SUS309S Stainless Hlau: Siab -Kev Ua Haujlwm Kub Ceev

Dec 25, 2025

Tso lus

SUS309S Stainless Steel: High-Temperature Performance OverviewThe difference between 304, 304L, 316 and 316L304 vs 304L stainless steel pipe comparison

Qhov tseem ceeb siab -Tswj yam ntxwv kub:

Oxidation Resistance: Mus txog 1900 ° F (1038 ° C) tsis yog -cyclic; Nyob ib ncig ntawm 1850 ° F (1010 ° C) nrog thermal cycling.

Corrosion Resistance: Superior rau Hom 304, tshwj xeeb tshaj yog nyob rau hauv siab - cua sov, oxidizing, thiab sulfurous (txog 1832 ° F / 1000 ° C) tej yam kev mob.

Lub zog: Khaws cov neeg kho tshuab kev ncaj ncees ntawm qhov kub siab, tsis zoo li ntau lwm cov hlau.

Carburization / Nitriding: Nruab nrab tsis kam; tsis yog rau carburizing heev (carbon{0}}nplua nuj) atmospheres.

Qhov zoo ntawm 'S' Qib (SUS309S):

Cov pa roj carbon tsawg (<0.08%): Tiv thaiv carbide nag lossis daus thaum lub sij hawm vuam, txo rhiab heev thiab txhim kho weldability.

Daim ntawv thov: Zoo dua haum rau welded Cheebtsam nyob rau hauv siab -temp kev pab cuam.

Kev siv ntau:

Muaj Furnaces & Boilers

Thaum tshav kub kub Exchangers

Thermal Processing Khoom

Kev kho cov khoom pov tseg

Xa kev nug