Qhov txawv ntawm 304, 304L, 316 thiab 316L
Dec 23, 2025
Tso lus
Marine qib stainless hlau, feem ntau hu ua 316, tiv taus qee yam kev cuam tshuam. Muaj ntau ntau hom 316 stainless hlau, suav nrog 316 L, F, N, H, thiab lwm yam. Txhua qhov sib txawv me ntsis thiab siv rau ntau lub hom phiaj. Lub npe "L" hauv 316L steel txhais tau hais tias muaj cov pa roj carbon tsawg dua hauv 316 steel. Nws yooj yim rau nco ntsoov vim "L" hauv cov ntsiab lus no txhais tau tias qis lossis qis.
Nta sib koom los ntawm 316 thiab 316L
Ob leeg 316 thiab 316L zoo ib yam li 304, uas yog siv rau hauv kev lag luam khoom noj, thiab lwm yam, tab sis hom 316 thiab 316L muaj kev tiv thaiv corrosion zoo dua thiab muaj zog ntawm qhov kub thiab txias. Lawv kuj yog ob qho tib si tsis yog - kho tau los ntawm kev kho cua sov thiab tuaj yeem ua tau yooj yim zoo li.
Qhov sib txawv ntawm 316 thiab 316L
316 stainless hlau muaj cov pa roj carbon ntau dua 316L. Qhov no yog ib qho yooj yim kom nco ntsoov, raws li L stands rau "qis" raws li tau hais ua ntej. Tab sis txawm hais tias nws muaj tsawg dua carbon, 316L zoo ib yam li 316 nyob rau hauv yuav luag txhua txoj kev. Lawv yog ob qho tib si muaj zog heev, corrosion resistant, thiab ib qho kev xaiv zoo rau cov xwm txheej high voltage.
316L yog qhov kev xaiv zoo dua rau cov haujlwm uas yuav tsum tau siv vuam ntau, vim nws muaj kev tiv thaiv ntau dua rau cov vuam lwj dua li 316. 316L kuj yog qhov kev xaiv zoo tshaj plaws ntawm cov hlau tsis muaj steel rau cov ntawv thov uas xav tau kub thiab corrosion kuj, ua rau nws nrov rau kev siv hauv kev tsim kho thiab sab nrauv.
Kev tsim- nce ntawm 316
316 steel yog austenitic chrome-nickel stainless hlau uas muaj nyob nruab nrab ntawm ob thiab peb feem pua molybdenum. Cov ntsiab lus molybdenum nce corrosion kuj, txhim kho kev tiv thaiv pitting hauv cov tshuaj chloride ion, thiab ua kom muaj zog ntawm qhov kub thiab txias.
316 stainless hlau yog tshwj xeeb tshaj yog zoo nyob rau hauv acidic thiab corrosive ib puag ncig. Cov hlau no muaj txiaj ntsig zoo hauv kev tiv thaiv corrosion los ntawm sulfuric acid, hydrochloric acid, acetic acid, formic acid thiab tartaric acid, nrog rau cov kua qaub sulfates thiab alkaline chlorides.
Qhov twg 316 feem ntau siv
Feem ntau siv rau stainless hlau 316 muaj xws li kev tsim kho ntawm cov pa manifolds, rauv qhov chaw, tshav kub exchangers, dav hlau cav qhov chaw, kev lag luam kws, li qub, twj tso kua mis qhov chaw, tshuaj txheej txheem khoom, tso tsheb hlau luam thiab evaporators.
