Hauv kev lag luam ntawm cov khoom siv hlau tsis muaj steel, SUS304 thiab SUS316 yog ob qho kev siv dav thiab cov qauv zoo heev. Lawv yog ob qho tib si austenitic stainless hlau uas muaj cov yam ntxwv xws li tsis yog- sib nqus, zoo toughness thiab kev ua tau zoo, tab sis lawv txawv ntawm ntau yam tseem ceeb.

 

SUS304 vs SUS316 Stainless Steel Chemical Composition

Khoom SUS 304(JIS G4303) SUS 316(JIS G4303)
Tshuaj muaj pes tsawg leeg    
- Chromium (Cr) 18.0–20.0% 16.0–18.0%
- Nickel (Ni) 8.0–10.5% 10.0–14.0%
- Molybdenum (Mo) Tsis Ntxiv 2.0–3.0%
- Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.08% Tsawg dua lossis sib npaug li 0.08%
- Manganese (Mn) Tsawg dua lossis sib npaug li 2.0% Tsawg dua lossis sib npaug li 2.0%
- Silicon (Si) Tsawg dua lossis sib npaug li 1.0% Tsawg dua lossis sib npaug li 1.0%
- Phosphorus (P) Tsawg dua lossis sib npaug li 0.045% Tsawg dua lossis sib npaug li 0.045%
- Sulfur (S) Tsawg dua lossis sib npaug li 0.030% Tsawg dua lossis sib npaug li 0.030%

 

SUS304 vs SUS316 Stainless Hlau Mechanical Properties

Mechanical Properties SUS 304(JIS G4303) SUS 316(JIS G4303)
- Tensile zog (MPa) Ntau dua lossis sib npaug li 520 Ntau dua lossis sib npaug li 520
- Yield zog (MPa) Ntau dua lossis sib npaug li 205 Ntau dua lossis sib npaug li 205
- Elongation (%) Ntau dua lossis sib npaug li 40% Ntau dua lossis sib npaug li 40%
- Hardness (Rockwell B) Tsawg dua lossis sib npaug li 92 Tsawg dua los yog sib npaug li 95
- Qhov ceev (g/cm³) 7.93 7.98

 

Dab tsi yog qhov txawv ntawm corrosion kuj ntawm SUS304 thiab SUS316 stainless hlau?

Ob leeg SUS304 thiab SUS316 yog austenitic stainless hlau, tab sis SUS316 yog qhov zoo dua li SUS304 hauv corrosion kuj vim qhov sib ntxiv ntawm 2-3% molybdenum (Mo). Qhov tseem ceeb sib txawv yog nyob rau hauv lub luag hauj lwm ntawm molybdenum: lub molybdenum nyob rau hauv SUS316 tsim ib tug denser oxide zaj duab xis (Cr₂O₃ + MoO₃), uas zoo tiv thaiv chloride ion (Cl⁻) corrosion, tshwj xeeb tshaj yog nyob rau hauv ib puag ncig uas muaj chlorine xws li dej hiav txwv thiab dej ntsev. Lub peev xwm los tiv thaiv pitting thiab crevice corrosion yog qhov zoo heev. SUS304 tsis muaj molybdenum thiab tso siab rau oxide zaj duab xis tsim los ntawm chromium (Cr) thiab npib tsib xee (Ni). Nws ua tau zoo nyob rau hauv cov huab cua zoo tib yam, dej tshiab los yog tsis muaj zog acidic ib puag ncig, tab sis nws yog nquag mus corrosion nyob rau hauv chloride ib puag ncig.
SUS316 muaj kev ua tau zoo nyob rau hauv qhov hnyav corrosive ib puag ncig vim qhov zoo ntawm molybdenum, tab sis tus nqi yog li 30-50% siab dua SUS304. Thaum xaiv, koj yuav tsum ntsuas ib puag ncig corrosiveness, pob nyiaj siv thiab khoom siv lub neej.

SUS316 Stainless Steel

Xa kev nug