ntau dua nees nkaum npaug siab dua.

Puas Thermal Conductivity cuam tshuam kev ua haujlwm

Lub thermal conductivity ruaj khov thiab ua kom pom tseeb ua kom ntseeg tau cov cua sov hloov hauv cov boilers, reactors, thiab cov cua kub exchangers. Tus nqi kuj tseem cuam tshuam rau qhov kub thiab txias ntawm thermal stress nyob rau hauv tuab - cov khoom siv phab ntsa, yog li cov neeg tsim qauv siv cov nqi luam tawm ntawm qhov ntsuas kub nruab nrab thaum xam qhov kub thiab txias ntawm phab ntsa.

Siab -Tsuas Txwv

SUS316 tuav lub zog muaj txiaj ntsig thiab tiv thaiv corrosion ntawm qhov kub thiab txias. Nws tuaj yeem siv tsis tu ncua txog li 870 ° C thiab txuas ntxiv mus txog li 925 ° C hauv cov huab cua oxidizing, txawm hais tias ntev li - lub zog siab tshaj 500 ° C qhov siab -carbon variant 316H tau pom zoo. Qhov qis coefficient ntawm thermal expansion ntawm austenitic steel pab tiv thaiv deformation thiab to hauv siab -kub tshuab.

Cov ntawv thov hauv Kev Hloov Kub Kub

SUS316 cov raj yog siv rau hauv cov raj xa hluav taws xob, cov raj boiler, cov kav dej, cov cua kub thiab txias, thiab cov khoom noj khoom haus - qib dej kub. Cov phab ntsa hauv du yuav txo tau cov dej tsis kam thiab txhim kho thermal efficiency, thiab cov ntsiab lus molybdenum tuav ntev -lub sij hawm stability nyob rau hauv chlorinated, acidic, los yog seawater ib puag ncig.

SUS316 piv rau SUS304 rau Kub Hloov

Tsis muaj qhov sib txawv tseem ceeb hauv kev hloov hluav taws xob ntawm SUS316 thiab SUS304. Txawm li cas los xij, vim tias SUS316 muaj kev tiv thaiv corrosion zoo dua, nws yog qhov kev xaiv zoo dua rau kev siv siab - kub qhov twg corrosion yog qhov tseem ceeb.

Cov lus nug nquag

Q: Dab tsi yog qhov thermal conductivity ntawm SUS316?

A: Txog 16.2 W ib meter ib Kelvin ntawm 20 ° C, nce mus rau 21.5 ntawm 500 ° C.

Q: Vim li cas stainless hlau conductivity tsawg?

A: Cov qauv austenitic thiab cov ntsiab lus alloying tawg ua kom sov- ua kev vibrations.

Q: Puas yog SUS316 zoo dua 304 rau kev hloov hluav taws xob?

A: Tsis yog, conductivity zoo ib yam; 316 yog nyiam rau corrosion kuj.

Q: Qhov ntsuas kub ntawm SUS316 yog dab tsi?

A: Kev siv tsis tu ncua txog li 870 ° C thiab siv txuas mus txog li 925 ° C.

Q: Dab tsi daim ntawv thov siv SUS316 raj?

A: Thaum tshav kub kub exchangers, boiler raj, chav kav dej, thiab cov dej kub.

Q: Qib twg pom zoo tshaj 500 degrees C?

A: 316H rau ntev - lub sij hawm siab - qhov kub thiab txias.

Tiv tauj peb rau SUS316 cov kav dej thiab cov raj nrog cov ntaub ntawv pov thawj thermal thiab mechanical khoom rau koj qhov project hloov tshav kub.