Nta thiab muaj pes tsawg leeg ntawm 316 thiab 316L steel
• Ceev: 7.99g/cm3
• Hluav taws xob tiv taus: 74 microhm-cm (20 degrees Celsius)
• Cov cua kub tshwj xeeb: 0.50 kJ / kg-K (0-100 degrees Celsius)
• Thermal conductivity: 16.2 W/m-k (100 degrees Celsius)
• Elasticity module (MPa): 193 x 10 3 nyob rau hauv voltage
• Melting point: 2,500-2,550 degrees Fahrenheit (1,371-1,399 degrees Celsius)
| Element | 316 Stainless hlau (Tswj %) | 316L Stainless hlau (Tswj %) | Qhov tseem ceeb sib txawv / Function |
|---|---|---|---|
| Cov pa roj carbon (C) | Tsawg dua lossis sib npaug li 0.08 | Tsawg dua los yog sib npaug0.03 | Qhov txawv tseem ceeb. Cov pa roj carbon qis hauv 316L txo qhov kev pheej hmoo ntawm kev sib tsoo thaum vuam. |
| Molybdenum (hli) | 2.00 - 3.00 | 2.00 - 3.00 | Qhov tseem ceeb additive. Txhim khu kev tiv thaiv rau pitting / crevice corrosion, tshwj xeeb tshaj yog nyob rau hauv chlorides. |
| Chromium (Cr) | 16.0 - 18.0 | 16.0 - 18.0 | Muab qhov yooj yim corrosion / oxidation kuj. |
| Nickel (Ni) | 10.0 - 14.0 | 10.0 - 14.0 | Stabilizes austenitic qauv, txhim kho ductility & toughness. |
| Manganese (Mn) | Tsawg dua los yog sib npaug rau 2.0 | Tsawg dua los yog sib npaug rau 2.0 | Pab kub ua haujlwm. |
| Silicon (Si) | Tsawg dua lossis sib npaug li 0.75 | Tsawg dua lossis sib npaug li 0.75 | Deoxidizer, txhim kho siab -temp lub zog. |
| Phosphorus (P) | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.045 | Tswj impurity. |
| Sulfur (S) | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 0.030 | Tswj impurity. |
| Nitrogen (N) | Tsawg dua lossis sib npaug li 0.10 | Tsawg dua lossis sib npaug li 0.10 | Tej zaum yuav ntxiv los txhim kho lub zog. |
| Hlau (Fe) | Tshuav | Tshuav | Base hlau. |

304 steel
304 stainless hlau yog feem ntau siv austenitic (tsis yog-magnetic) stainless hlau. Nws tseem hu ua "18/8" stainless hlau vim nws muaj pes tsawg leeg, uas muaj 18% chromium thiab 8 feem pua nickel. Lub 304 stainless hlau muaj qhov zoo tsim thiab vuam muaj peev xwm, nrog rau kev tiv thaiv corrosion thiab lub zog.
Hom stainless hlau no kuj muaj tensile zoo.
Nws tuaj yeem ua tau zoo li ntau hom, thiab tsis zoo li hom 302 stainless, nws tuaj yeem siv yam tsis muaj feritizing mos ci. Feem ntau stainless hlau 304 daim ntawv thov thaj chaw muaj nyob rau hauv cov zaub mov kev lag luam. Nws yog qhov zoo tagnrho rau brewing, mis nyuj ua thiab winemaking, nrog rau cov kav dej, cov poov xab lauj kaub, dej fermentation thiab cia tanks.
304 stainless hlau kuj muaj nyob rau hauv dab dej, ntsiav tshuaj, lub thawv kas fes, tub yees, qhov cub, khoom siv hauv chav ua noj thiab lwm yam khoom siv hauv chav ua noj. Nws tiv taus corrosion uas tuaj yeem tshwm sim los ntawm ntau yam tshuaj muaj nyob hauv txiv hmab txiv ntoo, nqaij thiab mis nyuj. Lwm daim ntawv thov suav nrog kev tsim vaj tsev, cov ntim tshuaj, cov khoom siv hluav taws xob, cov khoom siv mining, nrog rau cov txiv ntoo hauv hiav txwv, bolts thiab cov ntsia hlau . 304 kuj tseem siv rau hauv cov mining thiab dej lim dej nrog rau hauv kev lag luam dyeing.
304l hlau
304L stainless hlau yog ib qho ntxiv - qis- carbon version ntawm 304 steel hlau. Cov ntsiab lus qis dua ntawm 304L txo qis carbide nag lossis daus los ntawm kev sib tsoo. Yog li ntawd, 304L tuaj yeem siv "raws li welded" nyob rau hauv ib puag ncig corrosive hnyav, tshem tawm qhov xav tau rau fertifying glowing.
Lub 304L muaj peev xwm ua kom qis me ntsis dua li tus qauv 304, tab sis tseem siv dav ua tsaug rau nws cov kev siv ntau yam. Zoo li 304 stainless hlau, nws feem ntau yog siv hauv npias brewing thiab winemaking, tab sis kuj rau lub hom phiaj tshaj li kev lag luam khoom noj xws li hauv cov thawv tshuaj, mining thiab kev tsim kho. Nws yog qhov zoo tagnrho rau siv hauv cov khoom hlau xws li cov txiv ntoo thiab cov bolts raug cov ntsev.
