Dab tsi yog SUS316 Stainless Hlau Phaj & Coil?

SUS316 stainless hlau phaj & kauj yog molybdenum{1}}muaj cov khoom siv austenitic, hloov kho los ntawm SUS304. Nws cov molybdenum ntxiv ho txhim kho chloride corrosion kuj, haum rau ntug hiav txwv dej, marine thiab tsis muaj zog corrosive industrial scenarios.

Qib sib npaug (Horizontal)

UNS: S31600|JIS: SUS316|GB: 06Cr17Ni12Mo2|EN: X5CrNiMo17-12-2|W. Nr.: 1.4401

Chemical Composition (wt%, Kab rov tav)

C: Tsawg dua lossis sib npaug rau 0.08|Si: Tsawg dua lossis sib npaug rau 1.00|Mn: Tsawg dua lossis sib npaug rau 2.00|P: Tsawg dua lossis sib npaug rau 0.045|S: Tsawg dua lossis sib npaug rau 0.030|Cr: 16.00-18.00 Nws Nia: 10.00-14.00|Mo: 2.00-3.00 Nws Fe: Sib npaug

Cov khoom tseem ceeb (20 degree, Annealed, Kab rov tav)

Qhov ceev: 7.98g / cm³|Melting Point: 1375-1450 degree|Tensile zog: 515-690N/mm²|Yield Strength: Ntau dua lossis sib npaug rau 205N / mm²|Elongation: Ntau dua lossis sib npaug li 40%|Hardness: Tsawg dua los yog sib npaug rau 217HB

Cov yam ntxwv tseem ceeb

• Molybdenum-boosted corrosion kuj: Zoo tiv taus pitting thiab crevice corrosion los ntawm chloride ions, superior rau SUS304 • Excellence processability: Ib qho yooj yim rau daim ntawv thiab weld, haum rau complex-zoo li tus daim hlau / coils nyob rau hauv corrosive ib puag ncig • ruaj khov nruab nrab- kub mechanics • / kev sib npaug rau cov txheej txheem muaj zog scenario adaptability: Applied nyob rau hauv marine engineering, tshuaj ua thiab cov ntug dej hiav txwv architectural panels

SUS316 vs SUS316L Stainless hlau phaj & kauj (kab rov tav)

Cov ntsiab lus carbon: SUS316 (tsawg dua lossis sib npaug rau 0.08%)|SUS316L (tsawg dua lossis sib npaug rau 0.03%)|Tensile zog: SUS316 (515-690N/mm²)|SUS316L (485-650N/mm²)|Tom qab-weld Corrosion: SUS316 (Possible)|SUS316L (Tsis muaj)|Weld Adaptability: SUS316 (General)|SUS316L (zoo heev)

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, lossis ntim raws li cov neeg siv khoom xav tau.