SUS431 Stainless Hlau: Siab -Lub zog Martensitic Alloy

Jan 28, 2026

Tso lus

What is 1.4535 Stainless Steel?What is 1.4460 Stainless Steel?What is 1.4436 Stainless Steel?

SUS431 Stainless hlau tshuaj muaj pes tsawg leeg

 

Element

Kev sib xyaw (wt%)

Lub luag haujlwm / cuam tshuam

Cov pa roj carbon (C)

0.20-0.30%

Cov ntsiab lus carbon siab nce hardness thiab hnav tsis kam tom qab kev kho cua sov.

Manganese (Mn)

0.60-1.00%

Txhim kho lub zog thiab toughness, tshwj xeeb tshaj yog nyob rau hauv qis kub.

Chromium (Cr)

16.0 – 18.0%

Muab kev tiv thaiv corrosion thiab oxidation, txhim kho durability.

Nickel (Ni)

≤ 0.60%

Txhim kho formability thiab ductility, txawm tias qis dua hauv qib austenitic.

Phosphorus (P)

≤ 0.04%

Txo cov kab mob sulfur thiab txhim kho machinability.

 

 

SUS431 Stainless hlau lub cev muaj zog

 

Khoom

Tus nqi

Sau ntawv

Qhov ntom

7.80 g / cm³

Me ntsis denser dua li lwm yam martensitic stainless hlau, ua kom ruaj khov.

Melting Point

1,400-1,530 ° C

Haum rau ob qho tib si txias thiab kub ua haujlwm, zoo tagnrho rau kev siv siab - kub.

Thermal conductivity

26.3 W/m·K

Nruab nrab cua sov dissipation, haum rau siab - cov ntawv siv cua sov.

Hluav taws xob Resistivity

7.4 × 10⁻⁷ Ω·m

Tsawg hluav taws xob conductivity, zoo tagnrho rau cov uas tsis yog - hluav taws xob daim ntawv thov.

 

 

SUS431 Stainless Hlau Mechanical Properties

 

Khoom

Tus nqi

Kev xeem Standard/Condition

Tensile zog

700 MPa

ASTM A240 / A240M tus qauv

Yield zog

500 MPa

Haum rau siab -cov ntawv siv zog

Elongation (50 hli ntsuas)

15%

Nruab nrab ductility rau shaping thiab sib sau.

Brinell Hardness

450-500 HB

Ua tiav tom qab kev kho cua sov, muab kev hnav zoo heev.

Machinability Rating

55% (vs . 1212 steel ntawm 100%)

Haum rau machining, txawm tias nws yuav tsum tau qeeb ceev los tswj hardness.