Nta thiab muaj pes tsawg leeg ntawm 304 thiab 304L steels
• Ceev: 8.03/cm3
• Hluav taws xob tiv taus: 72 microhm-cm (20 degrees Celsius)
• Cov cua kub tshwj xeeb: 0.50 kJ / kg-K (0-100 degrees Celsius)
• Thermal conductivity: 16.3 W / m-k (100 degrees Celsius)
• Elasticity module (MPa): 193 x 10 3 nyob rau hauv voltage
• Melting point: 2,500-2,650 degrees Fahrenheit (1,399-1,454 degrees Celsius)
| Element | 304 Stainless hlau (Tswj %) | 304L Stainless hlau (Tswj %) | Qhov tseem ceeb sib txawv / ceeb toom |
|---|---|---|---|
| Cov pa roj carbon (C) | Tsawg dua lossis sib npaug li 0.08 | Tsawg dua los yog sib npaug0.03 | Qhov tseem ceeb sib txawv. Cov pa roj carbon tsawg hauv 304L tiv thaiv kev tsim teeb meem chromium carbide thaum vuam. |
| Chromium (Cr) | 18.0 - 20.0 | 18.0 - 20.0 | Zoo sib xws; muab corrosion kuj. |
| Nickel (Ni) | 8.0 - 10.5 | 8.0 - 12.0 | Zoo sib xws; stabilizes austenitic qauv. |
| Manganese (Mn) | Tsawg dua los yog sib npaug rau 2.0 | Tsawg dua los yog sib npaug rau 2.0 | Zoo sib xws. |
| Silicon (Si) | Tsawg dua lossis sib npaug li 0.75 | Tsawg dua lossis sib npaug li 0.75 | Zoo sib xws. |
| Phosphorus (P) | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.045 | Zoo sib xws. |
| Sulfur (S) | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 0.030 | Zoo sib xws. |
| Hlau (Fe) | Tshuav | Tshuav | Tshuav. |
Peb muab ntau yam ntawm cov qib stainless hlau, suav nrog cov dav siv 304 thiab 316 series, nrog rau cov qib tshwj xeeb xws li 430, 201, duplex, thiab super austenitic steels, tailored kom tau raws li ntau yam kev lag luam thiab ib puag ncig. Txawm hais tias koj xav tau kev tiv thaiv corrosion-cov kev daws teeb meem rau kev siv dej hiav txwv, zaub mov- qib kev ua raws, siab- qhov kub thiab txias, lossis kev cai tshwj xeeb, peb pab pawg kws tshaj lij tau npaj los pab.
Peb lub Hoobkas
Raws li cov kws tshaj lij stainless hlau cov khoom tsim khoom, peb muaj cov kab ntau lawm niaj hnub no suav nrog kev txiav txiav, laser txiav, CNC dabtsi yog khoov, vuam tsis siv neeg, thiab kho kom zoo nkauj. Kev siv cov cuab yeej ua tiav qib siab thiab kev tswj hwm kev tswj hwm zoo, peb tshwj xeeb hauv kev tsim cov khoom zoo - cov khoom tsis zoo stainless hlau uas ua tau raws li cov qauv thoob ntiaj teb, suav nrog cov khoom lag luam, cov khoom siv hauv tsev, cov khoom siv hauv tsev, thiab cov khoom tshwj xeeb.

Stainless hlau ntim
Txhawm rau kom ntseeg tau tias peb cov khoom siv stainless hlau muaj kev tiv thaiv los ntawm khawb, cuam tshuam, thiab xeb thaum lub sijhawm thauj mus los thiab khaws cia, peb muab cov txheej txheem ntim cov kev daws teeb meem: precision nto yog tiv thaiv nrog electrostatic tiv thaiv zaj duab xis los yog peelable anti{0}}corrosion coatings; cov yeeb nkab thiab daim hlau tau ruaj ntseg nrog cov yeeb yaj kiab wrapping thiab kev cai- ua kaum tiv thaiv; cov khoom txheem tau ntim rau hauv cov hnab tiv thaiv - xeb thiab cov hlwv hlwv; thiab cov thawv sab nrauv tau cim meej nrog cov dej noo- pov thawj thiab "qhov no sab saum toj" daim ntawv lo. Tag nrho cov ntim ua raws li cov qauv kev xa tawm, ntsuas kev tiv thaiv, ib puag ncig tus phooj ywg, thiab yooj yim ntawm kev ntim khoom, lav tias cov khoom tuaj txog hauv qhov zoo tshaj plaws rau peb cov neeg siv khoom thoob ntiaj teb.